Mn in misch-metal based superlattice metal hydride alloy – Part 2 Ni/MH battery performance and failure mechanism

K. Young, J. Koch, S. Yasuoka, H. Shen, L.A. Bendersky

Publisher page

Abstract

Abstract The performance and failure mode of Ni/MH batteries made from a series of Mn-modified A 2 B 7 superlattice and a commercially available AB 5 metal hydride alloys were studied and reported. Cells with the Mn-free A 2 B 7 alloy generally show improved low-temperature, higher peak power, and similar charge-retention behavior over those with a conventional AB 5 alloy. As Mn-additive amount increased, cell voltage and high-rate capacity improved, low temperature, charge retention, and cycle life first improved, but then deteriorated, and peak power and high temperature voltage stand deteriorated. Analysis of battery performance test results show the use of a superlattice alloy containing 2.3% Mn as the best overall alloy composition. Failure analysis of the highly cycled AB 5 alloy containing cells indicate a balanced degradation in negative, positive, separator, and a moderate loss of electrolyte. Same analysis on cells containing the various superlattice alloys suffered from a high degree of pulverization and oxidation of its negative electrode (with the 9.3% Mn content experiencing the worst amount of pulverization/oxidation) and a high degree of electrolyte loss.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen Storage and Materials · Fuel Cells and Related Materials · Magnesium Alloys: Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Yasuoka · J. Power Sources · 2006 · 156 · 66210.1016/j.jpowsour.2005.05.054 ↗
2. Yasuoka · Rare Earths · 2006 · 48 · 112
3. H. Teraoka, Development of Low Self-discharge Nickel-metal Hydride Battery. Available online: http://www.scribd.com/doc/9704685/Teraoka-Article-En.
4. Young · Materials · 2013 · 6 · 457410.3390/ma6104574 ↗
5. Young · Int. J. Hydrog. Energy · 2012 · 37 · 988210.1016/j.ijhydene.2012.03.117 ↗
6. Zhou · J. Alloys Compd. · 2013 · 580 · S37310.1016/j.jallcom.2013.03.014 ↗
7. Young · J. Power Sources. · 2015 · 277 · 42610.1016/j.jpowsour.2014.10.093 ↗
8. Young · J. Alloys Compd. · 2013 · 580 · S17110.1016/j.jallcom.2013.02.087 ↗
9. Young · J. Alloys Compd. · 2013 · 560 · 3310.1016/j.jallcom.2013.01.146 ↗
10. M.A. Fetcenko, S.R. Ovshinsky, K. Young, B. Reichman, T. Ouchi, J. Koch, W. Mays, U.S. Patent 6,830,725 B2 (2004).
11. M.A. Fetcenko, K. Young, S.R. Ovshinsky, T. Ouchi, U.S. Patent 7,393,500 B2 (2008).
12. Young · J. Alloys Compd. · 2011 · 509 · 399510.1016/j.jallcom.2010.12.205 ↗
13. Young · J. Alloys Compd. · 2011 · 509 · 761110.1016/j.jallcom.2011.04.102 ↗
14. Kong · J. Power Sources · 2012 · 213 · 12810.1016/j.jpowsour.2012.03.099 ↗
15. Shinyama · J. Power Sources · 2005 · 143 · 26510.1016/j.jpowsour.2004.11.051 ↗
16. Young · J. Alloys Compd. · 2012 · 543 · 9010.1016/j.jallcom.2012.07.125 ↗
17. Young · J. Power Sources · 2011 · 196 · 881510.1016/j.jpowsour.2011.06.010 ↗
18. Young · Int. J. Hydrog. Energy · 2011 · 36 · 354710.1016/j.ijhydene.2010.12.051 ↗
19. Young · Int. J. Hydrog. Energy · 2011 · 36 · 1229610.1016/j.ijhydene.2011.06.117 ↗
20. Young · J. Alloys Compd. · 2012 · 510 · 9710.1016/j.jallcom.2011.08.091 ↗
21. Young · J. Alloys Compd. · 2010 · 506 · 83110.1016/j.jallcom.2010.07.086 ↗
22. Young · J. Alloys Compd. · 2014 · 606 · 9710.1016/j.jallcom.2014.04.033 ↗
23. Schlapbach · J. Less Comm. Met. · 1980 · 73 · 14510.1016/0022-5088(80)90354-9 ↗
24. Schlapbach · Surf. Sci. · 1981 · 106 · 15710.1016/0039-6028(81)90194-1 ↗
25. Liu · J. Appl. Electrochem. · 1999 · 29 · 85510.1023/A:1003537900947 ↗
26. Liu · Int. J. Hydrog. Energy · 2004 · 29 · 45310.1016/S0360-3199(02)00058-7 ↗