journal article·2022-12

Corrosion inhibition of aluminum current collector by a newly synthesized 5-formyl-8-hydroxyquinoline for aqueous-based battery

Teshager Mekonnen Tekaligne, Semaw Kebede Merso, Sheng-Chiang Yang, Siao-Chun Liao, Feng-Yen Tsai, Fekadu Wubatu Fenta, Hailemariam Kassa Bezabih, Kassie Nigus Shitaw, Shi-Kai Jiang, Chia-Hsin Wang, She-Huang Wu, Wei-Nien Su, Bing Joe Hwang

Publisher page

Abstract

Aluminum foil is frequently used as a cathodic current collector for batteries because of its high electrical conductivity, low cost, robust electrochemical properties, and low density. However, as next-generation batteries are created, severe corrosion poses new challenges to aluminum current collectors, especially with no effective additive in an aqueous electrolyte so far. 5-formyl-8-hydroxyquinoline (FHQ) is designed and synthesized as an effective corrosion inhibitor for aluminum foil. Its corrosion inhibition efficacy and the passivation film are assessed by electrochemical methods and spectroscopy techniques. The corrosion rate in millimeters per year (mmpy) measured in the aqueous electrolyte of 21 m LiTFSI with the FHQ additive 1.37 × 10 −3 mmpy is much lower than 2.29 × 10 −2 mmpy in the unmodified electrolyte. Meanwhile, the Zn//LVPF configuration is developed as an efficient protocol to evaluate the corrosion prevention efficiency of inhibitors in an aqueous-based battery for the first time. The Zn//LVPF cell in the aqueous electrolyte with the FHQ additive provides much higher capacity retention and average Coulombic efficiency. Interestingly, the Al corrosion prevention efficiency of the developed additive is also testified in an organic electrolyte-based battery. This work paves a new pathway to develop effective Al corrosion inhibitors for lithium-ion batteries, especially in aqueous electrolytes.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Advancements in Battery Materials · Advanced battery technologies research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (73)

