journal article·2013-06

La0.8Sr1.2CoO4+δ–CGO composite as cathode on La0.9Sr0.1Ga0.8Mg0.2O3−δ electrolyte for intermediate temperature solid oxide fuel cells

Jun Zhou, Gang Chen, Kai Wu, Yonghong Cheng

Publisher page

Abstract

Abstract La 0.8 Sr 1.2 CoO 4+ δ (LSCO4) material with K 2 NiF 4 -type structure has been synthesized via a citric–nitrate process and characterized. Composite materials La 0.8 Sr 1.2 CoO 4+ δ -Ce 0.9 Gd 0.1 O 2− δ (CGO) (LSCO4–CGO) have been prepared and evaluated as cathode for intermediate temperature SOFC (IT-SOFC) based on La 0.9 Sr 0.1 Ga 0.8 Mg 0.2 O 3− δ (LSGM) electrolytes. LSCO4 oxide is chemically compatible with CGO and LSGM electrolyte at temperature up to 1000 °C. Compared with the pure LSCO4, the optimum composition of LSCO4–35 wt % CGO exhibits better electrochemical activity for oxygen reduction. Also, for LSCO4–35 wt % CGO electrode, SEM results suggest that better microstructure is obtained and the electrode forms good contact with the electrolyte after sintering at 1000 °C for 2 h. At 750 °C, the polarization resistance of the LSCO4–35 wt % CGO composite cathode is about 0.21 Ω cm 2 in air. A cell with a 1.2 mm thick LSGM electrolyte, NiO as anode, and LSCO4-35 wt % CGO as cathode displays a maximum power density of 515 mW cm −2 at 750 °C. These results indicate that LSCO4–CGO composite materials are promising cathode candidates for intermediate-temperature solid oxide fuel cells with LSGM electrolyte.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Brandon · Rev. Mater. Sci. · 2003 · 33 · 18310.1146/annurev.matsci.33.022802.094122 ↗
2. Xia · Adv. Mater. · 2002 · 14 · 52110.1002/1521-4095(20020404)14:7<521::AID-ADMA521>3.0.CO;2-C ↗
3. Park · Nature (London) · 2000 · 404 · 26510.1038/35005040 ↗
4. Aguadero · Solid State Ionics · 2008 · 179 · 39310.1016/j.ssi.2008.01.099 ↗
5. Li · Electrochem. Commun. · 2007 · 9 · 150810.1016/j.elecom.2007.02.013 ↗
6. Zhao · Solid State Ionics · 2008 · 179 · 145010.1016/j.ssi.2007.11.033 ↗
7. Huang · Int. J. Hydrogen Energy · 2010 · 35 · 265710.1016/j.ijhydene.2009.04.022 ↗
8. Wang · J. Power Sources · 2011 · 196 · 310410.1016/j.jpowsour.2010.11.106 ↗
9. Jin · J. Power Sources · 2008 · 182 · 48210.1016/j.jpowsour.2008.04.044 ↗
10. Bassat · Solid State Ionics · 2004 · 167 · 34110.1016/j.ssi.2003.12.012 ↗
11. Jennings · Solid State Ionics · 2000 · 152–153 · 663
12. Omata · Solid State Commun. · 1993 · 88 · 80710.1016/0038-1098(93)90882-N ↗
13. Vashook · Solid State Ionics · 1998 · 110 · 24510.1016/S0167-2738(98)00134-9 ↗
14. Ishikawa · Bull. Chem. Soc. Jpn. · 1987 · 60 · 129510.1246/bcsj.60.1295 ↗
15. Cao · Int. J. Hydrogen Energy · 2010 · 35 · 559410.1016/j.ijhydene.2010.03.046 ↗
16. Yin · J. Power Sources · 2011 · 196 · 623810.1016/j.jpowsour.2011.03.019 ↗
17. Kharton · J. Power Sources · 2004 · 177 · 26
18. Shimura · Solid State Ionics · 1997 · 104 · 7910.1016/S0167-2738(97)00394-9 ↗
19. Tarancon · J. Mater. Chem. · 2010 · 20 · 379910.1039/b922430k ↗
20. Skinner · Solid State Ionics · 2000 · 135 · 70910.1016/S0167-2738(00)00388-X ↗
21. Daroukh · Solid State Ionics · 2003 · 158 · 14110.1016/S0167-2738(02)00773-7 ↗
22. Hernández · Int. J. Hydrogen Energy · 2011 · 36 · 1570410.1016/j.ijhydene.2011.08.105 ↗
23. Wang · Mater. Lett. · 2006 · 60 · 117410.1016/j.matlet.2005.10.104 ↗
24. Boehm · Solid State Sci. · 2003 · 5 · 97310.1016/S1293-2558(03)00091-8 ↗
25. Boehm · Solid State Ionics · 2005 · 176 · 271710.1016/j.ssi.2005.06.033 ↗
26. Chroneos · J. Mater. Chem. · 2010 · 20 · 26610.1039/B917118E ↗
27. Lalanne · 2004 · 1351
28. Pérez-Coll · Fuel Cells · 2011 · 11 · 9110.1002/fuce.201000066 ↗
29. Nie · Solid State Ionics · 2006 · 177 · 192910.1016/j.ssi.2006.01.003 ↗
30. Munnings · Solid State Ionics · 2005 · 176 · 189510.1016/j.ssi.2005.06.002 ↗
31. Tealdi · Phys. Rev. B · 2010 · 82 · 17411810.1103/PhysRevB.82.174118 ↗
32. Jin · J. Alloys Compd. · 2009 · 474 · 57310.1016/j.jallcom.2008.07.002 ↗
33. Peng · J. Power Sources · 2012 · 201 · 17410.1016/j.jpowsour.2011.10.121 ↗
34. Zhou · Appl. Surf. Sci. · 2012 · 258 · 313310.1016/j.apsusc.2011.11.050 ↗
35. Steele · J. Solid State Ionics · 2000 · 129 · 9510.1016/S0167-2738(99)00319-7 ↗
36. Vashook · Solid State Ionics · 2006 · 177 · 182710.1016/j.ssi.2006.04.040 ↗
37. Fu · Electrochim. Acta · 2007 · 52 · 458910.1016/j.electacta.2007.01.001 ↗
38. Adler · Solid State Ionics · 1998 · 111 · 12510.1016/S0167-2738(98)00179-9 ↗
39. Adler · J. Electrochem. Soc. · 1996 · 143 · 355410.1149/1.1837252 ↗
40. Li · J. Alloys Compd. · 2008 · 448 · 11610.1016/j.jallcom.2006.10.032 ↗
41. Barbucci · Appl. Electrochem. · 2005 · 35 · 39910.1007/s10800-005-0791-z ↗
42. Kim · J. Mater. Chem. · 2007 · 17 · 250010.1039/b618345j ↗
43. Steele · Solid State Ionics · 1995 · 75 · 15710.1016/0167-2738(94)00182-R ↗
44. Wei · Electrochem. Solid-State Lett. · 2005 · 8 · A42810.1149/1.1951232 ↗