Long-term behaviour of solid oxide fuel cell interconnect materials in contact with Ni-mesh during exposure in simulated anode gas at 700 and 800 °C
Source abstract
Abstract
Abstract In the present study the long-term behaviour of two ferritic steels, Crofer 22 APU and Crofer 22H, in contact with a Ni-mesh during exposure in simulated anode gas, Ar–4%H 2 –2%H 2 O, at 700 and 800 °C for exposure times up to 3000 h was investigated. Ni diffusion from the Ni-mesh into the steel resulted in the formation of an austenitic zone whereas diffusion of iron and chromium from the steel into the Ni-mesh resulted in the formation of chromia base oxides in the Ni-mesh. Depending on the chemical composition of the steel, the temperature and the exposure time, interdiffusion processes between ferritic steel and Ni-mesh also resulted in σ -phase formation at the austenite–ferrite interface and in Laves-phase dissolution in the austenitic zone. The extent and morphology of the σ -phase formation are discussed on the basis of thermodynamic considerations, including reaction paths in the ternary alloy system Fe–Ni–Cr.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · High-Temperature Coating Behaviors · Fuel Cells and Related Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Zeng · Solid State Ionics · 2004 · 167 · 910.1016/j.ssi.2003.11.026 ↗
2. Yang · J. Electrochem. Soc. · 2003 · 150 · A118810.1149/1.1595659 ↗
3. Quadakkers · 1994 · 525
4. Quadakkers · Mater. High Temp. · 2003 · 20 · 115
5. Quadakkers · 2000 · 2 · 827
6. Huczkowski · Fuel Cells · 2006 · 6 · 9310.1002/fuce.200500110 ↗
7. Nielsen · 2002
8. Zhu · Mater. Sci. Eng. A · 2003 · 362 · 22810.1016/S0921-5093(03)00620-8 ↗
9. Huczkowski · J. Fuel Cell. Sci. Technol. · 2004 · 1 · 3010.1115/1.1782925 ↗
10. Huczkowski · Mater. Corros. · 2004 · 55 · 82510.1002/maco.200303798 ↗
11. Froitzheim · J. Fuel Cell. Sci. Technol. · 2010 · 710.1115/1.3182731 ↗
12. Niewolak · J. Electrochem. Soc. · 2012 · 159 · F72510.1149/2.033211jes ↗
13. Meulenberg · Oxid. Met. · 2002 · 57 · 110.1023/A:1013336510729 ↗
14. Nielsen · Fuel Cells · 2006 · 6 · 10010.1002/fuce.200500114 ↗
15. Shong · Mater. Chem. Phys. · 2012 · 134 · 67010.1016/j.matchemphys.2012.03.049 ↗
16. Hansson · J. Corros. Sci. Eng. · 2003 · 6 · 12
17. Froitzheim · 2008
18. Sarda · ECS Trans. · 2013 · 57 · 227910.1149/05701.2279ecst ↗
19. Leistikow · Werkst. Korros. · 1987 · 38 · 55610.1002/maco.19870381003 ↗
20. Thiele · Kraftwerkstechnik · 1997 · 2 · 143
21. Young · Corros. Sci. · 2011 · 53 · 213110.1016/j.corsci.2011.02.031 ↗
22. Singheiser · 2010 · vol. 1 · 482
23. Kajihara · Acta Metall. Mater. · 1995 · 43 · 80710.1016/0956-7151(94)00283-N ↗
24. Perkins · Metall. Trans. · 1973 · 4 · 253510.1007/BF02644255 ↗
25. Tokei · Appl. Surf. Sci. · 2000 · 165 · 2310.1016/S0169-4332(00)00285-3 ↗
26. Singhal · 2006
27. Hojda · 2003 · 20
28. Quadakkers · 2010
29. Asensio-Jimenez · Oxid. Met. · 2013 · 79 · 1510.1007/s11085-012-9323-5 ↗
30. Quadakkers · 2010 · vol. 1 · 407
31. Joubert · Prog. Mater. Sci. · 2008 · 53 · 52810.1016/j.pmatsci.2007.04.001 ↗
32. Zurek · Mater. Sci. Eng. A · 2008 · 477 · 25910.1016/j.msea.2007.05.035 ↗
33. Kuhn · Mater. Sci. Eng. A · 2011 · 528 · 588810.1016/j.msea.2011.03.112 ↗
34. Asensio · Electrochem. Solid State Lett. · 2011 · 14 · P1710.1149/1.3590258 ↗
35. Niewolak · Oxid. Met. · 2014 · 82 · 12310.1007/s11085-014-9481-8 ↗
36. MOB2 · 1999
37. Jansson · 1993 · 57
38. BT TTFE6 · 2009
39. Crofer® 22H, Material Data Sheet No. 4050, ThyssenKrupp VDM, June 2010.
40. Shemet · 2013
41. Meier · 2013 · 18