Embrittlement induced fracture behavior and mechanisms of perfluorosulfonic-acid membranes after chemical degradation
Source abstract
Abstract
Abstract Chemical and mechanical degradations of perfluorosulfonic-acid membranes are two factors contributing to the reduced durability of fuel cells. While the mechanisms of isolated chemical or mechanical degradation are extensively investigated, the impact of chemical degradation on mechanical degradation is not fully understood. In this paper, the fracture behavior of Nafion 212 membranes with different chemical degradation levels are investigated. To characterize the degradation level and probe the molecular origins of chemical degradation, fluoride release, Fourier-transformer infrared spectra, conductivity and swelling behavior are measured. It is found that chemical degradation causes predominant loss of side-chains. A transition from ductile to brittle fracture is observed with increasing degradation level. In addition, the cross-sections are examined to link fracture behavior with microstructure changes. While the decreased fracture toughness is attributed to reduced mechanical properties such as Young's modulus and break strain, the decreased crack propagation resistance is ascribed to reduced plastic zone size ahead of crack tip, which reduces the plastic energy dissipation. These findings not only provide new mechanical dataset of degraded membranes for performance and durability modelling to take into account of chemical degradation effect but also improve the understanding of membrane durability.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fuel Cells and Related Materials · Advanced Battery Technologies Research · Membrane-based Ion Separation Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. New insights into perfluorinated sulfonic-acid ionomers10.1021/acs.chemrev.6b00159 ↗
2. Effect of perfluorosulfonic acid membrane equivalent weight on degradation under accelerated stress conditions10.1016/j.electacta.2013.03.112 ↗
3. Degradation of a PEM fuel cell stack with Nafion® membranes of different thicknesses. Part II: ex situ diagnosis10.1016/j.jpowsour.2012.01.074 ↗
4. Degradation of a polymer exchange membrane fuel cell stack with Nafion® membranes of different thicknesses: Part I. In situ diagnosis10.1016/j.jpowsour.2010.06.023 ↗
5. Membrane durability: physical and chemical degradation
6. 3D visualization of membrane failures in fuel cells10.1016/j.jpowsour.2017.01.129 ↗
7. Tracking the evolution of mechanical degradation in fuel cell membranes using 4D in situ visualization10.1016/j.jpowsour.2018.11.049 ↗
8. Interplay between temperature and biaxial loading on creep behavior of perfluorosulfonic-acid membranes10.1016/j.jpowsour.2019.227309 ↗
9. Electrochemical/mechanical coupling in ion-conducting soft matter10.1021/acs.jpclett.5b01639 ↗
10. Advanced materials for improved PEMFC performance and life10.1016/j.jpowsour.2004.01.023 ↗
11. The chemistry of fuel cell membrane chemical degradation10.1149/1.2981859 ↗
12. Scientific aspects of polymer electrolyte fuel cell durability and degradation10.1021/cr050182l ↗
13. Current understanding of chemical degradation mechanisms of perfluorosulfonic acid membranes and their mitigation strategies: a review
14. Viscoelastic response of nafion. Effects of temperature and hydration on tensile creep10.1021/ma801811m ↗
15. Fatigue and creep to leak tests of proton exchange membranes using pressure-loaded blisters10.1016/j.jpowsour.2009.06.083 ↗
16. Biaxial fatigue crack propagation behavior of perfluorosulfonic-acid membranes10.1016/j.jpowsour.2018.02.002 ↗
17. Exploring the role of reinforcement in controlling fatigue crack propagation behavior of perfluorosulfonic-acid membranes10.1016/j.ijhydene.2018.02.034 ↗
18. Ex situ characterization and modelling of fatigue crack propagation in catalyst coated membrane composites for fuel cell applications10.1016/j.ijhydene.2019.03.108 ↗
19. Ex situ measurement and modelling of crack propagation in fuel cell membranes under mechanical fatigue loading10.1016/j.ijhydene.2017.06.151 ↗
20. Estimation of crack propagation in polymer electrolyte membrane fuel cell under vibration conditions10.1016/j.ijhydene.2017.02.119 ↗
21. A review of accelerated stress tests of MEA durability in PEM fuel cells10.1016/j.ijhydene.2008.10.012 ↗
22. Fuel cell perfluorinated sulfonic acid membrane degradation correlating accelerated stress testing and lifetime10.1021/cr200424d ↗
23. Membrane accelerated stress test development for polymer electrolyte fuel cell durability validated using field and drive cycle testing10.1149/2.0101806jes ↗
24. Accelerated stress test procedures for PEM fuel cells under actual load constraints: state-of-art and proposals10.1016/j.ijhydene.2015.07.026 ↗
