Abstract Sodium metal chloride batteries, also called as ZEBRA batteries, possess many merits such as low cost, high energy density and high safety, but their high operation temperature (270–350 °C) may cause several issues and limit their applications. Therefore, decreasing the operation temperature is of great importance in order to broaden their usage. Using a room temperature ionic liquid (RTIL) catholyte composed of sodium chloride buffered 1-ethyl-3-methylimidazolium chloride–aluminum chloride and a dense β″-aluminates solid electrolyte film with 500 micron thickness, we report an intermediate temperature sodium copper chloride battery which can be operated at only 150 °C, therefore alleviating the corrosion issues, improving the material compatibilities and reducing the operating complexities associated with the conventional ZEBRA batteries. The RTIL presents a high ionic conductivity (0.247 S cm−1) at 150 °C and a wide electrochemical window (−2.6 to 2.18 vs. Al3+/Al). With the discharge plateau at 2.64 V toward sodium and the specific capacity of 285 mAh g−1, this intermediate temperature battery exhibits an energy density (750 mWh g−1) comparable to the conventional ZEBRA batteries (728–785 mWh g−1) and superior to commercialized Li-ion batteries (550–680 mWh g−1), making it very attractive for renewable energy integration and other grid related applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Thermal Expansion and Ionic Conductivity · Inorganic Fluorides and Related Compounds
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Wang · Angew. Chem. Int. Ed. · 2013 · 52 · 196410.1002/anie.201206854 ↗
2. Wen · Solid State Ionics · 2008 · 179 · 169710.1016/j.ssi.2008.01.070 ↗
3. Gerovasili · J. Power Sources · 2014 · 251 · 13710.1016/j.jpowsour.2013.11.046 ↗
4. Lu · Energy Environ. Sci. · 2013 · 6 · 183710.1039/c3ee24244g ↗
5. Coetzer · J. Power Sources · 1986 · 18 · 37710.1016/0378-7753(86)80093-3 ↗
6. Sudworth · J. Power Sources · 1994 · 51 · 10510.1016/0378-7753(94)01967-3 ↗
7. Cleaver · J. Appl. Electrochem. · 1995 · 25 · 112810.1007/BF00242540 ↗
8. Prakash · J. Power Sources · 2000 · 87 · 19510.1016/S0378-7753(99)00473-5 ↗
9. Steinbock · J. Electrochem. Soc. · 2001 · 148 · A13210.1149/1.1341240 ↗
10. Dustmann · J. Power Sources · 2004 · 127 · 8510.1016/j.jpowsour.2003.09.039 ↗
11. Tilley · 2001
12. Hueso · Energy Environ. Sci. · 2013 · 6 · 73410.1039/c3ee24086j ↗
13. Lu · Energy Environ. Sci. · 2013 · 6 · 29910.1039/C2EE23606K ↗
14. Li · J. Power Sources · 2014 · 249 · 41410.1016/j.jpowsour.2013.10.110 ↗
15. Lu · ECS Trans. · 2010 · 28 · 710.1149/1.3492326 ↗
16. Lu · J. Power Sources · 2013 · 224 · 31210.1016/j.jpowsour.2012.09.108 ↗
17. Gray · J. Electrochem. Soc. · 1995 · 142 · 363610.1149/1.2048391 ↗
18. Gray · J. Electrochem. Soc. · 1996 · 143 · 382010.1149/1.1837301 ↗
19. Park · J. Electrochem. Soc. · 2001 · 148 · A134610.1149/1.1413479 ↗
20. Lang · Electrochim. Acta · 2006 · 51 · 388410.1016/j.electacta.2005.11.022 ↗
21. Yang · Ceram. Int. · 2014 · 40 · 905510.1016/j.ceramint.2014.01.118 ↗
22. Carlin · J. Appl. Electrochem. · 1996 · 26 · 114710.1007/BF00243740 ↗
23. Piersma · J. Electrochem. Soc. · 1996 · 143 · 90810.1149/1.1836557 ↗
24. Willkes · Inorg. Chem. · 1982 · 21 · 126310.1021/ic00133a078 ↗
25. Di · J. Power Sources · 1990 · 29 · 30110.1016/0378-7753(90)85005-W ↗
26. Pye · J. Electrochem. Soc. · 1997 · 144 · 193310.1149/1.1837724 ↗
27. Wu · J. Power Sources · 2000 · 88 · 23710.1016/S0378-7753(00)00372-4 ↗
28. Hu · J. Power Sources · 2012 · 219 · 110.1016/j.jpowsour.2012.07.025 ↗