journal article·2020-06Open access

In-situ experimental benchmarking of solid oxide fuel cell metal interconnect solutions

Manuel Bianco, Priscilla Caliandro, Stefan Diethelm, Shicai Yang, Alessandro Dellai, Jan Van herle, Robert Steinberger-Wilckens

Abstract

The progress in the diffusion of solid oxide fuel cell (SOFC) as commercial devices is not paired by literature production. Articles describing the behaviour of SOFC stacks are rare because of confidentiality reasons for commercial suppliers while research centres prefer to focus on single components or low technology readiness level research. This article aim to fill this gap presenting the analysis of three short stacks run in operative conditions for 10 000 h each. The stacks are characterized through voltage vs time curves, electron microscopy, and electrochemical impedance spectroscopy. Focus is given on the interconnect; notably on the different types of coatings, varying for composition (MnCo2O4, MnCo1.8Fe0.2O4) and deposition technique (atmospheric plasma spray-APS, physical vapour deposition-PVD, wet powder spraying-WPS). Nitriding of the steel substrate as a solution to improve the chromium retention properties is tested as well. indicate that coating deposition technique is the most important parameter, with single repeat unit (SRU) containing PVD coating showing the lowest voltage degradation rate. Commercial ferritic stainless steel K41 confirmed to be a reliable choice if coupled with a coating. Moreover, SRU containing WPS coating demonstrated to be more reliable than expected from standard area specific resistance 4-probe test.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Post-test characterization of a solid oxide fuel cell stack operated for more than 30,000 hours: the cell10.1016/j.jpowsour.2017.11.025 ↗
2. Development, manufacturing and deployment of SOFC-based products at SOLIDpower10.1149/07801.0117ecst ↗
3. A cogeneration system based on solid oxide and proton exchange membrane fuel cells with hybrid storage for off-grid applications10.3389/fenrg.2018.00139 ↗
4. Recent development of SOFC metallic interconnect10.1016/S1005-0302(10)60049-7 ↗
5. Synergism in the design of interconnect alloy–coating combinations solid for oxide fuel cells10.1016/j.scriptamat.2010.09.020 ↗
6. Water vapour effects on Fe–Cr alloy oxidation10.1007/s11085-009-9183-9 ↗
7. Effects of water vapor on oxidation behavior of ferritic stainless steels under solid oxide fuel cell interconnect exposure conditions10.1016/j.ssi.2005.03.019 ↗
8. Fundamental mechanisms involved in the degradation of nickel–yttria stabilized zirconia (Ni–YSZ) anode during solid oxide fuel cells operation: a review10.1016/j.ceramint.2015.09.006 ↗
9. Material and method selection for efficient solid oxide fuel cell anode: recent advancements and reviews10.1002/er.4210 ↗
10. Cathode-side electrical contact and contact materials for solid oxide fuel cell stacking: a review10.1016/j.ijhydene.2017.08.005 ↗
11. Novel materials for solid oxide fuel cell technologies: a literature review10.1016/j.ijhydene.2017.08.105 ↗
12. The effect of polarization on SOFC seal ageing, XII EFCF Proc
13. Effects of the first heat up procedure on mechanical properties of solid oxide fuel cell sealing materials10.1016/j.jpowsour.2015.03.012 ↗
14. An alkali-free barium borosilicate viscous sealing glass for solid oxide fuel cells10.1016/j.jpowsour.2014.07.088 ↗
15. Developing accelerated stress test protocols for solid oxide fuel cells and electrolysers: the European project AD ASTRA10.1149/09101.0563ecst ↗
16. Long-term operation of solid oxide fuel cells and preliminary findings on accelerated testing10.1016/j.ijhydene.2020.01.074 ↗
17. Classical statistical methodology for accelerated testing of solid oxide fuel cells10.1016/j.jpowsour.2018.05.034 ↗
