journal article·2015-06Open access

Structural correlations: Design levers for performance and durability of catalyst layers

Kateryna Artyushkova, Plamen Atanassov, Monica Dutta, Silvia Wessel, Vesna Colbow

Abstract

Abstract Durability of the catalyst layer (CL) is of vital importance in the large-scale deployment of PEMFCs. It is necessary to determine parameters that represent properties of catalysts layer and other cathode components for optimization of fuel cell performance and durability. The structure, morphology and surface chemistry of the catalyst powder affects the ionomer and catalyst interaction, ionomer dispersion in the catalyst layer and, for this reason, its morphology and chemistry. These, in turn, affect the catalyst layer effective properties such as thickness, porosity, tortuosity, diffusivity, conductivity and others, directly influencing electrode performance and durability. In this study, X-ray Photoelectron Spectroscopy and SEM are used to quantify surface species and morphology of membrane electrode assemblies (MEAs) tested under different accelerated stress test (AST) conditions. Correlations between composition, structure and morphological properties of cathode components and the catalyst layer have been developed and linked to catalyst layer performance losses. The key relationships between the catalyst layer effective properties and performance and durability provide design and optimization levers for making MEAs for different operating regimes.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advancements in Solid Oxide Fuel Cells

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. 2010
2. Ferreira-Aparicio · J. Power Sources · 2011 · 196 · 424210.1016/j.jpowsour.2010.10.059 ↗
3. Bae · Appl. Energ. · 2014 · 131 · 4810.1016/j.apenergy.2014.05.064 ↗
4. Dubau · Wiley Interdiscip. Rev. Energy Environ. · 2014 · 3 · 540
5. Zhang · Int. J. Hydrog. Energy · 2009 · 34 · 38810.1016/j.ijhydene.2008.10.012 ↗
6. Park · Electrochim. Acta · 2012 · 83 · 29410.1016/j.electacta.2012.07.117 ↗
7. Marcu · J. Power Sources · 2012 · 215 · 26610.1016/j.jpowsour.2012.05.010 ↗
8. Shao · J. Power Sources · 2007 · 171 · 55810.1016/j.jpowsour.2007.07.004 ↗
9. Trogadas · Carbon · 2014 · 75 · 510.1016/j.carbon.2014.04.005 ↗
10. 7-Catalyst ageing and degradation in polymer electrolyte membrane fuel cells
11. Avasarala · Electrochim. Acta · 2010 · 55 · 476510.1016/j.electacta.2010.03.056 ↗
12. Sharma · J. Power Sources · 2012 · 208 · 9610.1016/j.jpowsour.2012.02.011 ↗
13. Zhao · Electrochim. Acta · 2013 · 97 · 3310.1016/j.electacta.2013.02.062 ↗
14. Kim · Carbon · 2014 · 77 · 52510.1016/j.carbon.2014.05.058 ↗
15. Kim · Electrochim. Acta · 2014 · 134 · 41810.1016/j.electacta.2014.04.131 ↗
16. Peron · J. Power Sources · 2008 · 185 · 120910.1016/j.jpowsour.2008.06.098 ↗
17. Patel · J. Vac. Sci. Technol. A · 2012 · 3010.1116/1.4707153 ↗
18. Patel · Polym. Electrolyte Fuel Cells · 2011 · 11 · 845
19. Patel · Ecs Trans. · 2010 · 33 · 42510.1149/1.3484541 ↗
20. Castanheira · ACS Catal. · 2014 · 4 · 225810.1021/cs500449q ↗
21. Ferreira · J. Electrochem. Soc. · 2005 · 152 · A225610.1149/1.2050347 ↗
22. Srivastava · J. Power Sources · 2009 · 190 · 4010.1016/j.jpowsour.2008.09.038 ↗
23. Bigdeli · Rsc Adv. · 2014 · 4 · 6013510.1039/C4RA10375K ↗
24. Artyushkova · Rsc Adv. · 2012 · 2 · 430410.1039/c2ra00574c ↗
25. Artyushkova · J. Power Sources · 2012 · 214 · 30310.1016/j.jpowsour.2012.04.095 ↗
26. Reshetenko · J. Electrochem. Soc. · 2013 · 160 · F130510.1149/2.104311jes ↗
27. Santoro · Carbon · 2014 · 67 · 12810.1016/j.carbon.2013.09.071 ↗
28. Young · J. Electrochem. Soc. · 2010 · 157 · B42510.1149/1.3281899 ↗
29. Hitchcock · J. Power Sources · 2014 · 266 · 6610.1016/j.jpowsour.2014.04.119 ↗