Abstract For the proper function of solid oxide fuel cells (SOFC) their structural integrity must be maintained during their whole lifetime. Any cell fracture would cause leakage and partial oxidization of the anode, leading to a reduced performance, if not catastrophic failure of the whole stack. In this study, the mechanical strength of a state of the art SOFC, developed and produced by Hexis AG/Switzerland, was investigated with respect to the influence of temperature and ageing, whilst for the anode side of the cell the strength was measured under reducing and oxidizing atmospheres. Ball-on-3-Ball bending strength tests and fractography conducted on anode and cathode half-cells revealed the underlying mechanisms, which lead to cell fracture. They were found to be different for the cathode and the anode side and that they change with temperature and ageing. Both anode and cathode sides exhibit the lowest strength at T = 850 °C, which is greatly reduced to the initial strength of the bare electrolyte. This reduction is the consequence of the formation of cracks in the electrode layer which either directly penetrate into the electrolyte (anode side) or locally increase the stress intensity level of pre-existing flaws of the electrolytes at the interface (cathode side).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Fuel Cells and Related Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Nakajo · J. Power Sources · 2009 · 193 · 20310.1016/j.jpowsour.2008.12.050 ↗
2. Nakajo · Ceram. Int. · 2012 · 38 · 390710.1016/j.ceramint.2012.01.043 ↗
3. Fleischhauer · J. Power Sources · 2015 · 275 · 21710.1016/j.jpowsour.2014.10.083 ↗
4. Fleischhauer · J. Power Sources · 2015 · 273 · 23710.1016/j.jpowsour.2014.09.068 ↗
5. Selcuk · J. Mater. Sci. · 2001 · 36 · 117310.1023/A:1004833909780 ↗
6. Sorensen · J. Mater. Sci. · 1998 · 33 · 529110.1023/A:1004429829323 ↗
7. Sorensen · J. Eur. Ceram. Soc. · 2012 · 32 · 416510.1016/j.jeurceramsoc.2012.06.012 ↗
8. Mai · 2012
9. Börger · J. Eur. Ceram. Soc. · 2004 · 24 · 291710.1016/j.jeurceramsoc.2003.10.035 ↗
10. Börger · J. Eur. Ceram. Soc. · 2002 · 22 · 142510.1016/S0955-2219(01)00458-7 ↗
11. Bermejo · Eng. Fract. Mech. · 2013 · 101 · 10810.1016/j.engfracmech.2012.12.004 ↗
12. Danzer · J. Ceram. Soc. Jpn. · 2006 · 114 · 105410.2109/jcersj.114.1054 ↗
13. Bermejo · J. Eur. Ceram. Soc. · 2011 · 31 · 74510.1016/j.jeurceramsoc.2010.11.031 ↗
14. Hsueh · Dent. Mater. · 2006 · 22 · 46010.1016/j.dental.2005.04.037 ↗
15. Hsueh · Compos. Sci. Technol. · 2007 · 67 · 27810.1016/j.compscitech.2006.08.003 ↗
16. Young · 2002
17. Kuebler · Fuel Cells · 2010 · 10 · 106610.1002/fuce.201000040 ↗
18. Fleischhauer · J. Power Sources · 2014 · 258 · 38210.1016/j.jpowsour.2014.02.009 ↗
19. Tsoga · Acta Mater. · 2000 · 48 · 470910.1016/S1359-6454(00)00261-5 ↗
20. Mai · Solid State Ion. · 2006 · 177 · 210310.1016/j.ssi.2005.12.010 ↗
21. Hashida · Solid Oxide Fuel Cells 11 (Sofc-Xi) · 2009 · 25 · 156510.1149/1.3205692 ↗
22. Atkinson · Solid State Ion. · 2000 · 134 · 5910.1016/S0167-2738(00)00714-1 ↗
23. Ye · Int. J. Solids Struct. · 1992 · 29 · 263910.1016/0020-7683(92)90227-K ↗
24. Bermejo · J. Eur. Ceram. Soc. · 2012 · 32 · 25110.1016/j.jeurceramsoc.2011.09.008 ↗
25. Wiederhorn · J. Am. Ceram. Soc. · 1967 · 50 · 40710.1111/j.1151-2916.1967.tb15145.x ↗
26. Danzer · Adv. Eng. Mater. · 2008 · 10 · 27510.1002/adem.200700347 ↗