journal article·2014-03

Long-term evaluation of solid oxide fuel cell candidate materials in a 3-cell generic short stack fixture, Part II: Sealing glass stability, microstructure and interfacial reactions

Yeong-Shyung Chou, Jeffry W. Stevenson, Jung-Pyung Choi

Publisher page

Abstract

Abstract A generic solid oxide fuel cell stack test fixture was developed to evaluate candidate materials and processing methods under realistic conditions. Part II of the work examined the sealing glass stability, microstructure development, interfacial reaction, and volatility issues of a 3-cell stack with LSM-based cells. After 6000 h of testing, the refractory sealing glass YSO7 showed desirable chemical compatibility with YSZ electrolyte in that no discernable interfacial reaction was identified. In addition, no glass penetration into the thin electrolyte was observed. At the aluminized AISI441 interface, the protective alumina coating appeared to be corroded by the sealing glass. Air side interactions appeared to be more severe than fuel side interactions. Metal species such as Cr, Mn, and Fe were detected in the glass, but were limited to the vicinity of the interface. No alkaline earth chromates were found at the air side. Volatility was also studied in a similar glass and weight loss in a wet reducing environment was determined. Using the steady-state volatility data, the life time weight loss of refractory sealing glass YSO77 was estimated to be less than 0.1 wt%.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Chemical Looping and Thermochemical Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Minh · J. Am. Ceram. Soc. · 1993 · 76 · 56310.1111/j.1151-2916.1993.tb03645.x ↗
2. Steele · J. Mater. Sci. · 2001 · 36 · 105310.1023/A:1004853019349 ↗
3. Singhal · 1999 · vol. 99-19 · 39
4. Bolden · 1999 · vol. 99-19 · 80
5. Khandkar · 1999 · vol. 99-19 · 88
6. Meinhardt · J. Power Sources · 2008 · 182 · 18810.1016/j.jpowsour.2008.03.079 ↗
7. Chou · J. Power Sources · 2011 · 196 · 270910.1016/j.jpowsour.2010.11.020 ↗
8. Chou · J. Electrochem. Soc. · 2007 · 154 · B64410.1149/1.2733868 ↗
9. Yang · J. Electrochem. Soc. · 2003 · 150 · A109510.1149/1.1590325 ↗
10. Chou · J. Power Sources · 2008 · 185 · 100110.1016/j.jpowsour.2008.09.004 ↗
11. Simner · J. Electrochem. Soc. · 2005 · 152 · A74010.1149/1.1864332 ↗
12. Yokokawa · Solid State Ionics · 2006 · 177 · 319310.1016/j.ssi.2006.07.055 ↗
13. Taniguchi · J. Power Sources · 1995 · 55 · 7310.1016/0378-7753(94)02172-Y ↗
14. Zhen · J. Power Sources · 2007 · 170 · 6110.1016/j.jpowsour.2007.03.079 ↗
15. Fujita · J. Power Sources · 2004 · 131 · 26110.1016/j.jpowsour.2003.12.051 ↗
16. Komatsu · J. Power Sources · 2008 · 176 · 13210.1016/j.jpowsour.2007.10.068 ↗
17. Yang · Electrochem. Solid State Lett. · 2008 · 11 · B14010.1149/1.2929066 ↗
18. Choi · Int. J. Hydrogen Energy · 2011 · 36 · 454910.1016/j.ijhydene.2010.04.110 ↗
19. Chou · J. Power Sources · 2013
20. Zhang · J. Power Sources · 2012 · 205 · 30110.1016/j.jpowsour.2012.01.043 ↗
21. Greig · Am. J. Sci. · 1927 · 13 · 19
22. Phillips · J. Am. Ceram. Soc. · 1959 · 42 · 41210.1111/j.1151-2916.1959.tb12966.x ↗
23. Opila · J. Met. · 2011 · 58 · 22
24. Jacobson · J. Phys. Chem. Solid · 2005 · 66 · 47110.1016/j.jpcs.2004.06.044 ↗
25. Zhang · J. Am. Ceram. Soc. · 2008 · 91 · 256410.1111/j.1551-2916.2008.02479.x ↗