journal article·2018-05Open access

Effect of overcharge on Li(Ni0.5Mn0.3Co0.2)O2/Graphite lithium ion cells with poly(vinylidene fluoride) binder. I - Microstructural changes in the anode

Nancy Dietz Rago, Javier Bareño, Jianlin Li, Zhijia Du, David L. Wood, Leigh Anna Steele, Joshua Lamb, Scott Spangler, Christopher Grosso, Kyle Fenton, Ira Bloom

Abstract

Cells based on NMC/graphite, containing poly(vinylidene difluoride) (PVDF) binders in the positive and negative electrodes, were systematically overcharged to 100, 120, 140, 160, 180, and 250% state-of-charge (SOC). At 250% SOC the cell vented. Scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS) of the anodes showed several state-of-overcharge-dependent trends. Starting at 120% SOC, dendrites appeared and increased in concentration as the SOC increased. Dendrite morphology appeared to be dependent on whether the active material was on the “dull” or “shiny” side of the copper collector. Significantly more delamination of the active material from the collector was seen on the “shiny” side of the collector particularly at 180 and 250% SOC. Transition metals were detected at 120% SOC and increased in concentration as the SOC increased. There was considerable spatial heterogeneity in the microstructures across each laminate with several regions displaying complex layered structures.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Technologies Research · Advanced Battery Materials and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Noh · J. Power Sources · 2013 · 233 · 12110.1016/j.jpowsour.2013.01.063 ↗
2. Ouyang · J. Power Sources · 2015 · 279 · 62610.1016/j.jpowsour.2015.01.051 ↗
3. Wen · Mater. Express · 2012 · 210.1166/mex.2012.1075 ↗
4. Wen · J. Power Sources · 2014 · 264 · 15510.1016/j.jpowsour.2014.04.077 ↗
5. Lamb · J. Power Sources · 2014 · 247 · 101110.1016/j.jpowsour.2013.08.044 ↗
6. Narayana · ChemPhysChem · 2015 · 16 · 117910.1002/cphc.201402674 ↗
7. Yuan · Electrochim. Acta · 2015 · 178 · 68210.1016/j.electacta.2015.07.147 ↗
8. Makimura · J. Electrochem. Soc. · 2016 · 163 · A145010.1149/2.1171607jes ↗
9. Cui · J. Solid State Electrochem. · 2012 · 16 · 26510.1007/s10008-011-1316-9 ↗
10. Golubkov · RSC Adv. · 2015 · 5 · 5717110.1039/C5RA05897J ↗
11. Leising · J. Electrochem. Soc. · 2001 · 148 · A83810.1149/1.1379740 ↗
12. Xu · J. Electrochem. Soc. · 2012 · 159 · A67810.1149/2.024206jes ↗
13. Larsson · J. Electrochem. Soc. · 2014 · 161 · A161110.1149/2.0311410jes ↗
14. Liu · J. Electrochem. Soc. · 2015 · 162 · A220810.1149/2.0911510jes ↗
15. Lu · J. Electrochem. Soc. · 2014 · 159 · A56610.1149/2.jes035205 ↗
16. Arai · J. Electrochem. Soc. · 2015 · 162 · A95210.1149/2.0411506jes ↗
17. Devie · J. Electrochem. Soc. · 2015 · 162 · A103310.1149/2.0941506jes ↗
18. I. Bloom, et al., Effect of overcharge on Li(Ni0.5Mn0.3Co0.2)O2/graphite lithium ion cells with poly(vinylidene fluoride) binder. II - Chemical changes in the anode, (2017). [unpublished manuscript].
19. J. Bareno, et al., Effect of overcharge on Li(Ni0.5Mn0.3Co0.2)O2/graphite lithium ion cells with poly(vinylidene fluoride) binder. III - Chemical changes in the cathode, (2017). [unpublished manuscript].10.1016/j.jpowsour.2017.12.061 ↗
20. Li · MRS Adv. · 2016 · 1 · 102910.1557/adv.2016.6 ↗
21. Howe · J. Mater. Sci. · 2012 · 47 · 157210.1007/s10853-011-6029-z ↗
22. Orsini · J. Power Sources · 1998 · 76 · 1910.1016/S0378-7753(98)00128-1 ↗
23. Lithium metal anodes and rechargeable lithium metal batteries10.1007/978-3-319-44054-5 ↗
24. Steiger · J. Power Sources · 2014 · 261 · 11210.1016/j.jpowsour.2014.03.029 ↗
25. Bouchet · Nat. Nanotechnol. · 2014 · 9 · 57210.1038/nnano.2014.165 ↗
26. Below · J. Solid State Electrochem. · 2008 · 12 · 88510.1007/s10008-007-0449-3 ↗
27. Bang · J. Electrochem. Soc. · 2006 · 153 · A73110.1149/1.2171828 ↗
28. Yuan · Electrochim. Acta · 2015 · 178 · 68210.1016/j.electacta.2015.07.147 ↗
29. Aurbach · Solid State Ionics · 2002 · 148 · 40510.1016/S0167-2738(02)00080-2 ↗
30. Aurback · J. Power Sources · 2000 · 89 · 20610.1016/S0378-7753(00)00431-6 ↗
31. Zane · J. Power Sources · 2001 · 97–98 · 14610.1016/S0378-7753(01)00526-2 ↗
32. An · Carbon · 2016 · 105 · 5210.1016/j.carbon.2016.04.008 ↗
33. Lu · Adv. Energy Mater. · 2015 · 5 · 140099310.1002/aenm.201400993 ↗
34. Spotnitz · J. Power Sources · 2003 · 113 · 8110.1016/S0378-7753(02)00488-3 ↗
35. Verma · Electrochim. Acta · 2010 · 55 · 633210.1016/j.electacta.2010.05.072 ↗