Exceptionally stable polymer electrolyte for a lithium battery based on cross-linking by a residue-free process
Source abstract
Abstract
Abstract In this paper, we report the synthesis of cross-linked copolymers of glycidyl methacrylate (GMA) and poly (ethylene glycol) methyl methacrylate (PEGMA) for use as solid polymer electrolytes (SPE). The cross-linking is performed with volatile ethylene diamine, thus preventing the accumulation of undesirable precursors in the final membrane. The structure of the cross-linked polymer electrolyte was investigated by 13C solid NMR and its physical properties were examined by DSC, TGA and stress-strain tests. The ionic conductivities were determined by AC Impedance, which showed that the SPEs have good conductivities (10−5 Scm−1) at 80 °C. The highest capacity measured with these polymers was 151 mAh g−1 at C/6 and 80 °C for a LFP/SPE/Lithium battery. The retention capacity is high, at 97% after 80 cycles at different rates of cycling. The Young's modulus of the membranes is as high as 1 GPa. The SEM images showed no evidence of lithium dendrites and no degradation after cycling. Therefore, the polymer is a good candidate for battery operation over a long time. Especially important is the ability of this polymer to prevent growth of dendrites on the Li-metal electrode.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Advancements in Battery Materials · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Tarascon · Nature · 2001 · 414 · 35910.1038/35104644 ↗
2. Hammami · Nature · 2003 · 424 · 63510.1038/424635b ↗
3. Murata · Electrochimica Acta · 2000 · 45 · 150110.1016/S0013-4686(99)00365-5 ↗
4. Takehara · J. Power Sources · 1997 · 68 · 8210.1016/S0378-7753(96)02546-3 ↗
5. Armand · 1979 · p.131
6. Boden · Solid State Ionics · 1991 · 45 · 26110.1016/0167-2738(91)90160-D ↗
7. Marzantowicz · Electrochimica Acta · 2007 · 53 · 151810.1016/j.electacta.2007.03.032 ↗
8. Sun · Macromolecules · 2012 · 45 · 515110.1021/ma300775b ↗
9. Barteau · Macromolecules · 2013 · 46 · 898810.1021/ma401267w ↗
10. Borodin · Macromolecules · 2007 · 40 · 125210.1021/ma062128s ↗
11. Watanabe · J. Power Sources · 1999 · 81–82 · 78610.1016/S0378-7753(99)00250-5 ↗
12. Zuo · J. Mater. Chem. · 2012 · 22 · 2226510.1039/c2jm34270g ↗
13. Yuan · Macromolecules · 2013 · 46 · 91410.1021/ma3024552 ↗
14. Niitani · J. Electrochem. Soc. · 2009 · 156 · A57710.1149/1.3129245 ↗
15. Alloin · Solid State Ionics · 1993 · 60 · 310.1016/0167-2738(93)90267-7 ↗
16. Soo · J. Electrochem. Soc. · 1999 · 146 · 3210.1149/1.1391560 ↗
17. Zuo · J. Power Sources · 2013 · 239 · 11110.1016/j.jpowsour.2013.03.144 ↗
18. Alloin · J. Power Sources · 1995 · 54 · 3410.1016/0378-7753(94)02036-3 ↗
19. Elmér · J. Polym. Sci. Part A Polym. Chem. · 2006 · 44 · 219510.1002/pola.21324 ↗
20. Willgert · Solid State Ionics · 2013 · 236 · 2210.1016/j.ssi.2013.01.019 ↗
21. Walker · ACS Macro Lett. · 2012 · 1 · 73710.1021/mz300090m ↗
22. de Sainte Claire · Macromolecules · 2009 · 42 · 346910.1021/ma802469u ↗
23. Zhu · Polymer · 1990 · 31 · 172610.1016/0032-3861(90)90193-3 ↗
24. Emami · J. Polym. Sci. Part A Polym. Chem. · 2002 · 40 · 302110.1002/pola.10367 ↗
25. Choukourov · J. Phys. Chem. B · 2009 · 113 · 298410.1021/jp8107107 ↗
26. C.A.C. Sequeira, D.M.F. Santos, Polym. Electrolytes Fundam. Appl., p.131.
27. Luo · J. Appl. Polym. Sci. · 2011 · 120 · 297910.1002/app.33363 ↗
28. Patil · Soft Mater. · 2013 · 9 · 358910.1039/c3sm27525f ↗
29. Monroe · J. Electrochem. Soc. · 2003 · 150 · A137710.1149/1.1606686 ↗
30. Monroe · J. Electrochem. Soc. · 2004 · 151 · A88010.1149/1.1710893 ↗
31. Monroe · J. Electrochem. Soc. · 2005 · 152 · A39610.1149/1.1850854 ↗
32. Benaglia · Polym. Chem. · 2013 · 4 · 12410.1039/C2PY20646C ↗
33. Daigle · Polym. Chem. · 2013 · 4 · 44910.1039/C2PY20860A ↗
34. Garroway · Macromolecules · 1982 · 15 · 105110.1021/ma00232a019 ↗
35. Tavares · J. Appl. Polym. Sci. · 2000 · 78 · 235810.1002/1097-4628(20001220)78:13<2358::AID-APP120>3.0.CO;2-T ↗
36. Hutchinson · Macromolecules · 1998 · 31 · 154210.1021/ma971307u ↗
37. Stone · J. Electrochem. Soc. · 2012 · 159 · A22210.1149/2.030203jes ↗
38. Tran · Electrochimica Acta · 2013 · 88 · 53610.1016/j.electacta.2012.10.139 ↗
39. Glazer · J. Polym. Sci. · 1954 · 13 · 35510.1002/pol.1954.120137004 ↗
40. Bouchet · Nat. Mater. · 2013 · 12 · 45210.1038/nmat3602 ↗
41. Fan · Solid State Ionics · 2003 · 164 · 8110.1016/j.ssi.2003.08.004 ↗
42. Niitani · J. Power Sources · 2005 · 146 · 38610.1016/j.jpowsour.2005.03.102 ↗
43. Niitani · Electrochem. Solid-State Lett. · 2005 · 8 · A38510.1149/1.1940491 ↗
44. Hallinan · J. Electrochem. Soc. · 2013 · 160 · A46410.1149/2.030303jes ↗
45. Yuan · Macromolecules · 2013 · 46 · 91410.1021/ma3024552 ↗
46. Xue · J. Mater. Chem. A · 2015 · 3 · 1921810.1039/C5TA03471J ↗
47. Daigle · J. Power Sources · 2015 · 279 · 37210.1016/j.jpowsour.2014.12.061 ↗
48. Tran · Solid State Ionics · 2013 · 232 · 3710.1016/j.ssi.2012.11.007 ↗
49. Choi · Langmuir · 1999 · 15 · 844710.1021/la990312j ↗
50. Croce · J. Power Sources · 2006 · 162 · 68510.1016/j.jpowsour.2006.07.038 ↗