Underlying limitations behind impedance rise and capacity fade of single crystalline Ni-rich cathodes synthesized via a molten-salt route
Source abstract
Abstract
Layered oxide LiNi xMn yCo zO 2 (NMC) cathodes are often synthesized as polycrystalline secondary particles. Due to intergranular fracture stemming from volume changes of randomly oriented primary particles during charge/discharge, the synthesis of larger single-crystalline cathodes is of high interest. In this work, molten salt assisted growth of micron-sized Ni-rich crystals is achieved with excellent crystallinity, low cation mixing, and negligible impurities. However, electrochemical performance is compromised by high surface reactivity resulting in decomposition of electrolyte and subsequent formation of a thick CEI layer. While intergranular fracture is eliminated, planar gliding and severe intragranular fracture along the (003) plane occurs in the high voltage region within the first few cycles and is associated primarily with H2 to H3 structural transitions. In addition, H2 to H3 transitions are highly irreversible with cyclic voltammograms revealing polarization growth within <5 cycles. Subsequently, the single-crystalline material exhibited markedly reduced available capacity and enhanced capacity fade from sharp impedance growth compared to its polycrystalline counterpart. This work furthers a fundamental understanding into the limitations of single-crystalline Ni-rich cathodes, and the obstacles limiting the advantages offered by the single-crystalline morphology.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (69)
Show source-provided references
1. Automotive Li-ion batteries: current status and future perspectives10.1007/s41918-018-0022-z ↗
2. Breaking free from cobalt reliance in lithium-ion batteries10.1016/j.isci.2020.101505 ↗
3. Next-generation cobalt-free cathodes – a prospective solution to the battery industry's cobalt problem10.1002/aenm.202103050 ↗
4. Designing principle for Ni-rich cathode materials with high energy density for practical applications10.1016/j.nanoen.2018.04.062 ↗
5. Building safe lithium-ion batteries for electric vehicles: a review10.1007/s41918-019-00060-4 ↗
6. Ni‐Rich/Co‐Poor layered cathode for automotive Li‐ion batteries: promises and challenges
7. Prospect and reality of Ni-rich cathode for commercialization
8. Revealing mechanism of Li 3 PO 4 coating suppressed surface oxygen release for commercial Ni-rich layered cathodes10.1021/acsaem.0c00859 ↗
9. Bulk and surface degradation in layered Ni-rich cathode for Li ions batteries: defect proliferation via chain reaction mechanism10.1016/j.ensm.2020.11.016 ↗
10. Microstructural degradation of Ni-rich Li[Ni x Co y Mn 1 −x−y ]O 2 cathodes during accelerated calendar aging
11. Demonstrating apparently inconspicuous but sensitive impacts on the rollover failure of lithium-ion batteries at a high voltage10.1021/acsami.1c17408 ↗
12. Changing established belief on capacity fade mechanisms: thorough investigation of LiNi 1/3 Co 1/3 Mn 1/3 O 2 (NCM111) under high voltage conditions10.1021/acs.jpcc.6b11746 ↗
13. Evolution of structure and lithium dynamics in LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathodes during electrochemical cycling10.1021/acs.chemmater.9b00140 ↗
14. Research progress of single‐crystal nickel‐rich cathode materials for lithium ion batteries10.1002/smtd.202100234 ↗
15. Single-crystal high-nickel layered cathodes for lithium-ion batteries: advantages, mechanism, challenges and approaches
16. A perspective on single-crystal layered oxide cathodes for lithium-ion batteries10.1016/j.ensm.2021.02.003 ↗
17. Degradation mechanism of Ni-enriched NCA cathode for lithium batteries: are microcracks really critical?10.1021/acsenergylett.9b00733 ↗
