Degradation of oxygen reduction reaction kinetics in porous La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3-δ cathodes due to aging-induced changes in surface chemistry
Source abstract
Abstract
Abstract The modification of surface composition after long-term operation is one of the most reported degradation mechanisms of (La,Sr)(Co,Fe)O3-δ (LSCFO) cathodes for Solid Oxide Fuel Cells (SOFCs). Nevertheless, its effect on the oxygen reduction reaction kinetics of porous LSCFO cathodes has not been yet reliably established. In this work, La- and Sr-enrichment at the LSCFO surface of porous cathodes has been induced after 50 h aging at 800 °C under air. Such cation redistribution can extend up to ∼400 nm depth under the LSCFO surface as detected by high resolution Scanning Transmission Electron Microscopy-Energy Dispersive Spectroscopy maps acquired inside the cathode pores. The observed surface chemical changes hamper the oxygen surface exchange reaction at the LSCFO/gas interface. Accordingly, a suitable Electrochemical Impedance Spectroscopy analysis revealed that the oxygen ion conductivity remains practically unaltered during the aging treatment while the oxygen surface exchange resistance increases up to 1.8 times. As a result, the cathode impedance response deteriorates within the 10–0.1 Hz frequency range during the aging treatment, resulting in a total cathode area specific resistance increase of 150%. The methodology adopted has demonstrated to be very valuable for studying the degradation of SOFC cathodes produced by the modification of surface composition.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Materials for fuel-cell technologies10.1038/35104620 ↗
2. Progress in material selection for solid oxide fuel cell technology: a review10.1016/j.pmatsci.2015.01.001 ↗
3. Materials and technologies for SOFC-components10.1016/S0955-2219(01)00120-0 ↗
4. Surface segregation and poisoning in materials for low-temperature SOFCs10.1557/mrs.2014.170 ↗
5. Durability of solid oxide fuel cells10.1515/green.2011.015 ↗
6. Fundamental mechanisms limiting solid oxide fuel cell durability10.1016/j.jpowsour.2008.02.016 ↗
7. Mechanisms of performance degradation of (La,Sr)(Co,Fe)O3-δ solid oxide fuel cell cathodes10.1149/2.0031607jes ↗
8. Effect of Sr surface segregation of La0.6Sr0.4Co0.2Fe0.8O3-δ electrode on its electrochemical performance in SOC10.1149/2.0371512jes ↗
9. Degradation mechanisms of La-Sr-Co-Fe-O3 SOFC cathodes10.1149/1.2266160 ↗
10. Improved chemical and electrochemical stability of perovskite oxides with less reducible cations at the surface10.1038/nmat4659 ↗
11. Chemical heterogeneities on La0.6Sr0.4CoO3-δ thin films-correlations to cathode surface activity and stability10.1021/cm203501u ↗
12. In-situ surface analysis of SOFC cathode degradation using high temperature enviromental scanning electron microscopy10.1149/06801.0665ecst ↗
13. Insight into surface segregation and chromium deposition on La0.6Sr0.4Co0.2Fe0.8O3-δ cathodes of solid oxide fuel cells10.1039/C4TA01426J ↗
14. Strontium surface segregation in La0.58Sr0.4Co0.2Fe0.8O3-δ annealed under compression10.1016/j.ssi.2014.09.019 ↗
15. Surface chemistry of La0.6Sr0.4CoO3-δ thin films and its impact on the oxygen surface exchange resistance10.1039/C5TA05279C ↗
16. Correlating surface cation composition and thin film microstructure with the electrochemical performance of lanthanum strontium cobaltite (LSC) electrodes10.1039/C3TA15327D ↗
17. Relationship between cation segregation and the electrochemical oxygen reduction kinetics of La0.6Sr0.4CoO3-δ thin film electrodes10.1149/1.3581114 ↗
18. Mechanism of La0.6Sr0.4Co0.2Fe0.8O3-δ cathode degradation10.1557/jmr.2012.222 ↗
19. Effect of cation demixing on the electrochemical performance of LSCFO cathodes for SOFCs10.1149/06402.0011ecst ↗
20. The language of particle size
21. Rasband · 1997
22. High resolution FIB-TEM and FIB-SEM characterization of electrode/electrolyte interfaces in solid oxide fuel cells materials10.1016/j.ijhydene.2011.04.121 ↗
23. Scribner Associates · 2010
24. Effect of cobalt-doped electrolyte on the electrochemical performance of LSCFO/CGO interfaces10.1149/07207.0117ecst ↗
25. Review on ceramic interphases by transmission and scanning electron microscopy10.3139/147.110306 ↗
26. Reactivity at the Ln2NiO4+δ/electrolyte interface (Ln = La, Nd) studied by electrochemical impedance spectroscopy and transmission electron microscopy10.1016/j.jpowsour.2014.04.082 ↗
27. An investigation of the oxygen reduction reaction mechanism of La0.6Sr0.4Co0.2Fe0.8O3 using patterned thin films10.1016/j.ssi.2011.10.029 ↗
28. Impedance spectroscopy study on well-defined (La,Sr)(Co,Fe)O3-δ model electrodes10.1016/j.ssi.2006.02.045 ↗
29. Impedance studies of oxygen exchange on dense thin film electrodes of La0.5Sr0.5CoO3-δ10.1149/1.1394010 ↗
30. Electrode kinetics of porous mixed-conducting oxygen electrodes10.1149/1.1837252 ↗
31. Mechanism and kinetics of oxygen reduction on porous La1-xSrxCoO3-δ electrodes10.1016/S0167-2738(98)00179-9 ↗
32. Factors governing oxygen reduction in solid oxides fuel cell cathodes10.1021/cr020724o ↗
33. Impedance of SOFC electrodes: a review and a comprehensive case study on the impedance of LSM: YSZ cathodes10.1016/j.electacta.2013.10.053 ↗
34. Effect of low temperature in-situ sintering on the impedance and the performance of intermediate temperature solid oxide fuel cell cathodes10.1016/j.jpowsour.2013.06.067 ↗
35. Effect of aging on the electrochemical performance of LSM-YSZ cathodes10.1149/2.0181509jes ↗
36. Interpretation of the gerischer impedance in solid state ionics10.1016/S0167-2738(02)00185-6 ↗
37. Oxygen transport properties of dense and porous (La0.8Sr0.2)0.99Co0.8Ni0.2O3-δ10.1016/j.ssi.2009.07.012 ↗
38. Impedance of porous IT-SOFC LSCF: CGO composite cathodes10.1016/j.electacta.2011.05.042 ↗
39. Oxygen exchange kinetics of La0.58Sr0.4Co0.2Fe0.8O3 at 600 °C in dry and humid atmospheres10.1016/j.ssi.2011.03.019 ↗
40. Surface composition of perovskite-type materials studied by low energy ion scattering (LEIS)10.1016/j.ssi.2013.09.010 ↗
41. Cation diffusion in La0.6Sr0.4CoO3-δ below 800 °C and its relevance for Sr segregation10.1039/c3cp51906f ↗
42. Degradation mechanism of SOFC cathodes under CrO3 and SO2 impurity exposures10.1149/05101.0069ecst ↗