Effect of firing temperature on the microstructure and performance of PrBaCo2O5+δ cathodes on Sm0.2Ce0.8O1.9 electrolytes fabricated by spray deposition-firing processes
Source abstract
Abstract
Abstract The effect of firing temperature on the microstructure and performance of PrBaCo 2 O 5+ δ cathodes on Sm 0.2 Ce 0.8 O 1.9 electrolytes fabricated by spray deposition-firing processes is systematically studied by various characterization techniques. The grain size, porosity and particle connection of the electrode as well as the physical contact between the PrBaCo 2 O 5+ δ and Sm 0.2 Ce 0.8 O 1.9 layers are influenced differently by the firing temperature. The area specific resistances (ASRs) of the various PrBaCo 2 O 5+ δ cathodes are measured by electrochemical impedance spectroscopy in both symmetrical two-electrode and three-electrode configurations. The lowest ASR and cathode overpotential are achieved at a firing temperature of 1000 °C. Two main oxygen reduction reaction processes are proposed according to the oxygen partial pressure dependence of the electrode ASR. The rate-determining step is transmitted from a charge-transfer process at low firing temperatures to a non-charge-transfer process at high firing temperatures. A fuel cell with the PrBaCo 2 O 5+ δ cathode fired at an optimal temperature of 1000 °C delivers the attractive peak power density of 835 mW cm −2 at 650 °C, while this density is much lower for other firing temperatures. This result suggests the firing temperature of PrBaCo 2 O 5+ δ electrodes should be carefully optimized for practical applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Magnetic and transport properties of perovskites and related materials · Electronic and Structural Properties of Oxides
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Steele · Nature · 2001 · 414 · 34510.1038/35104620 ↗
2. Brandon · Annu. Rev. Mater. Res. · 2003 · 33 · 18310.1146/annurev.matsci.33.022802.094122 ↗
3. Fleig · Fuel Cells · 2006 · 6 · 28410.1002/fuce.200500209 ↗
4. Minh · J. Am. Ceram. Soc. · 1993 · 76 · 56310.1111/j.1151-2916.1993.tb03645.x ↗
5. Mogensen · Solid State Ionics · 1996 · 86–88 · 115110.1016/0167-2738(96)00280-9 ↗
6. Ralph · J. Electrochem. Soc. · 2003 · 150 · A151810.1149/1.1617300 ↗
7. Lee · J. Electrochem. Soc. · 2006 · 153 · A79410.1149/1.2172572 ↗
8. Hansen · Solid State Ionics · 2007 · 178 · 137910.1016/j.ssi.2007.07.012 ↗
9. Zhou · Electrochem. Commun. · 2008 · 10 · 164710.1016/j.elecom.2008.08.033 ↗
10. Leng · Solid State Ionics · 2004 · 170 · 910.1016/j.ssi.2004.02.026 ↗
11. Leng · Int. J. Hydrogen Energy · 2008 · 33 · 380810.1016/j.ijhydene.2008.04.034 ↗
12. Murray · Solid State Ionics · 2002 · 148 · 2710.1016/S0167-2738(02)00102-9 ↗
13. Wang · Solid State Ionics · 2005 · 176 · 45710.1016/j.ssi.2004.09.007 ↗
14. Bebelis · J. Appl. Electrochem. · 2007 · 37 · 1510.1007/s10800-006-9215-y ↗
15. Peña-Martínez · Electrochim. Acta · 2007 · 52 · 295010.1016/j.electacta.2006.09.004 ↗
16. Zhang · J. Power Sources · 2006 · 160 · 121110.1016/j.jpowsour.2006.03.035 ↗
17. Lv · Solid State Ionics · 2006 · 177 · 90110.1016/j.ssi.2006.01.038 ↗
18. Shao · Nature · 2004 · 431 · 17010.1038/nature02863 ↗
19. Peña-Martínez · Solid State Ionics · 2006 · 177 · 214310.1016/j.ssi.2006.05.042 ↗
20. Chen · Electrochim. Acta · 2007 · 52 · 734310.1016/j.electacta.2007.06.010 ↗
21. Zhou · Acta Mater. · 2008 · 56 · 268710.1016/j.actamat.2008.02.002 ↗
22. Zhao · J. Power Sources · 2008 · 182 · 50310.1016/j.jpowsour.2008.04.046 ↗
23. Taskin · Appl. Phys. Lett. · 2005 · 86 · 09191010.1063/1.1864244 ↗
24. Kim · Appl. Phys. Lett. · 2006 · 88 · 02410310.1063/1.2163257 ↗
25. Chang · Solid State Ionics · 2006 · 177 · 200910.1016/j.ssi.2006.05.047 ↗
26. Tarancon · J. Mater. Chem. · 2007 · 17 · 317510.1039/b704320a ↗
27. Taskin · Prog. Solid State Chem. · 2007 · 35 · 48110.1016/j.progsolidstchem.2007.01.014 ↗
28. Kim · J. Mater. Chem. · 2007 · 17 · 250010.1039/b618345j ↗
29. Tarancon · J. Power Sources · 2007 · 174 · 25510.1016/j.jpowsour.2007.08.077 ↗
30. Zhang · Acta Mater. · 2008 · 56 · 487610.1016/j.actamat.2008.06.004 ↗
31. Kim · J. Power Sources · 2009 · 194 · 70410.1016/j.jpowsour.2009.06.024 ↗
32. Kim · J. Electrochem. Soc. · 2008 · 155 · B38510.1149/1.2839028 ↗
33. Chen · J. Power Sources · 2009 · 188 · 9610.1016/j.jpowsour.2008.11.045 ↗
34. Gu · Electrochim. Acta · 2009 · 54 · 709410.1016/j.electacta.2009.07.040 ↗
35. Zhou · J. Power Sources · 2010 · 195 · 217410.1016/j.jpowsour.2009.10.062 ↗
36. Deng · Chem. Mater. · 2009 · 21 · 515410.1021/cm902094q ↗
37. Jorgensen · Solid State Ionics · 2001 · 139 · 110.1016/S0167-2738(00)00818-3 ↗
38. Murata · J. Power Sources · 2005 · 145 · 25710.1016/j.jpowsour.2004.12.063 ↗
39. Virkar · Solid State Ionics · 2000 · 131 · 18910.1016/S0167-2738(00)00633-0 ↗
40. Mitterdorfer · Solid State Ionics · 1998 · 111 · 18510.1016/S0167-2738(98)00195-7 ↗
41. Adler · J. Electrochem. Soc. · 1996 · 143 · 355410.1149/1.1837252 ↗
42. Adler · Solid State Ionics · 1998 · 111 · 12510.1016/S0167-2738(98)00179-9 ↗
43. Zhou · J. Electrochem. Soc. · 2009 · 156 · B88410.1149/1.3139044 ↗
44. Escudero · J. Electroanal. Chem. · 2007 · 611 · 10710.1016/j.jelechem.2007.08.006 ↗
45. Jorgensen · J. Electrochem. Soc. · 2001 · 148 · A43310.1149/1.1360203 ↗