18. Degradation and aging routes of Ni-rich cathode based Li-ion batteries10.3390/batteries6010008 ↗
19. Simultaneous enhancement of interfacial stability and kinetics of single-crystal LiNi 0.6 Mn 0.2 Co 0.2 O 2 through optimized surface coating and doping10.1021/acs.nanolett.0c03778 ↗
20. Comparison of single crystal and polycrystalline LiNi 0.5 Mn 0.3 Co 0.2 O 2 positive electrode materials for high voltage Li-ion cells10.1149/2.0991707jes ↗
21. J. Polycrystalline and single crystalline NCM cathode materials—quantifying particle cracking, active surface area, and lithium diffusion10.1002/aenm.202003400 ↗
22. Single-crystal nickel-rich layered-oxide battery cathode materials: synthesis, electrochemistry, and intra-granular fracture10.1016/j.ensm.2020.01.027 ↗
23. Lithium nickel cobalt manganese oxide synthesized using alkali chloride flux: morphology and performance as a cathode material for lithium ion batteries10.1021/am300386j ↗
24. Growth manner of octahedral-shaped Li(Ni 1/3 Co 1/3 Mn 1/3)O 2 single crystals in molten Na 2 SO 410.1021/acs.cgd.5b01723 ↗
25. Synthesis of single crystal LiNi 0.6 Mn 0.2 Co 0.2 O 2 with enhanced electrochemical performance for lithium ion batteries10.1149/2.0951805jes ↗
26. Mechanical and physical properties of LiNi0.33Mn0.33Co0.33O2 (NMC)10.1016/j.jeurceramsoc.2017.03.048 ↗
27. All-dry synthesis of single crystal NMC cathode materials for Li-ion batteries10.1149/1945-7111/abbcb1 ↗
28. A universal etching method for synthesizing high-performance single crystal cathode materials10.1016/j.nanoen.2021.106194 ↗
29. Temperature-swing synthesis of large-size single-crystal LiNi 0.6 Mn 0.2 Co 0.2 O 2 cathode materials10.1149/1945-7111/abdde0 ↗
30. Single-crystal based studies for correlating the properties and high-voltage performance of Li[Ni x Mn y Co 1−x−y ]O 2 cathodes10.1039/C8TA10329A ↗
31. Synthesis of single crystal LiNi 0.88 Co 0.09 Al 0.03 O 2 with a two-step lithiation method10.1149/2.0681910jes ↗
32. Comparison of single crystal and polycrystalline LiNi 0.5 Mn 0.3 Co 0.2 O 2 positive electrode materials for high voltage Li-ion cells10.1149/2.0991707jes ↗
33. Prospects and limitations of single-crystal cathode materials to overcome cross-talk phenomena in high-voltage lithium ion cells10.1039/D0TA11775G ↗
34. Assessing long‐term cycling stability of single‐crystal versus polycrystalline nickel‐rich NCM in pouch cells with 6 mAh cm −2 electrodes
35. On the sensitivity of the Ni-rich layered cathode materials for Li-ion batteries to the different calcination conditions10.3390/nano10102018 ↗
36. Superior cycle stability of single crystal nickel-rich layered oxides with micron-scale grain size as cathode material for lithium ion batteries10.20964/2020.06.03 ↗
37. Modified nickel-rich cathodes via conformal nanoparticle coating of precursors using a single reactor process10.1021/acsaem.1c03257 ↗
38. FTsalt · 2022
39. Effects of alkali cations and sulfate/chloride anions on the flux growth of {001}-Faceted β-Li 2 TiO 3 crystals10.1021/acs.cgd.6b01504 ↗
40. Powder characteristics of Pb(Mg1/3Nb2/3)O3 prepared by molten salt synthesis10.1111/j.1151-2916.1993.tb03770.x ↗
41. Oxygen anion solubility as a factor in molten flux crystal growth, synthesis, and characterization of four new reduced lanthanide molybdenum oxides: Ce 4.918(3) Mo 3 O 16 , Pr 4.880(3) Mo 3 O 16 , Nd 4.910(3) Mo 3 O 16 , and Sm 4.952(3) Mo 3 O 1610.1021/acs.cgd.6b00201 ↗
42. Surface regulation enables high stability of single-crystal lithium-ion cathodes at high voltage10.1038/s41467-020-16824-2 ↗
43. High performance cathode recovery from different electric vehicle recycling streams10.1021/acssuschemeng.8b02405 ↗
