Elucidating cycling rate-dependent electrochemical strains in sodium iron phosphate cathodes for Na-ion batteries
Source abstract
Abstract
Abstract Battery electrodes materials undergo significant mechanical instabilities which affect their longevity and exert rate-limitations during the cycling process. In this study, we investigate the rate-dependent mechanical response of sodium iron phosphate (NaFePO4, NFP) cathodes during Na intercalation via galvanostatic cycling at different rates by employing digital image correlation, electrochemical methods, and mathematical model. The mechanical behavior of the electrode shows strong dependance on the applied scan rate. At slower rates, electrode shows asymmetrical strain generation between anodic and cathodic cycles, which is attributed to the formation of cathode-electrolyte interface layers. The electrode undergoes smaller strain generation when cycled at slower rates when the same amount of Na ions is removed or inserted into the electrode. A mathematical model was developed to predict strain evolution in the composite electrode as well as the concentration profile of the Na ions in the electrode particles. Rate-dependent and time-dependent factors on the strain generation in the electrode are attributed to the capacity-dependent intercalation strains, rate-dependent mismatch strains, and time-dependent irreversible strains. The combination of in situ strain measurements with the analytical model provided new insight into the electrochemically induced mechanical deformations in Na-ion cathode electrodes.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (82)
Show source-provided references
1. 30 Years of lithium-ion batteries
2. Cost projection of state of the art lithium-ion batteries for electric vehicles up to 203010.3390/en10091314 ↗
3. Sodium-ion batteries10.1002/adfm.201200691 ↗
4. Towards K-ion and Na-ion batteries as “beyond Li-ion10.1002/tcr.201700057 ↗
5. Interphases in sodium-ion batteries10.1002/aenm.201703082 ↗
6. Accommodating high transformation strains in battery electrodes via the formation of nanoscale intermediate phases: operando investigation of olivine NaFePO410.1021/acs.nanolett.6b04971 ↗
7. Large plastic deformation in high-capacity lithium-ion batteries caused by charge and discharge10.1111/j.1551-2916.2011.04432.x ↗
8. Revealing the mechanism of sodium diffusion in NaxFePO4 using an improved force field10.1021/acs.jpcc.8b00230 ↗
9. In situ TEM investigation of congruent phase transition and structural evolution of nanostructured silicon/carbon anode for lithium ion batteries10.1021/nl204559u ↗
10. In situ TEM study of lithiation behavior of silicon nanoparticles attached to and embedded in a carbon matrix10.1021/nn303312m ↗
11. In situ TEM experiments of electrochemical lithiation and delithiation of individual nanostructures10.1002/aenm.201200024 ↗
12. β-SnSb for sodium ion battery anodes: phase transformations responsible for enhanced cycling stability revealed by in situ TEM10.1021/acsenergylett.8b00762 ↗
13. Germanium as a sodium ion battery material: in situ TEM reveals fast sodiation kinetics with high capacity10.1021/acs.chemmater.6b00200 ↗
14. Facile synthesis and in situ transmission electron microscopy investigation of a highly stable Sb2Te3/C nanocomposite for sodium-ion batteries10.1016/j.ensm.2017.07.010 ↗
15. Probing microstructure and phase evolution of α-MoO3 nanobelts for sodium-ion batteries by in situ transmission electron microscopy10.1016/j.nanoen.2016.07.017 ↗
16. In situ electron microscopy investigation of sodiation of titanium disulfide nanoflakes10.1021/acsnano.9b04222 ↗
17. In situ atomic force microscopy study of initial solid electrolyte interphase formation on silicon electrodes for Li-ion batteries10.1021/am500363t ↗
18. In situ atomic force microscopy analysis of morphology and particle size changes in Lithium Iron Phosphate cathode during discharge10.1016/j.jcis.2014.02.035 ↗
