The influence of temperature on a nutty-cake structural material: LiMn1−xFexPO4 composite with LiFePO4 core and carbon outer layer for lithium-ion battery
Source abstract
Abstract
The extremely low electronic conductivity, slow ion diffusion kinetics, and the Jahn–Teller effect of LiMnPO4 limit its electrochemical performance. In this work, a nutty-cake structural C–LiMn1−xFexPO4–LiFePO4 cathode material is synthesized by hydrothermal method and further calcined at different temperatures. The influence of calcination temperature on the electrochemical behavior is investigated by X-ray diffractometer, scanning electron microscope, field-emission high-resolution transmission electron microscope, energy-dispersive X-ray spectroscopy, electrochemical impedance spectroscopy and charge–discharge tests. And the performance of C–LiMn1−xFexPO4–LiFePO4 materials has a relationship with its crystal structure. The well-crystallized Sample-600 calcined at 600 °C shows the smallest charge transfer resistance, the largest lithium ion diffusion coefficient (DLi) and the best cycling stability. The discharge capacity of Sample-600 holds around 112 mAh g−1 after the 3rd cycle at 0.1 C rate. The performances improvement of C–LiMn1−xFexPO4–LiFePO4 material can be mainly attributed to the iron diffusion from the LiFePO4 core to the outer LiMnPO4 layer under appropriate calcination temperature.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Padhi · J. Electrochem. Soc. · 1997 · 144 · 118810.1149/1.1837571 ↗
2. Li · Electrochem. Solid-State Lett. · 2002 · 5 · A13510.1149/1.1475195 ↗
3. Islam · Chem. Mater. · 2005 · 17 · 508510.1021/cm050999v ↗
4. Kang · Nature · 2009 · 458 · 19010.1038/nature07853 ↗
5. Wolfenstine · J. Power Sources · 2004 · 136 · 15010.1016/j.jpowsour.2004.05.017 ↗
6. Yonemura · J. Electrochem. Soc. · 2004 · 151 · A135210.1149/1.1773731 ↗
7. Delacourt · J. Electrochem. Soc. · 2005 · 152 · A91310.1149/1.1884787 ↗
8. Chen · J. Power Sources · 2012 · 214 · 34410.1016/j.jpowsour.2012.04.089 ↗
9. Fang · Electrochim. Acta · 2012 · 71 · 26610.1016/j.electacta.2012.03.160 ↗
10. Wang · J. Alloys Compd. · 2012 · 532 · 2510.1016/j.jallcom.2012.04.008 ↗
11. Yang · J. Solid State Electrochem. · 2012 · 16 · 127110.1007/s10008-011-1523-4 ↗
12. Pivko · Chem. Mater. · 2012 · 24 · 104110.1021/cm203095d ↗
13. Kwon · Electrochim. Acta · 2012 · 69 · 3810.1016/j.electacta.2012.02.040 ↗
14. Wang · J. Power Sources · 2011 · 196 · 1025810.1016/j.jpowsour.2011.08.090 ↗
15. Moon · Ceram. Int. · 2012 · 38 · S47110.1016/j.ceramint.2011.05.042 ↗
16. Kumar · J. Electrochem. Soc. · 2011 · 158 · A22710.1149/1.3527059 ↗
17. Zaghib · J. Power Sources · 2012 · 204 · 17710.1016/j.jpowsour.2011.11.085 ↗
18. Amine · Electrochem. Commun. · 2005 · 7 · 66910.1016/j.elecom.2005.04.018 ↗
19. Richards · Aust. J. Chem. · 1978 · 31 · 182510.1071/CH9781825 ↗
20. Diefallah · Thermochim. Acta · 1992 · 202 · 110.1016/0040-6031(92)85144-K ↗
21. Zou · Key Eng. Mater. · 2012 · 519 · 12410.4028/www.scientific.net/KEM.519.124 ↗
22. Su · Nanoscale · 2011 · 3 · 396710.1039/c1nr10550g ↗
23. Lim · Chem. Mater. · 2008 · 20 · 456010.1021/cm8006364 ↗
24. Nam · Electrochem. Commun. · 2009 · 11 · 91310.1016/j.elecom.2009.02.031 ↗
25. Martha · Angew. Chem. Int. Ed. · 2009 · 48 · 855910.1002/anie.200903587 ↗
26. Yamada · J. Electrochem. Soc. · 2001 · 148 · A22410.1149/1.1348257 ↗
27. Nie · Solid State Commun. · 2010 · 150 · 4010.1016/j.ssc.2009.10.010 ↗
28. Liu · J. Power Sources · 2006 · 159 · 71710.1016/j.jpowsour.2005.10.098 ↗
29. Cui · Electrochim. Acta · 2010 · 55 · 92210.1016/j.electacta.2009.08.020 ↗