44. Minimization of the cation mixing in Li1+x(NMC)1−xO2 as cathode material10.1016/j.jpowsour.2009.09.029 ↗
45. Understanding fundamental effects of Cu impurity in different forms for recovered LiNi0.6Co0.2Mn0.2O2 cathode materials10.1016/j.nanoen.2020.105214 ↗
46. Quantitative analysis of Ni2+/Ni3+ in Li[NixMnyCoz]O2 cathode materials: non-linear least-squares fitting of XPS spectra10.1016/j.apsusc.2018.02.114 ↗
47. Controlling Ni 2+ from the surface to the bulk by a new cathode electrolyte interphase formation on a Ni-rich layered cathode in high-safe and high-energy-density lithium-ion batteries10.1021/acsami.0c22295 ↗
48. Revealing the degradation mechanism of Ni-rich cathode materials after ambient storage and related regeneration method10.1039/D0TA10378K ↗
49. Tuning the Li/Ni disorder of the NMC811 cathode by thermally driven competition between lattice ordering and structure decomposition10.1021/acs.jpcc.0c00720 ↗
50. Nasicon-type surface functional modification in core–shell LiNi 0.5 Mn 0.3 Co 0.2 O 2 @NaTi 2 (PO 4) 3 cathode enhances its high-voltage cycling stability and rate capacity toward Li-ion batteries10.1021/acsami.7b15808 ↗
51. Evaluating single-crystal and polycrystalline NMC811 electrodes in lithium-ion cells via non-destructive EIS alone10.1007/s10800-022-01713-x ↗
52. Activation mechanism of LiNi 0.80 Co 0.15 Al 0.05 O 2 : surface and bulk operando electrochemical, differential electrochemical mass spectrometry, and X-ray diffraction analyses10.1021/cm503833b ↗
53. Reaction heterogeneity in LiNi 0.8 Co 0.15 Al 0.05 O 2 induced by surface layer10.1021/acs.chemmater.7b02236 ↗
54. Surface-modified quaternary layered Ni-rich cathode materials by Li 2 ZrO 3 for improved electrochemical performance for high-power Li-ion batteries10.1021/acsaem.2c00224 ↗
55. Tuning cobalt‐free nickel‐rich layered LiNi 0.9 Mn 0.1 O 2 cathode material for lithium‐ion batteries10.1002/celc.202000443 ↗
56. Revealing the rate-limiting electrode of lithium batteries at high rates and mass loadings
57. Interfacial origin of performance improvement and fade for 4.6 V LiNi 0.5 Co 0.2 Mn 0.3 O 2 battery cathodes10.1021/jp501670g ↗
58. The cathode–electrolyte interface in the Li-ion battery10.1016/j.electacta.2004.03.049 ↗
59. Effect of particle size on LiNi 0.6 Mn 0.2 Co 0.2 O 2 layered oxide performance in Li-ion batteries10.1021/acsaem.1c03924 ↗
60. Reversible planar gliding and microcracking in a single-crystalline Ni-rich cathode10.1126/science.abc3167 ↗
61. Effect of lithiation upon the shear strength of NMC811 single crystals10.1149/1945-7111/ac6244 ↗
62. Mechanical properties of cathode materials for lithium-ion batteries10.1016/j.joule.2022.04.001 ↗
63. Bulk fatigue induced by surface reconstruction in layered Ni-rich cathodes for Li-ion batteries10.1038/s41563-020-0767-8 ↗
64. Improved cycling stability of Li[Ni 0.90 Co 0.05 Mn 0.05 ]O 2 through microstructure modification by boron doping for Li-ion batteries10.1002/aenm.201801202 ↗
65. Comprehensive study of Al- and Zr-modified LiNi 0.8 Mn 0.1 Co 0.1 O 2 through synergy of coating and doping10.1021/acsaem.0c01420 ↗
66. Targeted surface doping with reversible local environment improves oxygen stability at the electrochemical interfaces of nickel-rich cathode materials10.1021/acsami.9b14729 ↗
67. Stabilizing nickel-rich layered oxide cathodes by magnesium doping for rechargeable lithium-ion batteries10.1039/C8SC03385D ↗
68. From coating to dopant: how the transition metal composition affects alumina coatings on Ni-rich cathodes10.1021/acsami.7b13597 ↗
69. In situ inorganic conductive network formation in high-voltage single-crystal Ni-rich cathodes10.1038/s41467-021-25611-6 ↗