Abstract BaZr0.8Y0.2O3−δ (BZY) layers with various thicknesses (∼0.7, ∼1.7, ∼2.4 and ∼3.6 μm) are fabricated using the pulsed laser deposition (PLD) technique on anode-supported BaCe0.8Y0.2O3−δ (BCY) electrolyte films. Sm0.5Sr0.5CoO3−δ-SDC (SSC-SDC, 70:30 wt.%) cathode is applied onto the BZY/BCY bilayer electrolyte to form a single cell. The chemical stability of the BZY/BCY bilayer electrolytes improves with increasing BZY layer thickness. The BZY (∼3.6 μm)/BCY bilayer electrolyte shows an excellent chemical stability after treated in 100% CO2 atmosphere at 900 °C. The maximum power densities of 447, 370, 276, 218 and 163 mW cm−2 are measured with the BZY layer thicknesses of 0, 0.7, 1.7, 2.4 and 3.6 μm at 700 °C, respectively. In general, the BZY/BCY bilayer electrolyte cell with an optimum BZY layer thickness can improve chemical stability without great influence on the electrochemical performance for intermediate temperature solid oxide fuel cells.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Bi · Electrochem. Commun. · 2008 · 10 · 159810.1016/j.elecom.2008.08.024 ↗
2. Sun · J. Power Sources · 2013 · 229 · 9510.1016/j.jpowsour.2012.12.017 ↗
3. Iwahara · Solid State Ionics · 1981 · 3–4 · 35910.1016/0167-2738(81)90113-2 ↗
4. Bi · Energy Environ. Sci. · 2011 · 4 · 135210.1039/c0ee00387e ↗
5. Zuo · Adv. Mater. · 2006 · 18 · 331810.1002/adma.200601366 ↗
6. Kreuer · Annu. Rev. Mater. Res. · 2003 · 33 · 33310.1146/annurev.matsci.33.022802.091825 ↗
7. Fabbri · Chem. Soc. Rev. · 2010 · 39 · 435510.1039/b902343g ↗
8. Pergolesi · Nat. Mater. · 2010 · 9 · 84610.1038/nmat2837 ↗
9. Yamazaki · Chem. Mater. · 2009 · 21 · 275510.1021/cm900208w ↗
10. Kreuer · Solid State Ionics · 1999 · 125 · 28510.1016/S0167-2738(99)00188-5 ↗
11. Kreuer · Solid State Ionics · 2001 · 145 · 29510.1016/S0167-2738(01)00953-5 ↗
12. Joo · Solid State Ionics · 2006 · 177 · 105310.1016/j.ssi.2006.04.008 ↗
13. Pergolesi · Electrochem. Commun. · 2010 · 12 · 97710.1016/j.elecom.2010.05.005 ↗
14. Fabbri · Energy Environ. Sci. · 2008 · 1 · 35510.1039/b806655h ↗
15. Sun · J. Power Sources · 2011 · 196 · 6210.1016/j.jpowsour.2010.07.038 ↗
16. Liu · J. Membr. Sci. · 2012 · 415 · 39110.1016/j.memsci.2012.05.062 ↗
17. Fabbri · Adv. Mater. · 2012 · 24 · 19510.1002/adma.201103102 ↗
18. Guo · J. Power Sources · 2009 · 193 · 40010.1016/j.jpowsour.2009.03.044 ↗
19. Haile · J. Mater. Sci. · 2001 · 36 · 114910.1023/A:1004877708871 ↗
20. Ji · Solid State Ionics · 2011 · 203 · 910.1016/j.ssi.2011.09.016 ↗
21. Tong · J. Mater. Chem. · 2010 · 20 · 633310.1039/c0jm00381f ↗
22. Bi · J. Power Sources · 2009 · 191 · 42810.1016/j.jpowsour.2009.02.049 ↗
23. Tao · J. Power Sources · 2010 · 195 · 348110.1016/j.jpowsour.2009.12.047 ↗
24. Bi · J. Alloys Compd. · 2009 · 473 · 4810.1016/j.jallcom.2008.05.062 ↗
25. Xie · J. Alloys Compd. · 2009 · 472 · 55110.1016/j.jallcom.2008.05.036 ↗
26. Zhao · J. Power Sources · 2005 · 141 · 7910.1016/j.jpowsour.2004.08.057 ↗
27. Xia · Electrochem. Solid State Lett. · 2002 · 5 · A21710.1149/1.1503203 ↗
28. Fabbri · Solid State Ionics · 2008 · 179 · 55810.1016/j.ssi.2008.04.002 ↗
29. Lin · J. Power Sources · 2008 · 183 · 47910.1016/j.jpowsour.2008.05.075 ↗