Joint strength of a solid oxide fuel cell glass–ceramic sealant with metallic interconnect in a reducing environment
Source abstract
Abstract
Abstract Effects of reducing environment and thermal aging on the joint strength of a BaO–B2O3–Al2O3–SiO2 glass–ceramic sealant (GC-9) with a ferritic-stainless-steel interconnect (Crofer 22 H) for planar solid oxide fuel cells are investigated. A technique is developed for conducting mechanical tests at room temperature and 800 °C in H2-7 vol% H2O under shear and tensile loadings. Given an aged condition and loading mode, the joint strength at 800 °C is lower than that at room temperature in the given humidified hydrogen atmosphere. A thermal aging at 800 °C in H2-7 vol% H2O for 100 h or 1000 h enhances both shear and tensile joint strengths at room temperature but degrades them at 800 °C in the same reducing environment. Non-aged specimens show a comparable joint strength and fracture mode when tested in humidified hydrogen and in air under a given loading mode and testing temperature. The shear strength at 800 °C for joint specimens after a 1000-h thermal aging at 800 °C in air or humidified hydrogen is reduced by a similar extent of 19%, compared to the counterpart of non-aged joint specimens tested in the same oxidizing or reducing environment.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Catalysis and Oxidation Reactions · Electronic and Structural Properties of Oxides
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Fergus · J. Power Sources · 2005 · 147 · 4610.1016/j.jpowsour.2005.05.002 ↗
2. Lessing · J. Mater. Sci. · 2007 · 42 · 346510.1007/s10853-006-0409-9 ↗
3. Lin · J. Power Sources · 2007 · 164 · 23810.1016/j.jpowsour.2006.10.089 ↗
4. Lin · J. Power Sources · 2009 · 192 · 51510.1016/j.jpowsour.2009.03.010 ↗
5. Zhao · J. Power Sources · 2013 · 239 · 50010.1016/j.jpowsour.2013.04.043 ↗
6. Nakajo · Ceram. Int. · 2012 · 38 · 390710.1016/j.ceramint.2012.01.043 ↗
7. Batfalsky · J. Power Sources · 2006 · 155 · 12810.1016/j.jpowsour.2005.05.046 ↗
8. Haanappel · J. Power Sources · 2005 · 150 · 8610.1016/j.jpowsour.2005.02.015 ↗
9. Haanappel · J. Power Sources · 2005 · 141 · 10210.1016/j.jpowsour.2004.08.053 ↗
10. Haanappel · J. Mater. Sci. · 2005 · 40 · 158310.1007/s10853-005-0657-0 ↗
11. Menzler · J. Power Sources · 2005 · 152 · 15610.1016/j.jpowsour.2005.02.072 ↗
12. Goel · J. Power Sources · 2010 · 195 · 52210.1016/j.jpowsour.2009.08.007 ↗
13. Yang · J. Electrochem. Soc. · 2003 · 150 · A109510.1149/1.1590325 ↗
14. Yang · Solid State Ion. · 2003 · 160 · 21310.1016/S0167-2738(03)00160-7 ↗
15. Yang · J. Mater. Eng. Perform. · 2003 · 13 · 32710.1361/10599490419298 ↗
16. Smeacetto · Mater. Lett. · 2011 · 65 · 104810.1016/j.matlet.2010.12.050 ↗
17. Smeacetto · J. Eur. Ceram. Soc. · 2008 · 28 · 6110.1016/j.jeurceramsoc.2007.05.006 ↗
18. Smeacetto · J. Power Sources · 2009 · 190 · 40210.1016/j.jpowsour.2009.01.042 ↗
19. Smeacetto · J. Eur. Ceram. Soc. · 2008 · 28 · 252110.1016/j.jeurceramsoc.2008.03.035 ↗
20. Stephens · J. Power Sources · 2009 · 193 · 62510.1016/j.jpowsour.2009.02.080 ↗
21. Chou · J. Power Sources · 2008 · 184 · 23810.1016/j.jpowsour.2008.06.020 ↗
22. Chou · J. Power Sources · 2008 · 185 · 100110.1016/j.jpowsour.2008.09.004 ↗
23. Malzbender · J. Mater. Sci. · 2012 · 47 · 434210.1007/s10853-012-6286-5 ↗
24. Malzbender · Fuel Cells · 2012 · 12 · 4710.1002/fuce.201100116 ↗
25. Malzbender · J. Mater. Res. · 2003 · 18 · 92910.1557/JMR.2003.0127 ↗
26. Malzbender · Ceram. Eng. Sci. Proc. · 2005 · 26 · 28510.1002/9780470291221.ch34 ↗
27. Muller · Eng. Fract. Mech. · 2006 · 73 · 9910.1016/j.engfracmech.2005.12.001 ↗
28. Lin · J. Power Sources · 2012 · 205 · 30710.1016/j.jpowsour.2012.01.048 ↗
29. Lin · J. Power Sources · 2014 · 245 · 78710.1016/j.jpowsour.2013.07.047 ↗
30. Lin · J. Power Sources · 2014 · 261 · 22710.1016/j.jpowsour.2014.03.079 ↗
31. Chang · J. Power Sources · 2009 · 189 · 109310.1016/j.jpowsour.2008.12.102 ↗
32. Chang · J. Power Sources · 2010 · 195 · 315910.1016/j.jpowsour.2009.12.008 ↗
33. Chang · J. Power Sources · 2011 · 196 · 358310.1016/j.jpowsour.2010.12.035 ↗
34. Lin · J. Power Sources · 2013 · 241 · 1210.1016/j.jpowsour.2013.04.088 ↗
35. Chiu · J. Power Sources · 2011 · 196 · 200510.1016/j.jpowsour.2010.09.083 ↗
36. Chiu · J. Power Sources · 2012 · 198 · 14910.1016/j.jpowsour.2011.09.056 ↗
37. Chiu · J. Power Sources · 2012 · 219 · 11210.1016/j.jpowsour.2012.07.038 ↗
38. C.-K. Liu, T.-Y. Yung, K.-F. Lin, R.-Y. Lee, T.-S. Lee, Glass-Ceramic Sealant for Planar Solid Oxide Fuel Cells, United States Patent No. 7,897,530 B2 (2011).
39. Liu · 2007
40. Liu · 2007
41. Liu · 2008
42. Liu · 2009
43. Liu · ECS Trans. · 2009 · 25 · 149110.1149/1.3205683 ↗
44. Liu · Ceram. Eng. Sci. Proc. · 2015 · 35
45. Tomozawa · J. Non Cryst. Solids · 1994 · 179 · 16210.1016/0022-3093(94)90693-9 ↗
46. Fujita · J. Non Cryst. Solids · 2003 · 320 · 5610.1016/S0022-3093(03)00077-2 ↗
47. Jin · Int. J. Hydrog. Energy · 2013 · 38 · 1630810.1016/j.ijhydene.2013.09.124 ↗
48. Liu · J. Power Sources · 2008 · 185 · 119310.1016/j.jpowsour.2008.07.017 ↗