Evolution of the LiFePO4 positive electrode interface along cycling monitored by MAS NMR

Marine Cuisinier, Nicolas Dupré, Jean-Frédéric Martin, Ryoji Kanno, Dominique Guyomard

Publisher page

Abstract

Abstract Decreasing particle size ensures a good accessibility of LiFePO 4 to lithium ions and electrons and allows reaching the theoretical capacity and achieving high cycling rates. It nevertheless leads to an increase of the surface area and thus a subsequent amplification of the parasitic reactions at the interface between active material surface and electrolyte. The formation and evolution of the interphase on the surface of LiFePO 4 may affect strongly its electrochemical performance. This work aims at monitoring the interphase forming on LiFePO 4 upon its operation in a lithium battery, and correlating its evolution with the electrochemical behaviour of the active material. Combined XPS and multinuclear quantitative 7 Li, 1 H and 19 F NMR indicate a trend for the interphase structure that can be described as a mostly stable inner interphase composed of fluorinated inorganic products while outer lithiated organic species undergo a reversible formation at high potential and dissolution at low potential. Although an irreversible accumulation of interphase occurs, spin–spin relaxation time analysis indicates that interphasial species tend to stack on the top of each other rather than cover the whole active material surface. Moreover, the dissolution/precipitation process seems to prevent a blocking of the electrode surface by resistive species such as LiF.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Padhi · J. Electrochem. Soc. · 1997 · 144 · 118810.1149/1.1837571 ↗
2. Li · Adv. Mater. · 2005 · 17 · 98410.1002/adma.200400695 ↗
3. Nagata · J. Power Sources · 2005 · 146 · 76210.1016/j.jpowsour.2005.03.156 ↗
4. Tao · Rare Metals · 2007 · 27 · 280
5. Streltsov · Acta Crystallogr. · 1993 · B49 · 14710.1107/S0108768192004701 ↗
6. Huang · Electrochem. Solid-State Lett. · 2001 · 4 · A17010.1149/1.1396695 ↗
7. Mi · Mater. Lett. · 2005 · 59 · 12710.1016/j.matlet.2004.07.051 ↗
8. Yun · J. Power Sources · 2006 · 160 · 136110.1016/j.jpowsour.2006.02.097 ↗
9. Dominko · J. Electrochem. Soc. · 2005 · 152 · A60710.1149/1.1860492 ↗
10. Chung · Nat. Mater. · 2002 · 1 · 12310.1038/nmat732 ↗
11. Delacourt · J. Electrochem. Soc. · 2005 · 152 · A91310.1149/1.1884787 ↗
12. Yamada · J. Electrochem. Soc. · 2001 · 148 · A22410.1149/1.1348257 ↗
13. Aurbach · J. Power Sources · 1999 · 95 · 81
14. Aurbach · J. Power Sources · 2007 · 165 · 49110.1016/j.jpowsour.2006.10.025 ↗
15. Thomas · J. Electrochem. Soc. · 1985 · 132 · 152110.1149/1.2114158 ↗
16. Levi · J. Electrochem. Soc. · 1999 · 146 · 127610.1149/1.1391759 ↗
17. Chen · J. Power Sources · 2001 · 96 · 32110.1016/S0378-7753(00)00666-2 ↗
18. Aurbach · J. Power Sources · 2006 · 162 · 78010.1016/j.jpowsour.2005.07.009 ↗
19. Edström · Electrochim. Acta · 2004 · 50 · 39710.1016/j.electacta.2004.03.049 ↗
20. Eriksson · Langmuir · 2002 · 18 · 360910.1021/la011354m ↗
21. Nyten · J. Mater. Chem. · 2006 · 16 · 348310.1039/B605578H ↗
22. Herstedt · Electrochem. Solid-state Lett. · 2003 · 6 · A20210.1149/1.1594413 ↗
23. Dupré · J. Mater. Chem. · 2008 · 18 · 426610.1039/b807778a ↗
24. Dupré · Electrochem. Commun. · 2008 · 10 · 189710.1016/j.elecom.2008.10.004 ↗
25. Dupré · J. Power Sources · 2010 · 195 · 741510.1016/j.jpowsour.2010.05.042 ↗
26. Dupré · J. Power Sources · 2011 · 196 · 479110.1016/j.jpowsour.2010.07.049 ↗
27. Martin · Electrochem. Solid-State Lett. · 2007 · 11 · A1210.1149/1.2801016 ↗
28. Cuisinier · Electrochem. Commun. · 2010 · 12 · 23810.1016/j.elecom.2009.12.003 ↗
29. Martin · J. Power Sources · 2011 · 196 · 215510.1016/j.jpowsour.2010.09.120 ↗
30. Cuisinier · J. Mater. Chem. · 2011 · 21 · 1857510.1039/c1jm12649k ↗
31. Koltypin · J. Power Sources · 2007 · 174 · 124110.1016/j.jpowsour.2007.06.045 ↗
32. Ménétrier · Electrochem. Solid-State Lett. · 2004 · 7 · A14010.1149/1.1697905 ↗
33. Cuisinier · Solid State Nucl. Magn. Reson. · 2012 · 42 · 5110.1016/j.ssnmr.2011.09.001 ↗
34. D. Massiot. http://nmr.cemhti.cnrs-orleans.fr/dmfit/.
35. Grey · Chem. Rev. · 2004 · 104 · 449310.1021/cr020734p ↗
36. Dupré · J. Electrochem. Soc. · 2009 · 156 · C18010.1149/1.3098494 ↗
37. Nayeem · J. Chem. Phys. · 1988 · 89 · 460010.1063/1.454800 ↗
38. Davis · Phys. Chem. Chem. Phys. · 2011 · 13 · 517110.1039/c0cp01922d ↗
39. Swift · 1973 · 53
40. Kohler · 2001 · vol. 1 · 386
41. Chen · J. Electrochem. Soc. · 2002 · 149 · A118410.1149/1.1498255 ↗
42. Kim · Electrochem. Solid-State Lett. · 2006 · 9 · A43910.1149/1.2218308 ↗
43. Eshkenazi · Solid State Ionics · 2004 · 170 · 8310.1016/S0167-2738(03)00107-3 ↗
44. Dedryvère · J. Electrochem. Soc. · 2005 · 152 · A68910.1149/1.1861994 ↗
45. Aurbach · Langmuir · 1996 · 12 · 399110.1021/la9600762 ↗
46. Kang · J. Power Sources · 2008 · 175 · 52610.1016/j.jpowsour.2007.08.112 ↗
47. Scrocco · Phys. Rev. B · 1985 · 32 · 130610.1103/PhysRevB.32.1306 ↗
48. Ait-Salah · Z. Anorg. Allg. Chem. · 2006 · 632 · 159810.1002/zaac.200600090 ↗
49. Plakhotnyk · J. Fluorine Chem. · 2005 · 126 · 2710.1016/j.jfluchem.2004.09.027 ↗
50. Thevenin · J. Electrochem. Soc. · 1987 · 134 · 27310.1149/1.2100445 ↗