Interactions of nickel/zirconia solid oxide fuel cell anodes with coal gas containing arsenic
Source abstract
Abstract
Abstract The performance of anode-supported and electrolyte-supported solid oxide fuel cells was investigated in synthetic coal gas containing 0–10 ppm arsenic at 700–800 °C. Arsenic was found to interact strongly with nickel, resulting in the formation of nickel–arsenic solid solution, Ni5As2 and Ni11As8, depending on temperature, arsenic concentration, and reaction time. For anode-supported cells, loss of electrical connectivity in the anode support was the principal mode of degradation, as nickel was converted to nickel arsenide phases that migrated to the surface to form large grains. Cell failure occurred well before the entire anode was converted to nickel arsenide, and followed a reciprocal square root of arsenic partial pressure dependence that is consistent with a diffusion-based rate-limiting step. Failure occurred more quickly with electrolyte-supported cells, which have a substantially smaller nickel inventory. For these cells, time to failure varied linearly with the reciprocal arsenic concentration. Failure occurred when arsenic reached the anode/electrolyte interface, though agglomeration of nickel reaction products may have also contributed. Test performed with nickel/zirconia coupons showed that arsenic was essentially completely captured in a narrow band near the fuel gas inlet. Arsenic concentrations of ∼10 ppb or less are estimated to result in acceptable rates of fuel cell degradation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal Extraction and Bioleaching · Advancements in Solid Oxide Fuel Cells · Chemical Looping and Thermochemical Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. U.S. Dept. of Energy Office of Fossil Energy, FutureGen: Integrated Hydrogen, Electric Power Production and Carbon Sequestration Research Initiative, March 2004.
2. Williams · Int. J. Appl. Ceram. Technol. · 2005 · 2 · 29510.1111/j.1744-7402.2005.02031.x ↗
3. Williams · J. Power Sources · 2005 · 143 · 19110.1016/j.jpowsour.2004.12.003 ↗
4. Williams · Solid State Ionics · 2006 · 177 · 203910.1016/j.ssi.2006.02.051 ↗
5. Trembly · J. Power Sources · 2007 · 163 · 98610.1016/j.jpowsour.2006.10.020 ↗
6. Cayan · J. Power Sources · 2008 · 185 · 59510.1016/j.jpowsour.2008.06.058 ↗
7. Benson · 1996
8. Pigeaud · 1994
9. Ridler · 1997 · 225
10. Ng · Appl. Catal. · 1991 · 70 · 21310.1016/S0166-9834(00)84165-2 ↗
11. Ng · Appl. Catal. A · 1998 · 171 · 29310.1016/S0926-860X(98)00097-0 ↗
12. Quinn · Appl. Catal. A · 2004 · 264 · 10310.1016/j.apcata.2003.12.034 ↗
13. Nielsen · Appl. Catal. · 1984 · 11 · 12310.1016/S0166-9834(00)84046-4 ↗
14. Trembly · J. Power Sources · 2007 · 171 · 81810.1016/j.jpowsour.2007.06.087 ↗
15. Marina · ECS Trans. · 2008 · 11 · 6310.1149/1.3038909 ↗
16. Marina · 2008
17. Krishnan · 2008
18. Lide · 1993
19. T.B. Massalski, Binary Alloy Phase Diagrams, 2nd ed. with Updates, H. Okamoto, editor, ASM International, National Institute of Science and Technology, Materials Park, Ohio, 44073, 1996.
20. El-Boragy · Zeitschrift Fur Metallkunde · 1983 · 74 · 545
21. Heyding · Chemistry-Revue Canadienne De Chimie · 1957 · 35 · 120510.1139/v57-161 ↗
22. Kjekshus · Acta Chem. Scand. · 1973 · 27 · 58210.3891/acta.chem.scand.27-0582 ↗
23. A. Roine, HSC Chemistry 6, version 6.12, Outokumpu Research Oy, Pori, Finland, 2007, www.outotec.com.