High performance Si/C@CNF composite anode for solid-polymer lithium-ion batteries

Q. Si, K. Hanai, T. Ichikawa, A. Hirano, N. Imanishi, O. Yamamoto, Y. Takeda

Journal of Power Sources· Volume 196· Issue 16
Publisher page

Abstract

Abstract The electrochemical performance of a composite of nano-Si powder and a pyrolytic carbon of polyvinyl chloride (PVC) with carbon nanofiber (CNF) was examined as an anode for solid-polymer lithium-ion batteries. Nano-Si powder was firstly coated with carbon by pyrolysis of PVC and then mixed with CNF (referred to as Si/C@CNF) using a rotation mixer. The composite exhibited good cycling performance, but suffered from a large irreversible capacity loss of which the retention was less than 60%. In order to reduce the loss, a thin lithium sheet was attached to the Si/C@CNF electrode surface as a reducing agent. The irreversible capacity of the first cycle was lowered to as much as 0 mAh g−1 and after the third cycle, the lithium insertion and extraction efficiency was almost 100%. A reversible capacity of more than 1000 mAh g−1 was still maintained after 40 cycles.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Gauther · J. Electrochem. Soc. · 1985 · 132 · 133310.1149/1.2114112 ↗
2. Brissot · J. Power Sources · 1999 · 81–82 · 92510.1016/S0378-7753(98)00242-0 ↗
3. Imanishi · J. Power Sources · 2008 · 178 · 74410.1016/j.jpowsour.2007.09.035 ↗
4. Wen · J. Solid State Chem. · 1981 · 37 · 27110.1016/0022-4596(81)90487-4 ↗
5. Chan · J. Power Sources · 2009 · 189 · 3410.1016/j.jpowsour.2008.12.047 ↗
6. Kim · J. Electrochem. Soc. · 2005 · 152 · A52310.1149/1.1856990 ↗
7. Si · J. Power Sources · 2009 · 189 · 76110.1016/j.jpowsour.2008.08.007 ↗
8. Liu · Solid State Ionics · 2004 · 168 · 6110.1016/j.ssi.2004.01.031 ↗
9. Zuo · Mater. Chem. Phys. · 2009 · 115 · 75710.1016/j.matchemphys.2009.02.036 ↗
10. Liu · J. Power Sources · 2005 · 146 · 37610.1016/j.jpowsour.2005.03.022 ↗
11. Kobayashi · J. Power Sources · 2008 · 185 · 54210.1016/j.jpowsour.2008.05.067 ↗
12. Lee · J. Power Sources · 2005 · 141 · 15910.1016/j.jpowsour.2004.08.023 ↗
13. Park · J. Power Sources · 2006 · 158 · 65010.1016/j.jpowsour.2005.08.052 ↗
14. Li · J. Power Sources · 2008 · 184 · 47310.1016/j.jpowsour.2008.02.057 ↗
15. Si · J. Power Sources · 2010 · 195 · 172010.1016/j.jpowsour.2009.09.073 ↗
16. Saito · J. Power Sources · 2009 · 195 · 617210.1016/j.jpowsour.2009.11.076 ↗
17. Jarvis · J. Power Sources · 2006 · 162 · 80010.1016/j.jpowsour.2005.07.051 ↗
18. Obrovac · Electrochem. Solid State Lett. · 2004 · 7 · A9310.1149/1.1652421 ↗
19. Hatchard · J. Electrochem. Soc. · 2004 · 151 · A83810.1149/1.1739217 ↗