Multiscale tomographic analysis of the thermal failure of Na-Ion batteries
Source abstract
Abstract
Abstract In recent years, the ability to examine the processes that cause the catastrophic failure of batteries as a result of thermal runaway has improved substantially. In this work, the effect of thermal runaway on the microstructure of the electrodes of a Na-ion battery is examined using X-ray computed tomography for the first time. The thermal failure induced via accelerating rate calorimetry enabled the examination of failed electrodes, which were subsequently compared with fresh samples. Pre- and post-mortem microstructural analysis shows changes in both electrodes as a result of the thermal runaway process at the micrometre length-scale. It is seen that the cathode shows the largest changes in structure, with the anode remaining morphologically similar post-failure at the sub-micron length-scale. The formation of a highly X-ray attenuating layer, which is proposed to be a metallic product of the thermal runaway reaction, is observed, indicating that the thermal runaway mechanisms which occur in Na-ion batteries may be similar to those reported for Li-ion systems.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. Beauregard · 2008
2. JTSB · 2014
3. AAIB · 2015
4. NTSB · 2014
5. Ellis · Chem. Mater. · 2010 · 22 · 105910.1021/cm902023h ↗
6. U.S. Geological Survey · 2008
7. Palomares · Energy Environ. Sci. · 2012 · 5 · 588410.1039/c2ee02781j ↗
8. Vignarooban · Int. J. Hydrogen Energy · 2016 · 41 · 282910.1016/j.ijhydene.2015.12.090 ↗
9. Slater · Adv. Funct. Mater. · 2013 · 23 · 94710.1002/adfm.201200691 ↗
10. J. Barker, C.J. Wright, Storage and/or Transportation of Sodium-Ion Cells, U. S. Patent No. WO2016027082 A1, (2016).
11. Kim · Adv. Energy Mater. · 2012 · 2 · 71010.1002/aenm.201200026 ↗
12. Bommier · Carbon · 2014 · 76 · 16510.1016/j.carbon.2014.04.064 ↗
13. Stevens · J. Electrochem. Soc. · 2001 · 148 · A80310.1149/1.1379565 ↗
14. Thomas · Electrochim. Acta · 2002 · 47 · 330310.1016/S0013-4686(02)00250-5 ↗
15. Stevens · J. Electrochem. Soc. · 2000 · 147 · 127110.1149/1.1393348 ↗
16. Kubota · J. Electrochem. Soc. · 2015 · 162 · A253810.1149/2.0151514jes ↗
17. Chevrier · J. Electrochem. Soc. · 2011 · 158 · A101110.1149/1.3607983 ↗
18. Alcántara · Electrochem. Solid State Lett. · 2005 · 8 · A22210.1149/1.1870612 ↗
19. Thomas · Electrochim. Acta · 2001 · 46 · 335910.1016/S0013-4686(01)00536-9 ↗
20. Alcántara · Electrochem. Commun. · 2001 · 3 · 63910.1016/S1388-2481(01)00244-2 ↗
21. Xiao · Chem. Commun. · 2012 · 48 · 332110.1039/c2cc17129e ↗
22. Sun · Electrochem. Commun. · 2011 · 13 · 146210.1016/j.elecom.2011.09.020 ↗
23. Jiang · Nanomater. Energy · 2014 · 5 · 6010.1016/j.nanoen.2014.02.002 ↗
24. Jäckle · J. Chem. Phys. · 2014 · 141 · 17471010.1063/1.4901055 ↗
25. Ellis · Curr. Opin. Solid State Mater. Sci. · 2012 · 16 · 16810.1016/j.cossms.2012.04.002 ↗
26. Ong · Energy Environ. Sci. · 2011 · 4 · 368010.1039/c1ee01782a ↗
27. Kim · Electrochem. Commun. · 2012 · 18 · 6610.1016/j.elecom.2012.02.020 ↗
28. Kim · Adv. Energy Mater. · 2011 · 1 · 33310.1002/aenm.201000061 ↗
29. Han · Energy Environ. Sci. · 2015 · 8 · 8110.1039/C4EE03192J ↗
30. Ni · Adv. Sci. · 2017 · 4 · 160027510.1002/advs.201600275 ↗
31. Xiang · Adv. Mater. · 2015 · 27 · 534310.1002/adma.201501527 ↗
32. Hong · Nat. Commun. · 2014 · 5 · 533510.1038/ncomms6335 ↗
33. Chihara · Electrochim. Acta · 2013 · 110 · 24010.1016/j.electacta.2013.04.100 ↗
34. Zhu · Chem. Commun. · 2013 · 49 · 1137010.1039/c3cc46642f ↗
35. Su · ACS Nano · 2014 · 8 · 362010.1021/nn500194q ↗
36. Wang · Nat. Commun. · 2015 · 6 · 749610.1038/ncomms8496 ↗
37. Shearing · Electrochem. Commun. · 2010 · 12 · 37410.1016/j.elecom.2009.12.038 ↗
38. Yufit · Electrochem. Commun. · 2011 · 13 · 60810.1016/j.elecom.2011.03.022 ↗
39. Robinson · J. Power Sources · 2014 · 252 · 5110.1016/j.jpowsour.2013.11.059 ↗
40. Eastwood · Adv. Energy Mater. · 2014 · 410.1002/aenm.201300506 ↗
41. Finegan · Adv. Sci. · 2015 · 310.1002/advs.201500332 ↗
42. Finegan · Nat. Commun. · 2015 · 610.1038/ncomms7924 ↗
43. Finegan · Phys. Chem. Chem. Phys. · 2016 · 18 · 3091210.1039/C6CP04251A ↗
44. Robinson · J. Electrochem. Energy Convers. Storage · 2017 · 15
45. Xia · Electrochem. Solid State Lett. · 2011 · 15 · A110.1149/2.002201esl ↗
46. Smith · ECS Trans. · 2017 · 75 · 1310.1149/07522.0013ecst ↗
47. Shearing · Electrochem. Commun. · 2010 · 12 · 37410.1016/j.elecom.2009.12.038 ↗
48. Shearing · Microsc. Anal. · 2013 · 27
49. Heenan · Fuel Cell. · 2017 · 17 · 7510.1002/fuce.201600176 ↗
50. Eastwood · Nucl. Instrum. Methods Phys. Res. Sect. B Beam Interact. Mater. Atoms · 2014 · 324 · 11810.1016/j.nimb.2013.08.066 ↗
51. Cooper · Software · 2016 · 5 · 20310.1016/j.softx.2016.09.002 ↗
52. Robinson · J. Electrochem. Energy Convers. Storage · 2017 · 15
53. Hong · J. Mater. Chem. · 2014 · 2 · 1273310.1039/C4TA02068E ↗
54. Maleki · J. Electrochem. Soc. · 1999 · 146 · 322410.1149/1.1392458 ↗
55. Golubkov · RSC Adv. · 2014 · 4 · 363310.1039/C3RA45748F ↗
56. Taiwo · J. Microsc. · 2016 · 263 · 28010.1111/jmi.12389 ↗
57. Taiwo · Chem. Eng. Sci. · 2016 · 154 · 2710.1016/j.ces.2016.04.023 ↗
58. Irisarri · J. Electrochem. Soc. · 2015 · 162 · A247610.1149/2.0091514jes ↗
59. E. Kendrick, R. Gruar, M. Nishijima, H. Mizuhata, T. Otani, I. Asako, Y. Kamimura, Tin Containing Compounds, Patent No. WO2105177568A1, (2015).
60. Heenan · Nano. Energy · 2018 · 47 · 55610.1016/j.nanoen.2018.03.001 ↗