journal article·2021-03

Dynamic modeling of chemical membrane degradation in polymer electrolyte fuel cells: Effect of pinhole formation

Weibo Zheng, Liangfei Xu, Zunyan Hu, Yujie Ding, Jianqiu Li, Minggao Ouyang

Publisher page

Abstract

Abstract The continuous chemical degradation of the polymer membrane in polymer electrolyte fuel cells causes membrane pinhole formation, therefore substantial increase in the gas cross-over flux. In this paper, a numerical method to simulate the pinhole formation process during chemical degradation is proposed. The method assumes that a membrane pinhole is formed by connected local micro-pores, which are generated owing to the mass loss during chemical membrane degradation. In addition, pinhole formation is combined with reduction of the membrane thickness to account for the membrane structure changes. A dynamic chemical degradation model that incorporates the effects of membrane structure changes is validated against the experimental results of the accelerated stress test. Results confirm the proposed method increases the accuracy of the chemical degradation model in predicting the macroscopic properties, including cumulative mass loss, hydrogen cross-over and open circuit voltage. Formation of pinhole starts from the anode, where degradation is more severe, and propagates to the cathode. The model also systemically studies the effects of temperature, pressure, and relative humidity on chemical degradation. The degradation rate increases with elevated temperatures and pressures. The degradation is shown to be more severe at moderate relative humidity, and the comparison with experimental findings are discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (63)