25. Acceleration of chemical degradation of perfluorosulfonic acid ionomer membrane by mechanical stress: experimental evidence10.1149/1.3484584 ↗
26. Effect of mechanical compression on chemical degradation of nafion membranes10.1149/2.008405eel ↗
27. Mechanical endurance of polymer electrolyte membrane and PEM fuel cell durability10.1002/polb.20863 ↗
28. Decay in mechanical properties of catalyst coated membranes subjected to combined chemical and mechanical membrane degradation10.1002/fuce.201400040 ↗
29. Accelerated membrane durability testing of heavy duty fuel cells10.1149/2.0671501jes ↗
30. Membrane degradation during combined chemical and mechanical accelerated stress testing of polymer electrolyte fuel cells10.1016/j.jpowsour.2014.01.106 ↗
31. Deterioration of mechanical properties: a cause for fuel cell membrane failure10.1016/j.memsci.2010.02.060 ↗
32. Mechanical response of fuel cell membranes subjected to a hygro-thermal cycle10.1016/j.jpowsour.2006.05.020 ↗
33. Effect of mechanical vibrations on damage propagation in polymer electrolyte membrane fuel cells10.1016/j.ijhydene.2013.08.136 ↗
34. Model-based analysis of PFSA membrane mechanical response to relative humidity and load cycling in PEM fuel cells10.1149/2.0371806jes ↗
35. Modeling coupled durability and performance in polymer-electrolyte fuel cells: membrane effects10.1149/2.0281907jes ↗
36. Structure/property relationship of Nafion XL composite membranes10.1016/j.memsci.2016.06.004 ↗
37. Impact of hygrothermal aging on structure/function relationship of perfluorosulfonic-acid membrane10.1002/polb.23946 ↗
38. Structure-transport relationship of perfluorosulfonic-acid membranes in different cationic forms10.1016/j.electacta.2016.10.096 ↗
39. Application of the essential work of fracture (EWF) concept for polymers, related blends and composites: a review10.1016/j.progpolymsci.2010.07.001 ↗
40. In-plane biaxial cyclic mechanical behavior of proton exchange membranes10.1016/j.jpowsour.2017.06.040 ↗
41. Fracture property of Nafion XL composite membrane determined by R-curve method10.1016/j.jpowsour.2018.07.052 ↗
42. Effect of pretreatment on microstructure and mechanical properties of Nafion™ XL composite membrane10.1002/fuce.201900064 ↗
43. A degradation study of Nafion proton exchange membrane of PEM fuel cells10.1016/j.jpowsour.2007.03.061 ↗
44. Cerium migration during PEM fuel cell accelerated stress testing10.1149/2.0181609jes ↗
45. Local impact of humidification on degradation in polymer electrolyte fuel cells10.1016/j.jpowsour.2017.03.057 ↗
46. Impact of heat and water management on proton exchange membrane fuel cells degradation in automotive application10.1016/j.jpowsour.2016.07.004 ↗
47. Perfluorosulfonic acid membrane degradation in the hydrogen inlet region: a macroscopic approach10.1016/j.ijhydene.2015.10.066 ↗
48. FT-IR study of the microstructure of Nafion® membrane10.1016/j.memsci.2003.12.008 ↗
49. Effect of H2O2 on Nafion® properties and conductivity at fuel cell conditions10.1016/j.jpowsour.2010.11.133 ↗
50. Towards a NMR-based method for characterizing the degradation of nafion XL membranes for PEMFC10.1149/2.0231806jes ↗
51. Degradation of perfluorinated ionomer membranes for PEM fuel cells during processing with H2O210.1149/1.2186768 ↗
52. A performance and degradation study of Nafion 212 membrane for proton exchange membrane fuel cells10.1016/j.jpowsour.2009.04.038 ↗
53. Durability of perfluorinated ionomer membrane against hydrogen peroxide10.1016/j.jpowsour.2005.10.043 ↗
54. Ex situ investigation of the proton exchange membrane chemical decomposition10.1016/j.ijhydene.2008.01.052 ↗
55. Degradation mechanism study of perfluorinated proton exchange membrane under fuel cell operating conditions10.1016/j.electacta.2007.11.010 ↗
56. Chemical durability studies of perfluorinated sulfonic acid polymers and model compounds under mimic fuel cell conditions10.1021/ma071603z ↗
57. Progression in the morphology of fuel cell membranes upon conjoint chemical and mechanical degradation10.1149/2.0671607jes ↗
58. About the interactions controlling nafion's viscoelastic properties and morphology10.1021/acs.macromol.5b01559 ↗
59. An experimental investigation of humidity and temperature effects on the mechanical properties of perfluorosulfonic acid membrane10.1016/j.msea.2006.03.055 ↗
60. An experimental investigation of strain rate, temperature and humidity effects on the mechanical behavior of a perfluorosulfonic acid membrane10.1016/j.jpowsour.2012.04.094 ↗
61. Orientation of drawn Nafion at molecular and mesoscopic scales10.1021/ma035642w ↗
62. Understanding the formation of pinholes in PFSA membranes with the essential work of fracture (EWF)10.1016/j.ijhydene.2013.03.031 ↗
63. Research on the long-term stability of a PEMFC stack: analysis of pinhole evolution10.1016/j.ijhydene.2014.03.072 ↗