19. In situ atomic force microscopy studies on lithium (de)intercalation- induced morphology changes in LixCoO2 micro-machined thin film electrodesq10.1016/j.jpowsour.2012.09.017 ↗
20. Atomic force microscopy studies on molybdenum disulfide flakes as sodium-ion anodes10.1021/nl503871s ↗
21. In situ atomic force microscopic studies of single tin nanoparticle: sodiation and desodiation in liquid electrolyte10.1021/acsami.7b08870 ↗
22. Probing three-dimensional sodiation-desodiation equilibrium in sodium-ion batteries by in situ hard X-ray nanotomography
23. In situ X-ray diffraction investigation of CoSe2 anode for Na-ion storage: effect of cut-off voltage on cycling stability10.1016/j.electacta.2017.11.198 ↗
24. Structure of the high voltage phase of layered P2-Na2/3-z[Mn1/2Fe1/2]O2 and the positive effect of Ni substitution on its stability10.1039/C5EE01365H ↗
25. In situ electrochemical dilatometry study of capacity fading in nanoporous Ge-based Na-ion battery anodes10.1016/j.scriptamat.2019.01.030 ↗
26. A comprehensive insight into the volumetric response of graphite electrodes upon sodium co-intercalation in ether-based electrolytes10.1016/j.electacta.2019.03.036 ↗
27. Electrochemical strain evolution in iron phosphate composite cathodes during lithium and sodium ion intercalation10.1016/j.electacta.2020.136594 ↗
28. In situ measurements of strains in composite battery electrodes during electrochemical cycling10.1007/s11340-014-9873-3 ↗
29. In operando tracking phase transformation evolution of lithium iron phosphate with hard X-ray microscopy
30. Surface coverage and SEI induced electrochemical surface stress changes during Li deposition in a model system for Li-ion battery anodes10.1149/2.068306jes ↗
31. In situ stress measurement during aluminum anodizing using phase-shifting curvature interferometry10.1149/2.025311jes ↗
32. Fracture of electrodes in lithium-ion batteries caused by fast charging10.1063/1.3492617 ↗
33. The influence of surface mechanics on diffusion induced stresses within spherical nanoparticles10.1063/1.3000442 ↗
34. Diffusion-induced stress, interfacial charge transfer, and criteria for avoiding crack initiation of electrode particles10.1149/1.3298892 ↗
35. Evolution of stress within a spherical insertion electrode particle under potentiostatic and galvanostatic operation10.1016/j.jpowsour.2009.01.021 ↗
36. A mathematical model of stress generation and fracture in lithium manganese oxide10.1149/1.2185287 ↗
37. Stress generation and fracture in lithium insertion materials10.1007/s10008-006-0095-1 ↗
38. Li · 2020
39. In-situ characterization of strain in lithium battery working electrodes10.1016/j.jpowsour.2014.08.035 ↗
40. Sodiation vs. Lithiation of FePO4: a comparative kinetic study10.1016/j.electacta.2016.09.041 ↗
41. In-situ preparation and electrochemical characterization of submicron sized NaFePO4 cathode material for sodium-ion batteries10.1016/j.electacta.2017.02.107 ↗
42. The mechanism of NaFePO4 (de)sodiation determined by in situ X-ray diffraction10.1039/C4CP01089B ↗
43. Crystal chemistry of Na insertion/deinsertion in FePO 4- NaFePO 410.1039/c2jm33639a ↗
44. Investigation of sodium insertion-extraction in olivine Na: XFePO4 (0 ≤ x ≤ 1) using first-principles calculations10.1039/C6CP00762G ↗
45. Rate dependence of the reaction mechanism in olivine NaFePO4 Na-ion cathode material10.1002/er.4078 ↗
46. Na-vacancy and charge ordering in Na≈2/3FePO410.1021/cm501110v ↗
47. Strain evolution in lithium manganese oxide electrodes10.1007/s11340-018-0381-8 ↗
48. Electrochemical strain evolution in iron phosphate composite cathodes during lithium and sodium ion intercalation10.1016/j.electacta.2020.136594 ↗
49. Controlling expansion in lithium manganese oxide composite electrodes via surface modification10.1149/2.0021912jes ↗
