Proton exchange membrane fuel cell reversible performance loss induced by carbon monoxide produced during operation
Source abstract
Abstract
Abstract Cyclic voltammetry measurements at the anode have been carried out and reveal the presence of carbon monoxide in steady-state operation, with pure hydrogen. Experiments have been performed both in single cell and in stack to find out its origin. The contamination of the anode catalyst is partly due the reverse-water gas shift (RWGS) with carbon dioxide from the cathode. However, this study shows a temperature-activated and time-related corrosion mechanism which appears under humidified hydrogen. Due to this degradation mechanism, a reversible 25 mV-loss of performances is observed and can be recovered by oxidizing carbon monoxide on the anode.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advanced battery technologies research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Scientific aspects of polymer electrolyte fuel cell durability and degradation10.1021/cr050182l ↗
2. Wang · 2012
3. Carbon support oxidation in PEM fuel cell cathodes10.1016/j.jpowsour.2007.08.053 ↗
4. Investigation of the recoverable degradation of PEM fuel cell operated under drive cycle and different humidities10.1016/j.ijhydene.2014.02.023 ↗
5. Reversible and irreversible degradation in fuel cells during Open Circuit Voltage durability testing10.1016/j.jpowsour.2008.04.009 ↗
6. Recoverable cathode performance loss in direct methanol fuel cells10.1149/1.2136073 ↗
7. Transient platinum oxide formation and oxygen reduction on carbon-supported platinum and platinum-cobalt alloy electrocatalysts10.1149/2.018401jes ↗
8. Mass spectrometric investigation of the electrochemical behavior of adsorbed carbon monoxide at platinum in 0.2 M sulphuric acid10.1016/0013-4686(77)85090-1 ↗
9. Size effects on reactivity of Pt nanoparticles in CO monolayer oxidation: the role of surface mobility10.1039/b303911k ↗
10. Real surface area measurements in electrochemistry10.1016/0022-0728(92)80162-W ↗
11. Electrocatalytic corrosion of carbon support in PEMFC cathodes10.1149/1.1630412 ↗
12. Investigation of carbon corrosion behavior and kinetics in proton exchange membrane fuel cell cathode electrodes10.1149/2.120306jes ↗
13. Y. Okajima, A. Yamamoto, M. Sudoh, S. Sakai, Y. Matsumoto, « Effect of carbon dioxide in hydrogen on PEMFC for using reformed gas from biogas », vol. 79. Electrochem. Soc. Jpn., p. 346-348.10.5796/electrochemistry.79.346 ↗
14. Quantifying the ‘reverse water gas shift’ reaction inside a PEM fuel cell10.1016/j.apcatb.2004.08.016 ↗
15. The influence of carbon dioxide on PEM fuel cell anodes10.1016/S0378-7753(02)00227-6 ↗
16. Degradation of proton exchange membrane fuel cells due to CO and CO2 poisoning10.1016/j.jpowsour.2008.11.107 ↗
17. Modelling study of CO2 poisoning on PEMFC anodes10.1016/j.jpowsour.2004.05.004 ↗
18. Behaviour modelling of a PEMFC operating on diluted hydrogen feed10.1002/er.1424 ↗
19. A review on performance degradation of proton exchange membrane fuel cells during startup and shutdown processes: causes, consequences, and mitigation strategies10.1016/j.jpowsour.2012.01.059 ↗
20. A reverse-current decay mechanism for fuel cells10.1149/1.1896466 ↗
21. The influence of Pt-activation on the corrosion of carbon in gas diffusion electrodes—a dems study10.1016/S0022-0728(84)80252-1 ↗
22. Study of electrochemical instabilities of PEMFC electrodes in aqueous solution by means of membrane inlet mass spectrometry10.1016/j.jelechem.2006.03.055 ↗
23. Durability investigation of carbon nanotube as catalyst support for proton exchange membrane fuel cell10.1016/j.jpowsour.2005.09.039 ↗
24. Carbon corrosion in proton-exchange membrane fuel cells: from model experiments to real-life operation in membrane electrode assemblies10.1021/cs500449q ↗
25. Characterization of vulcan electrochemically oxidized under simulated PEM fuel cell conditions10.1149/1.1649756 ↗
26. An investigation into factors affecting the stability of carbons and carbon supported platinum and platinum/cobalt alloy catalysts during 1.2V potentiostatic hold regimes at a range of temperatures10.1016/j.jpowsour.2006.11.004 ↗
27. Surface oxidation of carbon supports due to potential cycling under PEM fuel cell conditions10.1016/j.electacta.2010.03.056 ↗
28. Imaging of highly oriented pyrolytic graphite corrosion accelerated by Pt particles10.1016/j.elecom.2005.08.014 ↗
29. Stability of Pt-Catalyzed highly oriented pyrolytic graphite against hydrogen peroxide in acid solution10.1149/1.2130665 ↗
30. Oxygen reduction on a high-surface area Pt/Vulcan carbon catalyst: a thin-film rotating ring-disk electrode study10.1016/S0022-0728(00)00407-1 ↗
31. Novel technique for measuring oxygen crossover through the membrane in polymer electrolyte membrane fuel cells10.1016/j.ijhydene.2013.04.142 ↗
32. Electrochemical measurement of the oxygen permeation rate through polymer electrolyte membranes10.1149/2.081306jes ↗
33. The role of carbon materials in heterogeneous catalysis10.1016/S0008-6223(97)00173-5 ↗
34. A new approach to the problem of carbon monoxide poisoning in fuel cells operating at low temperatures10.1149/1.2095401 ↗
35. The CO poisoning mechanism of the hydrogen oxidation reaction in proton exchange membrane fuel cells10.1149/1.1473775 ↗
36. Carbon monoxide poisoning of proton exchange membrane fuel cells10.1002/er.713 ↗
37. Effect of CO gas and anode-metal loading on H2 oxidation in proton exchange membrane fuel cell10.1016/S0378-7753(01)00838-2 ↗
38. ChemInform abstract: performance data of a proton exchange membrane fuel cell using H2/CO as fuel gas10.1002/chin.199714018 ↗
39. Quantitative analysis of the performance impact of low-level carbon monoxide exposure in proton exchange membrane fuel cells10.1016/j.jpowsour.2012.11.062 ↗
40. Effect of contaminants on polymer electrolyte membrane fuel cells10.1016/j.pecs.2010.06.003 ↗
41. Effect of fuel utilization on the carbon monoxide poisoning dynamics of polymer electrolyte membrane fuel cells10.1016/j.jpowsour.2014.02.016 ↗
42. Local degradation analysis of a real long-term operated DMFC stack MEA10.1016/j.jpowsour.2012.07.048 ↗
43. Investigation of platinum oxidation in PEM fuel cells at various relative humidities10.1149/1.2372230 ↗
44. H. H. Voss, R. H. Barton, M. Sexsmith, et M. Turchyn, « Conditioning and maintenance methods for fuel cells », U. S. 2003/0224227 A1, 2003.
45. Extent of PEMFC cathode surface oxidation by oxygen and water measured by CV10.1149/1.1649698 ↗
46. The possible failure mode and effect analysis of membrane electrode assemblies and their potential solutions in direct methanol fuel cell systems for portable applications10.1016/j.ijhydene.2010.05.107 ↗
47. High-efficiency active DMFC system for portable applications10.1109/TPEL.2011.2106144 ↗
48. Influence of contamination with inorganic impurities on the durability of a 1 kW DMFC system10.1002/fuce.201300047 ↗
49. Paganelli · 2013
50. Local catalyst support degradation during polymer electrolyte fuel cell start-up and shutdown10.1149/2.019212jes ↗