Abstract

Abstract Water management in polymer–electrolyte membrane fuel cells (PEMFCs) has a major impact on fuel cell performance and durability. To investigate the two-phase flow patterns in PEMFC gas flow channels, the volume of fluid (VOF) method was employed to simulate the air–water flow in a 3D cuboid channel with a 1.0 mm × 1.0 mm square cross section and a 100 mm in length. The microstructure of gas diffusion layers (GDLs) was simplified by a number of representative opening pores on the 2D GDL surface. Water was injected from those pores to simulate water generation by the electrochemical reaction at the cathode side. Operating conditions and material properties were selected according to realistic fuel cell operating conditions. The water injection rate was also amplified 10 times, 100 times and 1000 times to study the flow pattern formation and transition in the channel. Simulation results show that, as the flow develops, the flow pattern evolves from corner droplet flow to top wall film flow, then annular flow, and finally slug flow. The total pressure drop increases exponentially with the increase in water volume fraction, which suggests that water accumulation should be avoided to reduce parasitic energy loss. The effect of material wettability was also studied by changing the contact angle of the GDL surface and channel walls, separately. It is shown that using a more hydrophobic GDL surface is helpful to expel water from the GDL surface, but increases the pressure drop. Using a more hydrophilic channel wall reduces the pressure drop, but increases the water residence time and water coverage of the GDL surface.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advancements in Solid Oxide Fuel Cells

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Anderson · J. Power Sources · 2010 · 195 · 453110.1016/j.jpowsour.2009.12.123 ↗
2. Liu · Int. J. Hydrogen Energy · 2008 · 33 · 1040
3. Hussaini · J. Power Sources · 2009 · 187 · 44410.1016/j.jpowsour.2008.11.030 ↗
4. Dunbar · J. Power Sources · 2008 · 182 · 7610.1016/j.jpowsour.2008.03.057 ↗
5. Lu · Int. J. Hydrogen Energy · 2009 · 34 · 344510.1016/j.ijhydene.2008.12.025 ↗
6. Zhang · J. Power Sources · 2010 · 195 · 323110.1016/j.jpowsour.2009.11.113 ↗
7. Zhang · J. Power Sources · 2008 · 183 · 64310.1016/j.jpowsour.2008.05.080 ↗
8. Zhang · J. Power Sources · 2009 · 189 · 102310.1016/j.jpowsour.2009.01.010 ↗
9. Anderson · J. Power Sources · 2010 · 195 · 416810.1016/j.jpowsour.2009.12.134 ↗
10. Chen · J. Power Sources · 2010 · 195 · 112210.1016/j.jpowsour.2009.09.004 ↗
11. Bazylak · Int. J. Hydrogen Energy · 2009 · 34 · 384510.1016/j.ijhydene.2009.02.084 ↗
12. Weber · Chem. Rev. · 2004 · 104 · 467910.1021/cr020729l ↗
13. Wang · Chem. Rev. · 2004 · 104 · 472710.1021/cr020718s ↗
14. Wang · J. Power Sources · 2001 · 94 · 4010.1016/S0378-7753(00)00662-5 ↗
15. Mazumder · J. Electrochem. Soc. · 2003 · 150 · A150310.1149/1.1615608 ↗
16. Berning · J. Electrochem. Soc. · 2003 · 150 · A158910.1149/1.1621412 ↗
17. Gurau · J. Electrochem. Soc. · 2010 · 157 · B51210.1149/1.3294708 ↗
18. Quan · J. Power Sources · 2005 · 152 · 13110.1016/j.jpowsour.2005.02.075 ↗
19. Theodorakakos · J. Colloid Interface Sci. · 2006 · 300 · 67310.1016/j.jcis.2006.04.021 ↗
20. Zhan · J. Power Sources · 2006 · 160 · 110.1016/j.jpowsour.2005.12.081 ↗
21. Shirani · J. Fuel Cell Sci. Technol. · 2008 · 5 · 04100810.1115/1.2930774 ↗
22. Cai · J. Power Sources · 2006 · 161 · 84310.1016/j.jpowsour.2006.04.110 ↗
23. Zhu · J. Power Sources · 2007 · 172 · 28710.1016/j.jpowsour.2007.07.024 ↗
24. Bazylak · J. Power Sources · 2008 · 176 · 24010.1016/j.jpowsour.2007.10.066 ↗
25. Zhu · Microfluid. Nanofluid. · 2008 · 4 · 54310.1007/s10404-007-0209-9 ↗
26. Zhu · J. Power Sources · 2008 · 181 · 10110.1016/j.jpowsour.2008.03.005 ↗
27. Fang · Int. J. Multiphase Flow · 2008 · 34 · 69010.1016/j.ijmultiphaseflow.2007.08.008 ↗
28. Quan · J. Power Sources · 2005 · 152 · 13110.1016/j.jpowsour.2005.02.075 ↗
29. Jiao · J. Power Sources · 2006 · 154 · 12410.1016/j.jpowsour.2005.04.003 ↗
30. Jiao · J. Power Sources · 2006 · 157 · 22610.1016/j.jpowsour.2005.06.041 ↗
31. Quan · J. Power Sources · 2007 · 164 · 22210.1016/j.jpowsour.2006.09.110 ↗
32. Le · J. Power Sources · 2008 · 182 · 19710.1016/j.jpowsour.2008.03.047 ↗
33. Le · Electrochim. Acta · 2009 · 54 · 213710.1016/j.electacta.2008.10.029 ↗
34. Ding · J. Power Sources · 2010 · 195 · 727810.1016/j.jpowsour.2010.05.059 ↗
35. Sundén · 2005
36. FLUENT 6.3 UDF Manual, 2006
37. Le · J. Power Sources · 2010 · 195 · 730210.1016/j.jpowsour.2010.05.045 ↗
38. Bevers · J. Power Sources · 1996 · 63 · 19310.1016/S0378-7753(96)02465-2 ↗
39. Lim · Electrochim. Acta · 2004 · 49 · 414910.1016/j.electacta.2004.04.009 ↗