Abstract

Nowadays, the operating temperature of polymer electrolyte membrane fuel cell stacks is typically limited to 80 °C due to water management issues of membrane materials. In the present work, short-term operation at elevated temperatures up to 120 °C and long-term steady-state operation under automotive relevant conditions at 80 °C are examined using a 30-cell stack developed at DLR. The high temperature behavior is investigated by using temperature cycles between 90 and 120 °C without adjustment of the gases dew points, to simulate a short-period temperature increase, possibly caused by an extended power demand and/or limited heat removal. This galvanostatic test demonstrates a fully reversible performance decrease of 21 ± 1% during each thermal cycle. The irreversible degradation rate is about a factor of 6 higher compared to the one determined by the long-term test. The 1200-h test at 80 °C demonstrates linear stack voltage decay with acceptable degradation rate, apart from a malfunction of the air compressor, which results in increased catalyst degradation effects on individual cells. This interpretation is based on an end-of-life characterization, aimed to investigate catalyst, electrode and membrane degradation, by determining hydrogen crossover rates, high frequency resistances, electrochemically active surface areas and catalyst particle sizes.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advanced battery technologies research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. A review of polymer electrolyte membrane fuel cell durability test protocols10.1016/j.jpowsour.2011.07.082 ↗
2. A review of PEM fuel cell durability: degradation mechanisms and mitigation strategies10.1016/j.jpowsour.2008.06.006 ↗
3. Experimental comparison between external and internal humidification in proton exchange membrane fuel cells for road vehicles10.1016/j.ijhydene.2015.03.012 ↗
4. A review on water balance in the membrane electrode assembly of proton exchange membrane fuel cells10.1016/j.ijhydene.2009.09.017 ↗
5. Degradation aspects of water formation and transport in proton exchange membrane fuel cell: a review10.1016/j.jpowsour.2013.04.044 ↗
6. Role of the glass transition temperature of nafion 117 membrane in the preparation of the membrane electrode assembly in a direct methanol fuel cell (DMFC)10.1016/j.ijhydene.2012.05.121 ↗
7. Investigation of locally resolved current density distribution of segmented PEM fuel cells to detect malfunctions10.1149/1.3428993 ↗
8. Validation of an externally oil-cooled 1 kWel HT-PEMFC stack operating at various experimental conditions10.1016/j.ijhydene.2013.05.174 ↗
9. Thermal management strategies for a 1 kWe stack of a high temperature proton exchange membrane fuel cell10.1016/j.applthermaleng.2012.04.041 ↗
10. Influence of the phosphoric acid-doping level in a polybenzimidazole membrane on the cell performance of high-temperature proton exchange membrane fuel cells10.1016/j.jpowsour.2008.12.115 ↗
11. Proton conductivity of phosphoric acid doped polybenzimidazole and its composites with inorganic proton conductors10.1016/j.memsci.2003.09.002 ↗
12. Experimental study of water transport in a polybenzimidazole-based high temperature PEMFC10.1016/j.ijhydene.2011.09.159 ↗
13. Effects of temperature and humidity on the cell performance and resistance of a phosphoric acid doped polybenzimidazole fuel cell10.1016/j.jpowsour.2010.05.057 ↗
14. High temperature (HT) polymer electrolyte membrane fuel cells (PEMFC) – A review10.1016/j.jpowsour.2012.11.126 ↗
15. Situ PEM fuel cell electrochemical surface area and catalyst utilization measurement
16. Diagnostic tools in PEM fuel cell research: part I electrochemical techniques10.1016/j.ijhydene.2008.01.013 ↗
17. Determination of the electrochemically active surface area of Pt/C PEM fuel cell electrodes using different adsorbates
18. Electrochemical impedance study of electrode-membrane assemblies in PEM fuel cells10.1149/1.1392588 ↗
19. Preparation and characterization of highly dispersed electrocatalytic materials
20. Electrocatalytic oxidation of methanol on platinum nanoparticles electrodeposited onto porous carbon substrates10.1023/A:1018434609543 ↗
21. Fuel cell membrane characterizations10.1080/15583724.2015.1011275 ↗
22. Effect of metal oxides as co-catalysts for the electro-oxidation of methanol on platinum-ruthenium10.1016/S0378-7753(99)00321-3 ↗
23. Catalytic activity vs. size correlation in platinum catalysts of PEM fuel cells prepared on carbon black by different methods10.1016/j.ijhydene.2009.07.073 ↗
24. Review: durability and degradation issues of PEM fuel cell components10.1002/fuce.200700053 ↗
25. Aspects of the chemical degradation of PFSA ionomers used in PEM fuel cells10.1002/fuce.200400050 ↗
26. In situ EPR investigation of polymer electrolyte membrane degradation in fuel cell applications10.1016/j.jpowsour.2003.09.047 ↗
27. Diagnosis of MEA degradation under accelerated relative humidity cycling10.1016/j.jpowsour.2011.01.088 ↗
28. Influence of ageing in fuel cell on membrane/electrodes interfaces10.1016/j.jpowsour.2010.12.014 ↗
29. Quantitative characterization of catalyst layer degradation in PEM fuel cells by X-ray photoelectron spectroscopy10.1016/j.electacta.2009.02.028 ↗
30. Membrane electrode assembly degradation under idle conditions via unsymmetrical reactant relative humidity cycling10.1016/j.jpowsour.2012.01.133 ↗
31. Degradation mechanisms of Pt/C fuel cell catalysts under simulated start-stop conditions10.1021/cs300024h ↗
32. Analysis of electrocatalyst degradation in PEMFC caused by cell reversal during fuel starvation10.1016/j.jpowsour.2003.12.035 ↗
33. Analysis of degradation in PEMFC caused by cell reversal during air starvation10.1016/j.ijhydene.2008.02.049 ↗
34. Degradation of polymer electrolyte membranes10.1016/j.ijhydene.2006.05.006 ↗
35. Kinoshita · 1988
36. Characterization of vulcan electrochemically oxidized under simulated PEM fuel cell conditions10.1149/1.1649756 ↗
37. Electrocatalytic corrosion of carbon support in PEMFC cathodes10.1149/1.1630412 ↗
38. Thermal and electrochemical durability of carbonaceous composites used as a bipolar plate of proton exchange membrane fuel cell10.1016/j.jpowsour.2010.04.045 ↗
39. XPS analysis of the degradation of nafion10.1007/s002160051454 ↗
40. Durability of PEFCs at high humidity conditions10.1149/1.1830355 ↗
41. Two fuel cell cars in every garage?10.1149/2.F05053IF ↗