Highly reversal-tolerant anodes using Ti4O7-supported platinum with a very small amount of water-splitting catalyst
Source abstract
Abstract
Gross fuel starvation can seriously damage the anode of polymer electrolyte fuel cells (PEFCs) due to the exceptionally high anodic potential induced by oxygen evolution and carbon corrosion reactions to generate protons, instead of hydrogen oxidation. In this report, we describe a highly effective reversal-tolerant anode catalyst (RTA) based on Pt/Ti 4O 7 with a very small amount of Ir. A membrane electrode assembly (MEA) using a Pt/Ti 4O 7 RTA including 0.04 mg Ir cm −2 shows almost no performance loss even after severe cell reversal. This is in clear contrast with the results obtained with an Pt/C RTA including the same amount of Ir, for which a significant voltage loss is observed after a cell reversal test. Moreover, the reversal-tolerance of Pt/Ti 4O 7 RTA is considerably high even with a very small amount of Ir, as low as 0.014 mg Ir cm −2. An Ir/Ti 4O 7 based anode also shows superior RTA property as well as the mitigation of start-up/shut-down degradation due to the limited activity of Ir for the oxygen reduction reaction. A post-mortem analysis of the tested MEA confirmed that Pt/Ti 4O 7 RTA alleviates damage to not only the catalyst layer but also the micro porous layer, which leads to a better RTA property for the Pt/Ti 4O 7.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electrocatalysts for Energy Conversion · Fuel Cells and Related Materials · Advanced battery technologies research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Yoshida · Interface · 2015 · 45
2. Ralph · Platin. Met. Rev. · 2002 · 46 · 11710.1595/003214002X463117135 ↗
3. Knights · J. Power Sources · 2004 · 127 · 12710.1016/j.jpowsour.2003.09.033 ↗
4. Taniguchi · J. Power Sources · 2004 · 130 · 4210.1016/j.jpowsour.2003.12.035 ↗
5. Ralph · ECS Trans. · 2006 · 1 · 6710.1149/1.2214545 ↗
6. Lim · J. Electrochem. Soc. · 2017 · 164 · F158010.1149/2.0731714jes ↗
7. Arai · SAE Int. J. Altern. Powertrains · 2017 · 6 · 14510.4271/2017-01-1179 ↗
8. Perry · ECS Trans. · 2006 · 3 · 78310.1149/1.2356198 ↗
9. S. D. Knights, D. P. Wilkinson, S. A. Campbell, J. L. Taylor, J. M. Gascoyne, T. R. Ralph, US Patent 6936370 (2005).
10. Mandal · J. Power Sources · 2018 · 397 · 39710.1016/j.jpowsour.2018.06.083 ↗
11. You · J. Electrochem. Soc. · 2018 · 165 · F309410.1149/2.0121806jes ↗
12. Hong · J. Power Sources · 2016 · 328 · 28010.1016/j.jpowsour.2016.07.002 ↗
13. Moore · J. Power Sources · 2019 · 417 · 5310.1016/j.jpowsour.2019.02.006 ↗
14. Moore · J. Phys. Chem. C · 2019 · 123 · 2336110.1021/acs.jpcc.9b05652 ↗
15. Bartholomew · Phys. Rev. · 1969 · 187 · 82810.1103/PhysRev.187.828 ↗
16. Ioroi · Electrochem. Commun. · 2005 · 7 · 18310.1016/j.elecom.2004.12.007 ↗
17. Ioroi · Phys. Chem. Chem. Phys. · 2010 · 12 · 752910.1039/b923218d ↗
18. Ioroi · J. Power Sources · 2013 · 223 · 18310.1016/j.jpowsour.2012.09.063 ↗
19. R. Shimoi, T. Horibe, Japanese Patent 5755833 (2015).
20. Yu · ECS Trans. · 2006 · 3 · 79710.1149/1.2356199 ↗
21. Kinoshita · 1988
22. Ioroi · J. Electrochem. Soc. · 2008 · 155 · B32110.1149/1.2833310 ↗
23. Liu · J. Electrochem. Soc. · 2010 · 157 · B90610.1149/1.3391737 ↗
24. Ghosh · J. Power Sources · 2017 · 362 · 29110.1016/j.jpowsour.2017.07.017 ↗
25. Pokhrel · J. Power Sources · 2016 · 329 · 33010.1016/j.jpowsour.2016.08.092 ↗
26. Durst · J. Electrochem. Soc. · 2015 · 162 · F19010.1149/2.0981501jes ↗
27. Reiser · Electrochem. Solid State Lett. · 2005 · 8 · A27310.1149/1.1896466 ↗
28. Durst · ECS Trans. · 2015 · 69 · 6710.1149/06917.0067ecst ↗
29. 1987 · 139