journal article·2016-01

A flexible all-inorganic fuel cell membrane with conductivity above Nafion, and durable operation at 150 °C

Y. Ansari, T.G. Tucker, W. Huang, I.S. Klein, S.-Y. Lee, J.L. Yarger, C.A. Angell

Publisher page

Abstract

Abstract The search for fuel cell membranes has focused on carbon backbone polymers, among which Nafion seems to best survive the most severe of the degradation mechanisms – attack by peroxide radicals. Less attention has been given to inorganic membranes because of their generally inflexible nature and lower conductivity, though some SiO 2 -Nafion composites have shown improved properties. Nafion dominates, despite needing hydration, which then restricts operation to below 100 °C (so CO poisoning problems persist). Described herein is a low cost, flexible, and all-inorganic fiberglass reinforced gel membrane with conductivity exceeding that of Nafion at any temperature above 60 °C. Using Teflon fuel cells, maximum currents > 1 Acm −2 and OCV of 1.03 V at 150 °C are demonstrated. No detectable loss of cell potential was observed over 24 h during 50 mAcm −2 constant current operation at 120 °C while, at 150 °C and maximum power, the degradation rate is intermediate among other high conductivity H 3 PO 4 -PBI type membranes. The structure of the membrane is deduced, mainly from 29 Si solid state-NMR. The −115 ppm resonance, which is extreme for Q 4 Si(O) structures, identifies a zeolite-like SiO 2 network, which is “floppy”. 31 P and 1 H NMR establish nano-permeating H 3 PO 4 as the source of the exceptional conductivity.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advancements in Solid Oxide Fuel Cells

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Kreuer · J. Membr. Sci. · 2001 · 185 · 2910.1016/S0376-7388(00)00632-3 ↗
2. Peighambardoust · Int. J. Hydrogen Energy · 2010 · 35 · 934910.1016/j.ijhydene.2010.05.017 ↗
3. Zhang · Chem. Rev. · 2012 · 112 · 278010.1021/cr200035s ↗
4. Ghassemzadeh · J. Phys. Chem. C · 2010 · 114 · 1463510.1021/jp102533v ↗
5. Endoh · JESS Lett. · 2004 · 7 · A209
6. Feng · J. Phys. Chem. B · 2011 · 115 · 590310.1021/jp2002194 ↗
7. Asano · J. Amer. Chem. Soc. · 2006 · 128 · 176210.1021/ja0571491 ↗
8. Ji · Energies · 2009 · 2 · 105710.3390/en20401057 ↗
9. Zhai · J. Power Sources · 2007 · 169 · 25910.1016/j.jpowsour.2007.03.004 ↗
10. Aili · Int. J. Hydrogen Energy · 2011 · 36 · 698510.1016/j.ijhydene.2011.03.058 ↗
11. Tang · Electrochem. Commun. · 2007 · 9 · 200310.1016/j.elecom.2007.05.024 ↗
12. Kwak · Solid State Ion. · 2003 · 160 · 30910.1016/S0167-2738(03)00191-7 ↗
13. Li · Prog. Polym. Sci. · 2009 · 34 · 44910.1016/j.progpolymsci.2008.12.003 ↗
14. Belieres · Chem. Commun. Camb. · 2006 · 479910.1039/B611150E ↗
15. Susan · Chem. Commun. · 2003 · 93810.1039/b300959a ↗
16. Lee · J. Power Sources · 2010 · 195 · 590910.1016/j.jpowsour.2009.11.045 ↗
17. Park · J. Mater. Sci. Lett. · 2000 · 19 · 225110.1023/A:1006785110000 ↗
18. Tsvetkova · Glass Phys. Chem. · 2008 · 34 · 6810.1134/S1087659608010100 ↗
19. Matsuda · Solid State Ion. · 2002 · 154–155 · 68710.1016/S0167-2738(02)00518-0 ↗
20. Zhang · Chem. Rev. · 2012 · 112 · 278010.1021/cr200035s ↗
21. Kato · J. Membr. Sci. · 2007 · 303 · 4310.1016/j.memsci.2007.06.064 ↗
22. Zeng · ACS Appl. Mater. Interfaces · 2013 · 5 · 1124010.1021/am403479t ↗
23. Ansari · J. Power Sources · 2013 · 237 · 4710.1016/j.jpowsour.2013.03.003 ↗
24. Ansari · Provisional Pat. Appl. · 2012 · 2012
25. Li · Electrochim. Acta · 2010 · 55 · 212
26. Chung · J. Chem. Phys. · 2000 · 112 · 851510.1063/1.481454 ↗
27. Vilciauskas · Nat. Chem. · 2012 · 4 · 46210.1038/nchem.1329 ↗
28. Dippel · Solid State Ion. · 1993 · 61 · 4110.1016/0167-2738(93)90332-W ↗
29. Angell · Chem. Rev. · 1990 · 90 · 52310.1021/cr00101a006 ↗
30. Bernardi · J. Electrochem. Soc. · 1990 · 137 · 334410.1149/1.2086220 ↗
31. Springer · J. Electrochem. Soc. · 1991 · 138 · 233410.1149/1.2085971 ↗
32. Bernardi · J. Electrochem. Soc. · 1992 · 139 · 247710.1149/1.2221251 ↗
33. Mosdale · Electrochim. Acta · 1995 · 40 · 41310.1016/0013-4686(94)00289-D ↗
34. Okada · J. Electroanal. Chem. · 1996 · 413 · 4910.1016/0022-0728(96)04669-4 ↗
35. St-Pierre · J. New Mater. Electrochem. Syst. · 2000 · 3 · 99
36. Zhang · J. Magn. Reson. Im. · 2008 · 193 · 25910.1016/j.jmr.2008.05.005 ↗
37. Ji · Energies · 2009 · 2 · 105710.3390/en20401057 ↗
38. Liu · J. New Mater. Electrochem. Syst. · 2001 · 4 · 227
39. J. Thomson, Arizona State University, 2011 (Ph. D. Thesis).
40. Tsuchida · J. Phys. Soc. Jpn. · 2006 · 75 · 05480110.1143/JPSJ.75.054801 ↗
41. Krawietz · J. Am. Chem. Soc. · 1998 · 120 · 850210.1021/ja9813461 ↗
42. Elisa · J. Non Cryst. Solids · 2010 · 356 · 49510.1016/j.jnoncrysol.2009.12.006 ↗
43. Jähnigen · Chem. Commun. · 2012 · 48 · 767510.1039/c2cc31600e ↗
44. Magi · J. Phys. Chem. · 1984 · 88 · 151810.1021/j150652a015 ↗
45. Inagaki · Phys. Chem. Chem. Phys. · 2013 · 15 · 1352310.1039/c3cp51829a ↗
46. Greaves · Science · 2005 · 308 · 129910.1126/science.1109411 ↗
47. Dove · Phys. Rev. Lett. · 1997 · 78 · 107010.1103/PhysRevLett.78.1070 ↗
48. Thorpe · 1999
49. Matar · J. Power Sources · 2010 · 195 · 18110.1016/j.jpowsour.2009.06.084 ↗
50. Linares · J. Electrochem. Soc. · 2012 · 159 · F19410.1149/2.014207jes ↗
51. Xiao · Fuel Cells · 2005 · 5 · 28710.1002/fuce.200400067 ↗
52. Thomson · ECS Trans. · 2008 · 13 · 2110.1149/1.3055403 ↗