18. Metallic interconnectors for solid oxide fuel cells – a review
19. Air side contamination in solid oxide fuel cell stack testing10.1016/j.jpowsour.2010.10.058 ↗
20. Chromate formation at the interface between a solid oxide fuel cell sealing glass and interconnect alloy10.1016/j.jpowsour.2012.01.043 ↗
21. Interface reactivity study between La0.6Sr0.4Co0.2Fe0.8O3−δ (LSCF) cathode material and metallic interconnect for fuel cell10.1016/j.jpowsour.2010.09.063 ↗
22. Relationship between electrochemical properties of SOFC cathode and composition of oxide layer formed on metallic interconnects10.1016/j.jpowsour.2003.12.050 ↗
23. Tanasini · 2011
24. Chromium poisoning of LaMnO3-based cathode within generalized approach10.1002/fuce.201200164 ↗
25. Chromium deposition and poisoning of cathodes of solid oxide fuel cells – a review10.1016/j.ijhydene.2013.10.042 ↗
26. Metallic interconnects for solid oxide fuel cell: a review on protective coating and deposition techniques10.1016/j.ijhydene.2016.03.195 ↗
27. A review of recent progress in coatings, surface modifications and alloy developments for solid oxide fuel cell ferritic stainless steel interconnects10.1016/j.jpowsour.2009.09.069 ↗
28. Spinel and perovskite functional layers between plansee metallic interconnect (Cr‐5 wt % Fe‐1 wt % Y 2 O 3) and ceramic ( La0.85Sr0.15 ) 0.91MnO3 cathode materials for solid oxide fuel cells10.1149/1.1393891 ↗
29. Ex-situ experimental benchmarking of solid oxide fuel cell metal interconnects10.1016/j.jpowsour.2019.226900 ↗
30. Evaluation of protective coatings for SOFC interconnects10.1149/06801.1597ecst ↗
31. Composite Cu-LaFeO3 conversion coatings on a 18Cr ferritic stainless steel for IT-SOFC interconnects: effect of long-term air exposure at 700°C on Cr diffusion barrier and electrical properties10.1149/2.0101803jes ↗
32. Metals · 2010
33. Post-test analysis of a solid oxide fuel cell stack operated for 35,000 h, XII EFCF proceedings
34. Post-test characterization of an SOFC short-stack after 17,000 hours of steady operation10.1149/1.3569994 ↗
35. Component interactions after long-term operation of an SOFC stack with LSM cathode10.1016/j.jpowsour.2011.10.117 ↗
36. Durability test and degradation behavior of a 2.5 kW SOFC stack with internal reforming of LNG10.1016/j.ijhydene.2013.09.140 ↗
37. Post-test characterization of metallic materials and adjacent components in an SOFC stack after 34,000 h operation at 700 °C10.1002/fuce.201800050 ↗
38. Lifetime issues for solid oxide fuel cell interconnects
39. A direct manufacturing cost model for solid‐oxide fuel cell stacks10.1002/fuce.201700012 ↗
40. 2014
41. Manufacturing cost model for planar 5 kWel SOFC stacks at Forschungszentrum Jülich10.1016/j.ijhydene.2020.01.082 ↗
42. Thermodynamic considerations on Cr poisoning in SOFC cathodes10.1016/j.ssi.2006.07.055 ↗
43. Mechanism of breakaway oxidation of Fe–Cr and Fe–Cr–Ni alloys in dry and wet carbon dioxide
44. Corrosion behaviour of nitrided ferritic stainless steels for use in solid oxide fuel cell devices10.1016/j.corsci.2019.108414 ↗
45. The effect of grain size on the corrosion behaviour of inconel 600 in high-temperature steam10.1016/0010-938X(81)90024-X ↗
46. Comparison of different manganese-cobalt-iron spinel protective coating for SOFC interconnects
47. Degradation mechanisms of La – Sr – Co – Fe – O3 SOFC cathodes10.1149/1.2266160 ↗
48. Surface segregation in lanthanum strontium manganite thin films and its potential effect on the oxygen reduction reaction10.1149/2.0131710jes ↗
49. Effect of Sr content and strain on Sr surface segregation of La1–xSrxCo0.2Fe0.8O3−δ as cathode material for solid oxide fuel cells10.1021/acsami.6b07118 ↗
50. Studies on the defect structure of strontium oxide10.1016/0022-3697(68)90076-0 ↗
51. Caliandro · 2018