Show source-provided references
1. Tarascon · Nature · 2001 · 414 · 35910.1038/35104644 ↗
2. Armand · Nature · 2008 · 451 · 65210.1038/451652a ↗
3. Richa · Resour. Conserv. Recycl. · 2014 · 83 · 6310.1016/j.resconrec.2013.11.008 ↗
4. Whitehead · J. Electrochem. Soc. · 2005 · 152 · A210510.1149/1.2039587 ↗
5. Braithwaite · J. Electrochem. Soc. · 1999 · 146 · 44810.1149/1.1391627 ↗
6. Scrosati · Energy Environ. Sci. · 2011 · 4 · 328710.1039/c1ee01388b ↗
7. Li · Science · 1994 · 264 · 111510.1126/science.264.5162.1115 ↗
8. Li · J. Appl. Electrochem. · 2017 · 47 · 83910.1007/s10800-017-1081-2 ↗
9. Wang · Adv. Energy Mater. · 2012 · 2 · 83010.1002/aenm.201200065 ↗
10. Wessells · J. Power Sources · 2011 · 196 · 288410.1016/j.jpowsour.2010.10.098 ↗
11. Song · Chemelectrochem · 2014 · 1 · 87110.1002/celc.201300248 ↗
12. Alias · J. Power Sources · 2015 · 274 · 23710.1016/j.jpowsour.2014.10.009 ↗
13. Kim · Chem. Rev. · 2014 · 114 · 1178810.1021/cr500232y ↗
14. Choi · Nat. Rev. Mater. · 2016 · 110.1038/natrevmats.2016.13 ↗
15. Moosbauer · J. Chem. Eng. Data · 2010 · 55 · 179410.1021/je900867m ↗
16. Zhang · J. Electrochem. Soc. · 2005 · 152 · B44810.1149/1.2041867 ↗
17. Yang · J. Power Sources · 2006 · 161 · 57310.1016/j.jpowsour.2006.03.058 ↗
18. Zhang · J. Power Sources · 2002 · 109 · 45810.1016/S0378-7753(02)00110-6 ↗
19. Zhang · J. Electrochem. Soc. · 2006 · 153 · B34410.1149/1.2214465 ↗
20. Morita · Electrochim. Acta · 2002 · 47 · 278710.1016/S0013-4686(02)00164-0 ↗
21. Myung · J. Mater. Chem. · 2011 · 21 · 989110.1039/c0jm04353b ↗
22. Li · Mater. Corros. · 2016 · 67 · 97810.1002/maco.201608843 ↗
23. Yang · J. Electrochem. Soc. · 2000 · 147 · 439910.1149/1.1394077 ↗
24. Ma · J. Phys. Chem. Lett. · 2017 · 8 · 107210.1021/acs.jpclett.6b02933 ↗
25. Theivaprakasam · npj Materials Degradation · 2018 · 2 · 1310.1038/s41529-018-0033-6 ↗
26. Jüttner · Corrosion Sci. · 1989 · 29 · 27910.1016/0010-938X(89)90036-X ↗
27. Li · ACS Appl. Mater. Interfaces · 2019 · 11 · 3282610.1021/acsami.9b06442 ↗
28. Cho · Electrochem. Commun. · 2012 · 22 · 110.1016/j.elecom.2012.05.018 ↗
29. Meng · RSC Adv. · 2017 · 7 · 4301410.1039/C7RA08170G ↗
30. Meng · RSC Adv. · 2017 · 7
31. Krim · Chem. Eng. Commun. · 2009 · 196 · 153610.1080/00986440903155451 ↗
32. Guo · RSC Adv. · 2014 · 4 · 4195610.1039/C4RA04931D ↗
33. Popoola · Corrosion Rev. · 2019 · 37 · 7110.1515/corrrev-2018-0058 ↗
34. Choi · Surf. Coating. Technol. · 2012 · 206 · 235410.1016/j.surfcoat.2011.10.030 ↗
35. L.T. Popoola, 37 (2019) 71-102.10.1515/corrrev-2018-0058 ↗
36. 3 - corrosion inhibition with rare earth metal compounds in aqueous solutions
37. Kabanda · Int. J. Electrochem. Sci. · 2012 · 7 · 881310.1016/S1452-3981(23)18034-5 ↗
38. Ahamad · Corrosion Sci. · 2010 · 52 · 147210.1016/j.corsci.2010.01.015 ↗
39. Ma · J. Mol. Struct.: THEOCHEM · 2006 · 774 · 1910.1016/j.theochem.2006.06.044 ↗
40. Feng · J. Electroanal. Chem. · 2007 · 602 · 11510.1016/j.jelechem.2006.12.016 ↗
41. Guadalupe · J. Electroanal. Chem. · 2011 · 655 · 16410.1016/j.jelechem.2011.01.039 ↗
42. Obot · Mater. Chem. Phys. · 2010 · 122 · 32510.1016/j.matchemphys.2010.03.037 ↗
43. Vijayakumar · J. Mol. Struct.: THEOCHEM · 2006 · 770 · 2310.1016/j.theochem.2006.04.030 ↗
44. Zarrouk · J. Saudi Chem. Soc. · 2014 · 18 · 45010.1016/j.jscs.2011.09.011 ↗
45. Ju · Corrosion Sci. · 2008 · 50 · 86510.1016/j.corsci.2007.10.009 ↗
46. Lam · Bioorg. Med. Chem. Lett · 2014 · 24 · 36710.1016/j.bmcl.2013.10.072 ↗
47. Bard · 2001 · 5
48. El Faydy · Phys. Chem. Chem. Phys. · 2018 · 20 · 2016710.1039/C8CP03226B ↗
49. Zhang · Corrosion Sci. · 2012 · 61 · 110.1016/j.corsci.2012.03.045 ↗
50. Bulteau · New J. Chem. · 2020 · 44 · 1520910.1039/D0NJ02824J ↗
51. Bhaskara · Int. J. Corrosion. · 2021 · 202110.1155/2021/5869915 ↗
52. Prakashaiah · Corrosion Sci. · 2018 · 136 · 32610.1016/j.corsci.2018.03.021 ↗
53. Singh · Res. Chem. Intermed. · 2015 · 41 · 290110.1007/s11164-013-1398-3 ↗
54. Amin · Corrosion Sci. · 2011 · 53 · 87310.1016/j.corsci.2010.10.022 ↗
55. Elgahawi · J. Bio Tribo Corrosion. · 2017 · 3 · 5510.1007/s40735-017-0116-x ↗
56. Singh · Corrosion Sci. · 2010 · 52 · 15210.1016/j.corsci.2009.08.050 ↗
57. Hür · Prog. Org. Coating · 2006 · 57 · 14910.1016/j.porgcoat.2006.08.004 ↗
58. Gobara · J. Inorg. Organomet. Polym. Mater. · 2018 · 28 · 159810.1007/s10904-018-0790-2 ↗
59. Jüttner · Electrochim. Acta · 1990 · 35 · 150110.1016/0013-4686(90)80004-8 ↗
60. Haldhar · Mater. Chem. Front. · 2018 · 2 · 122510.1039/C8QM00120K ↗
61. Bouoidina · Chem. Res. Chin. Univ. · 2019 · 35 · 8510.1007/s40242-019-8205-7 ↗
62. Baer · J. Vac. Sci. Technol. · 2019 · 3710.1116/1.5065501 ↗
63. Wagner · 2003
64. Chiter · npj Materials Degradation · 2021 · 5 · 5210.1038/s41529-021-00198-x ↗
65. Olbasa · ACS Appl. Energy Mater. · 2020 · 3 · 449910.1021/acsaem.0c00183 ↗
66. Olbasa · Adv. Funct. Mater. · 2021
67. Xia · Angew. Chem. Int. Ed. · 2018 · 57 · 394310.1002/anie.201713291 ↗
68. Hao · Energy Environ. Sci. · 2020 · 13 · 391710.1039/D0EE02162H ↗
69. Brütsch · Thin Solid Films · 1985 · 126 · 31310.1016/0040-6090(85)90326-8 ↗
70. Higashi · Nat. Commun. · 2016 · 710.1038/ncomms11801 ↗
71. Hu · Joule · 2020 · 4 · 31010.1016/j.joule.2019.11.018 ↗
72. Hyams · J. Electrochem. Soc. · 2007 · 154 · C39010.1149/1.2742321 ↗
73. Dahbi · J. Power Sources · 2011 · 196 · 974310.1016/j.jpowsour.2011.07.071 ↗