journal article·2009-10

Applications of spin coating of polymer precursor and slurry suspensions for Solid Oxide Fuel Cell fabrication

Piotr Jasinski, Sebastian Molin, Maria Gazda, Vladimir Petrovsky, Harlan U. Anderson

Journal of Power Sources· Volume 194· Issue 1
Publisher page

Abstract

In this paper a ceramic deposition method that does not require a high temperature sintering step is presented. The method is used for a fabrication of electrolyte layers for SOFCs and high temperature protective coatings of stainless steel. The preparation of polymeric precursors and ceramic slurries are described and structure evolution of the deposited layers during heat treatment is discussed. Application of described method might help in eliminating problems related to excessive steel corrosion of metal supported SOFCs or reaction between electrolyte and cathode during high temperature sintering process.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Will · Solid State Ionics · 2000 · 131 · 7910.1016/S0167-2738(00)00624-X ↗
2. Beckel · J. Power Sources · 2007 · 173 · 32510.1016/j.jpowsour.2007.04.070 ↗
3. Singhal · 2003
4. Fergus · Mater. Sci. Eng. A · 2005 · 397 · 27110.1016/j.msea.2005.02.047 ↗
5. Anderson · J. Power Sources · 2004 · 129 · 18810.1016/j.jpowsour.2003.11.039 ↗
6. Huang · Ceram. Int. · 2003 · 29 · 48510.1016/S0272-8842(02)00191-8 ↗
7. Kim · Ceram. Int. · 2006 · 32 · 22310.1016/j.ceramint.2005.01.016 ↗
8. Xu · Ceram. Int. · 2005 · 31 · 106110.1016/j.ceramint.2004.11.005 ↗
9. Wang · J. Power Sources · 2007 · 163 · 95710.1016/j.jpowsour.2006.09.064 ↗
10. Wang · J. Power Sources · 2007 · 164 · 1710.1016/j.jpowsour.2006.09.090 ↗
11. Chen · Solid State Ionics · 2007 · 177 · 345510.1016/j.ssi.2006.10.003 ↗
12. Ai · J. Membr. Sci. · 2006 · 286 · 25510.1016/j.memsci.2006.10.003 ↗
13. Ai · J. Power Sources · 2006 · 159 · 63710.1016/j.jpowsour.2005.11.057 ↗
14. Chen · J. Power Sources · 2006 · 160 · 43610.1016/j.jpowsour.2006.01.079 ↗
15. Chen · J. Power Sources · 2007 · 172 · 74210.1016/j.jpowsour.2007.05.035 ↗
16. Hui · J. Power Sources · 2007 · 172 · 84010.1016/j.jpowsour.2007.05.036 ↗
17. Pan · Surf. Coat. Technol. · 2005 · 200 · 124210.1016/j.surfcoat.2005.07.083 ↗
18. Jasinski · J. Electrochem. Soc. · 2005 · 152 · A45410.1149/1.1846711 ↗
19. Petrovsky · Electrochem. Solid-State Lett. · 2004 · 7 · A13810.1149/1.1697904 ↗
20. Suzuki · J. Electrochem. Soc. · 2004 · 151 · A147310.1149/1.1782141 ↗
21. Suzuki · Solid State Ionics · 2006 · 177 · 207110.1016/j.ssi.2005.12.016 ↗
22. Suzuki · Electrochem. Solid-State Lett. · 2005 · 8 · A34110.1149/1.1928237 ↗
23. M.P. Pechini, US Patent 3,231,328 (1966).
24. Plonczak · J. Power Sources · 2008 · 181 · 110.1016/j.jpowsour.2007.12.019 ↗
25. H.U. Anderson, M.M. Nasrallah, C.-C. Chen, US Patent 5,494,700 (1996).
26. T. Suzuki, P. Jasinski, V. Petrovsky, H.U. Anderson, X.-D. Zhou, US Patent 2006/2080864 A1 (2006).
27. Simner · Electrochem. Solid-State Lett. · 2006 · 9 · A47810.1149/1.2266160 ↗
28. Simner · Solid State Ionics · 2003 · 161 · 1110.1016/S0167-2738(03)00158-9 ↗
29. Matus · Solid State Ionics · 2005 · 176 · 44310.1016/j.ssi.2004.09.056 ↗
30. Hui · J. Power Sources · 2007 · 167 · 33610.1016/j.jpowsour.2007.02.070 ↗
31. Tucker · J. Power Sources · 2008 · 175 · 44710.1016/j.jpowsour.2007.09.032 ↗
32. Tucker · J. Power Sources · 2007 · 171 · 47710.1016/j.jpowsour.2007.06.076 ↗
33. Mosleh · Mater. Sci. Eng. B · 2007 · 144 · 3810.1016/j.mseb.2007.07.089 ↗
34. Tuller · Solid State Ionics · 2000 · 131 · 14310.1016/S0167-2738(00)00629-9 ↗
35. Fontana · J. Power Sources · 2007 · 171 · 65210.1016/j.jpowsour.2007.06.255 ↗