X-ray photoelectron spectroscopy investigation on electrochemical degradation of proton exchange membrane fuel cell electrodes

Shuang Ma Andersen, Rajnish Dhiman, Eivind Skou

Publisher page

Abstract

Abstract X-ray photoelectron spectroscopy studies were systematically carried out on the electrodes before and after the electrochemical stress tests in an aqueous electrolyte at 20 °C and 70 °C. The electrodes have different ionomer structures (no ionomer, only ionomer, physically mixed ionomer and hot pressed ionomer) but have identical, commercial catalyst and catalyst loading. A significant degree of carbon corrosion, platinum migration and ionomer degradation were observed in the electrodes after the treatment. The degradation of the ionomer in the electrode is more severe than that of membrane. The electrode structure and the corresponding interface are crucial for the catalyst performance and durability.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrocatalysts for Energy Conversion · Fuel Cells and Related Materials · Advanced battery technologies research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Yuan · J. Power Sources · 2011 · 196 · 910710.1016/j.jpowsour.2011.07.082 ↗
2. Zhang · J. Power Sources · 2009 · 194 · 58810.1016/j.jpowsour.2009.06.073 ↗
3. Othman · Int. J. Hydrogen Energy · 2012 · 37 · 35710.1016/j.ijhydene.2011.08.095 ↗
4. Sharma · J. Power Sources · 2012 · 208 · 9610.1016/j.jpowsour.2012.02.011 ↗
5. U.S. Department of Energy · 2007
6. Ohma · ECS Trans. · 2011 · 41 · 77510.1149/1.3635611 ↗
7. Ma · Solid State Ionics · 2007 · 178 · 156810.1016/j.ssi.2007.10.007 ↗
8. Tucker · J. Electrochem. Soc. · 2005 · 152 · A184410.1149/1.1993488 ↗
9. Niya · J. Power Sources · 2013 · 240 · 28110.1016/j.jpowsour.2013.04.011 ↗
10. Lee · J. Power Sources · 2013 · 230 · 10110.1016/j.jpowsour.2012.12.030 ↗
11. Wang · Nanoscale · 2014 · 6 · 137710.1039/C3NR04663J ↗
12. Kakinuma · Electrochm. Acta · 2013 · 110 · 31610.1016/j.electacta.2013.06.127 ↗
13. He · Carbon · 2011 · 49 · 8210.1016/j.carbon.2010.08.045 ↗
14. Zhao · Carbon · 2014 · 67 · 40910.1016/j.carbon.2013.10.012 ↗
15. He · J. Phys. Chem. C · 2013 · 117 · 2530510.1021/jp408653f ↗
16. Mauritz · Chem. Rev. · 2004 · 104 · 453510.1021/cr0207123 ↗
17. Gebel · Polymer · 2000 · 41 · 582910.1016/S0032-3861(99)00770-3 ↗
18. Malek · Electrocatalysis · 2011 · 2 · 14110.1007/s12678-011-0047-0 ↗
19. Andersen · ACS Appl. Mater. Interfaces · 2014 · 6 · 1656510.1021/am5028956 ↗
20. Andersen · J. Power Sources · 2015 · 274 · 121710.1016/j.jpowsour.2014.10.162 ↗
21. Andersen · Solid State Ionics · 2013 · 231 · 9410.1016/j.ssi.2012.11.020 ↗
22. Jao · Int. J. Hydrogen Energy · 2012 · 37 · 1362310.1016/j.ijhydene.2012.02.035 ↗
23. Sugawara · J. Electrochem. Soc. · 2012 · 159 · F77910.1149/2.017212jes ↗
24. Imai · J. Am. Chem. Soc. · 2009 · 131 · 629310.1021/ja810036h ↗
25. Gu · J. Phys. Chem. C · 2007 · 111 · 1738810.1021/jp074948s ↗
26. Maiyalagan · J. Mater. Chem. · 2012 · 22 · 528610.1039/c2jm16541d ↗
27. Jang · J. Electrochem. Sci. Technol. · 2011 · 2 · 13110.33961/JECST.2011.2.3.131 ↗
28. Jo · Polym. Degrad. Stab. · 2012 · 97 · 101010.1016/j.polymdegradstab.2012.03.016 ↗
29. Parry · J. Power Sources · 2011 · 196 · 253010.1016/j.jpowsour.2010.11.027 ↗
30. Chen · J. Power Sources · 2007 · 169 · 28810.1016/j.jpowsour.2007.03.037 ↗
31. Zhang · Electrochim. Acta · 2009 · 54 · 402510.1016/j.electacta.2009.02.028 ↗
32. Briggs · 1992 · 234
33. Chuang · J. Vac. Sci. Technol. · 1983 · A1 · 123610.1116/1.572293 ↗
34. Schulze · Fresenius J. Anal. Chem. · 1999 · 365 · 10610.1007/s002160051454 ↗