50. Cathode/electrolyte interface-dependent changes in stress and strain in lithium iron phosphate composite cathodes10.1149/2.1391912jes ↗
51. Electrochemical stiffness changes in lithium manganese oxide electrodes10.1002/aenm.201601778 ↗
52. Electrochemical stiffness in lithium-ion batteries10.1038/nmat4708 ↗
53. Reversible and irreversible deformation mechanisms of composite graphite electrodes in lithium-ion batteries10.1149/2.0751609jes ↗
54. Voltage hysteresis of lithium ion batteries caused by mechanical stress10.1039/C5CP06179B ↗
55. Voltage decay and redox asymmetry mitigation by reversible cation migration in lithium-rich layered oxide electrodes10.1038/s41563-019-0572-4 ↗
56. Discharge model for the lithium iron-phosphate electrode10.1149/1.1785012 ↗
57. Comparison of electrochemical performances of olivine NaFePO4 in sodium-ion batteries and olivine LiFePO4 in lithium-ion batteries10.1039/C2NR32758A ↗
58. In situ stress evolution in Li 1+x Mn 2 O 4 thin films during electrochemical cycling in Li-ion cells10.1149/2.0161613jes ↗
59. Thin film graphite electrodes with low stress generation during Li-intercalation10.1016/j.carbon.2011.02.067 ↗
60. An investigation of intercalation-induced stresses generated during lithium transport through Li1-δCoO2 film electrode using a laser beam deflection method10.1016/j.electacta.2004.05.004 ↗
61. LiFePO4 storage at room and elevated temperatures10.1016/S0378-7753(03)00215-5 ↗
62. Deformation and stress in electrode materials for Li-ion batteries10.1016/j.pmatsci.2014.02.001 ↗
63. Zhao · 2020
64. In situ stress evolution in Li 1+x Mn 2 O 4 thin films during electrochemical cycling in Li-ion cells10.1149/2.0161613jes ↗
65. A high precision coulometry study of the SEI growth in Li/graphite cells10.1149/1.3557892 ↗
66. Influence of electrolyte additives on the cathode electrolyte interphase (CEI) formation on LiNi1/3Mn1/3Co1/3O2 in half cells with Li metal counter electrode10.1016/j.jpowsour.2016.08.023 ↗
67. Review on modeling of the anode solid electrolyte interphase (SEI) for lithium-ion batteries10.1038/s41524-018-0064-0 ↗
68. Solvent diffusion model for aging of lithium-ion battery cells10.1149/1.1644601 ↗
69. Electrochemical kinetics of SEI growth on carbon black I: Experiments
70. Comparing anode and cathode electrode/electrolyte interface composition and morphology using soft and hard X-ray photoelectron spectroscopy10.1016/j.electacta.2013.03.010 ↗
71. Cooperation between active material, polymeric binder and conductive carbon additive in lithium ion battery cathode10.1021/jp208428w ↗
72. Unveiling the roles of binder in the mechanical integrity of electrodes for lithium-ion batteries10.1149/2.088309jes ↗
73. Nonfilling carbon coating of porous silicon micrometer-sized particles for high-performance lithium battery anodes10.1021/nn505410q ↗
74. Non-invasive in situ dynamic monitoring of elastic properties of composite battery electrodes by EQCM-D10.1002/anie.201501787 ↗
75. Combining rules for predicting the thermoelastic properties of particulate filled polymers, polymers, polyblends, and foams10.1002/pc.750020403 ↗
76. Numerical simulation of intercalation-induced stress in Li-ion battery electrode particles10.1149/1.2759840 ↗
77. “Electrochemical shock” of intercalation electrodes: a fracture mechanics analysis10.1149/1.3464773 ↗
78. The effect of stress on battery-electrode capacity10.1149/2.0371704jes ↗
79. Strain accommodation and potential hysteresis of LiFePO4 cathodes during lithium ion insertion/extraction10.1016/j.jpowsour.2010.08.008 ↗
80. Abnormal operando structural behavior of sodium battery material: influence of dynamic on phase diagram of NaxFePO410.1016/j.elecom.2013.11.017 ↗
81. Diffusion mediated lithiation stresses in Si thin film electrodes10.1149/2.009209jes ↗
82. In situ measurements of stress-potential coupling in lithiated silicon10.1149/1.3489378 ↗