Physical and electrochemical characterization of Bi2O3-doped scandia stabilized zirconia
Source abstract
Abstract
Abstract Electrolytes based on Sc 2 O 3 –ZrO 2 exhibit the highest ionic conductivity of zirconia based systems, however, stabilization of the electrochemical properties at operational temperatures, 600–1000 °C, are needed before implementation into SOFCs. Trace additions of Bi 2 O 3 are a known sintering aid for zirconia systems. Crystal structures, electrical properties and long-term stability of Bi 2 O 3 -doped 10ScSZ systems were investigated. The addition of more than 1.0 mol% Bi 2 O 3 resulted in suppression of the rhombohedral to cubic phase transformation at 600 °C and cubic phase stabilization at room temperature. The ionic conductivity of 10ScSZ was also improved by Bi 2 O 3 additions. A maximum conductivity of 0.034 S cm −1 at 700 °C was observed in 2 mol% Bi 2 O 3 -doped 10ScSZ sintered at 1300 °C. No phase change was observed in 10ScSZ after annealing at 1000 °C. A certain amount of monoclinic phase, and dramatic conductivity decrease, were observed in Bi 2 O 3 -doped samples sintered below 1200 °C after annealing. However, 10ScSZ and 2 mol% Bi 2 O 3 -doped 10ScSZ sintered at 1300 °C show no significant conductivity degradation with annealing. Samples with more than 1 mol% Bi 2 O 3 and sintered above 1300 °C resulted in good ionic conductivity and stability.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Catalysis and Oxidation Reactions
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Politova · Solid State Ionics · 2004 · 168 · 15310.1016/j.ssi.2004.02.007 ↗
2. Badwal · Solid State Ionics · 2000 · 136/137 · 9110.1016/S0167-2738(00)00356-8 ↗
3. Lei · Solid State Ionics · 2005 · 176 · 279110.1016/j.ssi.2005.09.005 ↗
4. Yamamoto · Electrochim. Acta · 2000 · 45 · 242310.1016/S0013-4686(00)00330-3 ↗
5. Fergus · J. Power Sources · 2006 · 162 · 3010.1016/j.jpowsour.2006.06.062 ↗
6. Yamamoto · Solid State Ionics: New Dev. · 1996 · 221
7. Yamamoto · Solid State Ionics · 1995 · 79 · 13710.1016/0167-2738(95)00044-7 ↗
8. Tietz · Solid State Ionics · 1997 · 100 · 28910.1016/S0167-2738(97)00356-1 ↗
9. Hirano · Solid State Ionics · 2003 · 158 · 21510.1016/S0167-2738(02)00912-8 ↗
10. Sarat · J. Power Sources · 2006 · 160 · 89210.1016/j.jpowsour.2006.02.007 ↗
11. Bai · 2006
12. Wang · Mater. Lett. · 2005 · 59 · 257910.1016/j.matlet.2004.07.065 ↗
13. Bai · 2007 · vol. 7
14. Haering · Solid State Ionics · 2005 · 176 · 26110.1016/j.ssi.2004.07.039 ↗
15. Kosacki · Solid State Ionics · 2002 · 152/153 · 43110.1016/S0167-2738(02)00382-X ↗