Electrochemical cleaning: An in-Situ method to reverse chromium poisoning in solid oxide fuel cell cathodes
Source abstract
Abstract
Abstract Chromium poisoning is one of the primary factors that affect solid oxide fuel cell (SOFC) durability. In this study, an electrochemical cleaning method has been employed to reverse the effects of chromium poisoning. Two cells were fabricated and poisoned under identical conditions by operating them at 800 °C in the presence of a Cr source. Both poisoned cells exhibited a significant reduction in maximum power density and an increase in polarization resistance. One of the poisoned cells, designated as the baseline cell, was cooled to room temperature after poisoning. Microstructural observation of the baseline cell showed significant contamination of the cathode active layer by chromium oxide and (Cr,Mn) spinel deposits. The other poisoned cell was electrochemically cleaned for 2 h under a mild electrolytic condition. As a result of the electrochemical cleaning process, the chromium oxide deposits were substantially removed leading to a significant reduction of Cr concentration in the cathode, especially at the cathode/electrolyte interface. A substantial fraction of the cell performance loss was also reversed. To the best of our knowledge, this is a first demonstration of reversing the effects of chromium poisoning using a rapid in-situ process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Running on natural gas10.1038/23144 ↗
2. Solid oxide fuel cells (SOFCs): a review of an environmentally clean and efficient source of energy10.1016/S1364-0321(02)00014-X ↗
3. Solid oxide fuel cell technology—features and applications10.1016/j.ssi.2004.07.042 ↗
4. Fuel cell electric vehicle as a power plant and SOFC as a natural gas reformer: an exergy analysis of different system designs10.1016/j.apenergy.2016.03.107 ↗
5. Application of solid oxide fuel cell technology for power generation—a review10.1016/j.rser.2012.11.031 ↗
6. Prospects of different fuel cell technologies for vehicle applications10.1016/S0378-7753(02)00029-0 ↗
7. Interaction between chromia forming alloy interconnects and air10.1016/S0167-2738(97)00247-6 ↗
8. Worldwide SOFC technology overview and benchmark10.1111/j.1744-7402.2005.02049.x ↗
9. Evaluation of fuel cell system efficiency and degradation at development and during commercialization10.1016/j.jpowsour.2005.10.109 ↗
10. Fundamental mechanisms limiting solid oxide fuel cell durability10.1016/j.jpowsour.2008.02.016 ↗
11. Chromium vaporization from metallic interconnect and retention by perovskite layers10.1149/199919.0774PV ↗
12. Chromium vapor species over solid oxide fuel cell interconnect materials and their potential for degradation processes10.1149/1.1837264 ↗
13. Chromium poisoning of La 1-x Sr x MnO 3±δ cathodes and electrochemical validation of chromium getters in intermediate temperature-solid oxide fuel cells10.1149/2.0931913jes ↗
14. Microstructural degradation of (La,Sr)MnO[sub 3]∕YSZ cathodes in solid oxide fuel cells with uncoated E-Brite interconnects10.1149/1.3515073 ↗
15. Chromium poisoning of perovskite cathodes by the ODS alloy Cr5Fe1Y2O3 and the high chromium ferritic steel Crofer22APU10.1149/1.2172563 ↗
16. Chromium deposition and poisoning of cathodes of solid oxide fuel cells – a review10.1016/j.ijhydene.2013.10.042 ↗
17. Cu1. 3Mn1. 7O4 spinel coatings deposited by electrophoretic deposition on Crofer 22 APU substrates for solid oxide fuel cell applications10.1016/j.surfcoat.2016.09.028 ↗
18. CuMn1. 8O4 protective coatings on metallic interconnects for prevention of Cr-poisoning in solid oxide fuel cells10.1016/j.jpowsour.2017.12.031 ↗
19. Prevention of SOFC cathode degradation in contact with Cr-containing alloy10.1016/j.jpowsour.2003.12.051 ↗
20. A review of recent progress in coatings, surface modifications and alloy developments for solid oxide fuel cell ferritic stainless steel interconnects10.1016/j.jpowsour.2009.09.069 ↗
21. Reduction of chromium vaporization from SOFC interconnectors by highly effective coatings10.1016/j.jpowsour.2006.08.013 ↗
22. The effect of chromium oxyhydroxide on solid oxide fuel cells10.1149/1.3266930 ↗
23. Chromium poisoning of LSM-YSZ SOFC cathodes10.1149/1.1806392 ↗
24. Degradation phenomena in the cathode of a solid oxide fuel cell with an alloy separator10.1016/0378-7753(94)02172-Y ↗
25. Chromium poisoning effects on performance of (La,Sr)MnO 3 -based cathode in anode-supported solid oxide fuel cells10.1149/2.0441707jes ↗
26. Polarization measurements on single-step co-fired solid oxide fuel cells (SOFCs)10.1016/j.jpowsour.2007.03.003 ↗
27. Roles of humidity and cathodic current in chromium poisoning of Sr-doped LaMnO3-based cathodes in solid oxide fuel cells10.1016/j.jpowsour.2017.06.005 ↗
28. Recent advances in high temperature electrolysis using solid oxide fuel cells: a review10.1016/j.jpowsour.2011.12.019 ↗
29. Chromium vaporization of bare and of coated iron–chromium alloys at 1073 K10.1016/j.ssi.2006.12.010 ↗
30. Electrochemical properties of a SOFC cathode in contact with a chromium-containing alloy separator10.1016/S0167-2738(00)00654-8 ↗
31. Deposition of chromium species at Sr‐doped LaMnO3 electrodes in solid oxide fuel cells. I. Mechanism and kinetics10.1149/1.1394012 ↗
32. A fundamental study of chromium deposition on solid oxide fuel cell cathode materials10.1016/j.jpowsour.2006.02.017 ↗
33. Formation of chromium containing impurities in (La, Sr) MnO3 solid-oxide-fuel-cell cathodes under stack operating conditions and its effect on performance10.1016/j.ceramint.2016.03.010 ↗
34. A fundamental study of chromium deposition and poisoning at (La0.8Sr0.2)0.95(Mn1−xCox)O3 ± δ (0.0≤ x ≤1.0) cathodes of solid oxide fuel cells10.1016/j.ijhydene.2010.09.087 ↗