journal article·2016-08Open access

In-tank hydrogen-ferric ion recombination

S. Selverston, R.F. Savinell, J.S. Wainright

Abstract

Abstract An H2 Fe3+ recombination method is being developed for all-iron flow batteries. Working principles are described and a proof-of-concept in-tank reactor is demonstrated. A membrane-less galvanic reactor is characterized using potential, polarization and impedance measurements at hydrogen partial pressures ranging from 0.3 to 11.3 psig. Through a vertical reactor geometry, hydrogen recombination rates of up to 60 mA cm−2 were measured at PH2 = 4.5 psig for a reactor with a platinum loading of 3.2 mg cm−2, based on the geometric catalyzed area. This is equivalent to over 375 mA cm−2 with respect to the cross sectional area of the reactor at the waterline. This rate is sufficient that the reactor will readily fit inside the positive reservoir of a flow battery. The reactor was found to be resistant to degradation by flooding or catalyst loss.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced battery technologies research · Hybrid Renewable Energy Systems · Electrocatalysts for Energy Conversion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Investigation of factors affecting performance of the iron redox battery10.1149/1.2127366 ↗
2. Studies of iron-ligand complexes for an all-iron flow battery application10.1149/2.0761410jes ↗
3. Maximizing plating density and efficiency for a negative deposition reaction in a flow battery10.1016/j.jpowsour.2014.06.125 ↗
4. An investigation into factors affecting the iron plating reaction for an all-iron flow battery10.1149/2.0591501jes ↗
5. A high efficiency iron-chloride redox flow battery for large-scale energy storage10.1149/2.0161601jes ↗
6. Nguyen · 2010 · 54
7. Kinetics of ferric oxyhydroxide precipitation10.1016/0169-7722(93)90042-Q ↗
8. Iron(III) hydrolysis and solubility at 25 °C10.1021/es070174h ↗
9. Iron solubility, colloids and their impact on iron (oxyhydr)oxide formation from solution10.1016/j.earscirev.2015.09.003 ↗
10. L. H. Thaller, Electrochemical Cell for Rebalancing Redox Flow System, U. S. Patent 4159366 (1979) 2–6.
11. Gahn · 1985
12. Acevedo · 1983
13. R. F. Gahn, Method and Apparatus for Rebalancing a Redox Flow Cell, Patent #4,576,878 (1986) 1–6.
14. Evans · 2014
15. Chang · 2014
16. Oxygenation of ferrous iron10.1021/ie50614a030 ↗
17. Investigation of a method to hinder charge imbalance in the vanadium redox flow battery10.1016/j.jpowsour.2012.11.148 ↗