Show source-provided references
1. Fuel cell system for Honda CLARITY fuel cell10.1016/j.etran.2020.100046 ↗
2. Status of hydrogen fuel cell electric buses worldwide10.1016/j.jpowsour.2014.06.055 ↗
3. Polymer electrolyte fuel cell system level modelling and simulation of transient behavior
4. 3D failure analysis of pure mechanical and pure chemical degradation in fuel cell membranes10.1149/2.0451713jes ↗
5. Structure/property relationship of Nafion XL composite membranes10.1016/j.memsci.2016.06.004 ↗
6. Mechanical failure and mitigation strategies for the membrane in a proton exchange membrane fuel cell10.1016/j.rser.2019.109289 ↗
7. Quantifying the structural changes of perfluorosulfonated acid ionomer upon reaction with hydroxyl radicals10.1021/ja4037466 ↗
8. Visualizing chemical reactions and crossover processes in a fuel cell inserted in the ESR resonator: detection by spin trapping of oxygen radicals, nafion-derived fragments, and hydrogen and deuterium atoms10.1021/jp901597f ↗
9. Nafion degradation in PEFCs from end plate iron contamination10.1016/S0013-4686(03)00026-4 ↗
10. Kinetic simulation of the chemical stabilization mechanism in fuel cell membranes using cerium and manganese redox couples10.1149/2.075202jes ↗
11. Membrane degradation mechanisms in PEMFCs10.1149/1.2734869 ↗
12. Chemical durability studies of perfluorinated sulfonic acid polymers and model compounds under mimic fuel cell conditions10.1021/ma071603z ↗
13. Advanced materials for improved PEMFC performance and life10.1016/j.jpowsour.2004.01.023 ↗
14. Development of a method for clarifying the perfluorosulfonated membrane degradation mechanism in a fuel cell environment10.1149/1.2800171 ↗
15. In situ and operando characterization of proton exchange membrane fuel cells10.1002/adma.201901900 ↗
16. Effect of relative humidity on membrane degradation rate and mechanism in PEM fuel cells10.1149/1.2811696 ↗
17. Degradation analysis and modeling of reinforced catalyst coated membranes operated under OCV conditions10.1016/j.jpowsour.2008.05.074 ↗
18. Macroscopic in-situ modeling of chemical membrane degradation in polymer electrolyte fuel cells10.1149/2.0031409jes ↗
19. Physical modeling of chemical membrane degradation in polymer electrolyte membrane fuel cells: influence of pressure, relative humidity and cell voltage10.1016/j.jpowsour.2018.10.085 ↗
20. A degradation study of Nafion proton exchange membrane of PEM fuel cells10.1016/j.jpowsour.2007.03.061 ↗
21. Effect of free radical-induced degradation on water permeation through PFSA ionomer membranes10.1016/j.ijhydene.2015.07.118 ↗
22. Simultaneous electroosmotic and permeation flows through a Nafion membrane. 1. Aqueous electrolyte solutions10.1016/j.jcis.2004.04.066 ↗
23. Comparison of two accelerated Nafion™ degradation experiments10.1016/j.polymdegradstab.2007.10.001 ↗
24. A performance and degradation study of Nafion 212 membrane for proton exchange membrane fuel cells10.1016/j.jpowsour.2009.04.038 ↗
25. Effect of H2O2 on Nafion® properties and conductivity at fuel cell conditions10.1016/j.jpowsour.2010.11.133 ↗
26. Modeling chemical degradation of a polymer electrolyte membrane and its impact on fuel cell performance10.1149/1.3414024 ↗
27. A kinetic model for the chemical degradation of perfluorinated sulfonic acid ionomers: weak end groups versus side chain cleavage10.1016/j.polymer.2007.07.043 ↗
28. Modeling and simulation of the degradation of perfluorinated ion-exchange membranes in PEM fuel cells10.1149/1.3077573 ↗
29. Radical (HO●, H● and HOO●) formation and ionomer degradation in polymer electrolyte fuel cells10.1149/1.3581040 ↗
30. Mitigation of chemical membrane degradation in fuel cells: understanding the effect of cell voltage and iron ion redox cycle10.1002/cssc.201402957 ↗
31. In-situ modeling of chemical membrane degradation and mitigation in ceria-supported fuel cells10.1149/2.1201712jes ↗
32. Modeling the effect of chemical membrane degradation on PEMFC performance10.1149/2.0351806jes ↗
33. A multiparadigm modeling investigation of membrane chemical degradation in PEM fuel cells10.1149/2.0931514jes ↗
34. Study of fuel cell structure and heating method development of JARI's standard single cell10.1016/j.jpowsour.2005.02.090 ↗
35. Recoverable performance loss due to membrane chemical degradation in PEM fuel cells10.1149/2.063207jes ↗
36. Effects of operating parameters on hydrogen crossover rate through Nafion® membranes in polymer electrolyte membrane fuel cells10.1016/j.renene.2013.01.046 ↗
37. Modeling of fuel cell cold start and dimension reduction simplification method10.1149/1945-7111/ab6ee7 ↗
38. Comparison of self-humidification effect on polymer electrolyte membrane fuel cell with anodic and cathodic exhaust gas recirculation10.1016/j.ijhydene.2019.11.150 ↗
39. Dynamic contact angle modeling of droplet reattachment at the gas channel wall in polymer electrolyte fuel cells
40. Pt-oxide coverage-dependent oxygen reduction reaction (ORR) kinetics10.1149/2.088205jes ↗
41. Modeling of PEM fuel cell Pt/C catalyst degradation10.1016/j.jpowsour.2007.12.007 ↗
42. Comprehensive analysis of galvanostatic charge method for fuel cell degradation diagnosis10.1016/j.apenergy.2018.01.005 ↗
43. A novel diagnostic methodology for fuel cell stack health: performance, consistency and uniformity10.1016/j.enconman.2019.02.031 ↗
44. Modeling of H2O2 formation in PEMFCs, electrochim
45. Hydrogen peroxide formation rates in a PEMFC anode and cathode10.1149/1.2801980 ↗
46. Durability of perfluorosulfonic acid and hydrocarbon membranes: effect of humidity and temperature10.1149/1.2806798 ↗
47. Oxygen reduction reaction on Pt and Pt bimetallic surfaces: a selective review10.1002/1615-6854(200107)1:2<105::AID-FUCE105>3.0.CO;2-9 ↗
48. Modeling of the mixed potential in hydrogen peroxide-based fuel cells10.1016/j.ijhydene.2014.02.169 ↗
49. PEM fuel cell open circuit voltage (OCV) in the temperature range of 23°C to 120°C10.1016/j.jpowsour.2006.09.026 ↗
50. Reversible and irreversible degradation in fuel cells during Open Circuit Voltage durability testing10.1016/j.jpowsour.2008.04.009 ↗
51. Adsorption of bisulfate and sulfate anions on a Pt(111) electrode10.1021/jp003536f ↗
52. Oxygen reduction reaction on PtCo nanocatalyst: (Bi)sulfate anion poisoning10.1186/s11671-018-2574-6 ↗
53. A multiscale decomposition method for pore-scale simulation of multiphase transport and reactions in cathode catalyst layers of proton exchange membrane fuel cells
54. Chapter 5 - fuel cell operating conditions
55. Berechnung verschiedener physikalischer Konstanten von heterogenen Substanzen. I. Dielektrizitätskonstanten und Leitfähigkeiten der Mischkörper aus isotropen Substanzen10.1002/andp.19354160705 ↗
56. Standard electrode potential of Fe3+ + e- = Fe2+ from 5-35.deg10.1021/je60054a002 ↗
57. Atmospheric chemistry of perfluorinated carboxylic Acids: reaction with OH radicals and atmospheric lifetimes10.1021/jp036343b ↗
58. Transport in polymer-electrolyte membranes10.1149/1.1639157 ↗
59. Free volume and permeabilities of O2 and H2 in Nafion membranes for polymer electrolyte fuel cells10.1016/j.polymer.2008.05.003 ↗
60. The effects of catalyst layer microstructure and water saturation on the effective diffusivity in PEMFC10.1149/2.0711807jes ↗
61. The effect of humidity on the degradation of Nafion® membrane10.1016/j.polymdegradstab.2009.05.016 ↗
62. Effects of fuel cell operating conditions on proton exchange membrane durability at open‐circuit voltage10.1002/fuce.201900173 ↗
63. Factors determining the gas crossover through pinholes in polymer electrolyte fuel cell membranes10.1016/j.electacta.2012.07.013 ↗