The influence of the pyrolysis temperature on the electrochemical behavior of carbon-rich SiCN polymer-derived ceramics as anode materials in lithium-ion batteries
Source abstract
Abstract
Abstract Within this study we report on the impact of the pyrolysis temperature on the structural and electrochemical properties of the poly(phenylvinylsilylcarbodiimide) derived silicon carbonitride (SiCN) ceramic. Materials pyrolysed at 800 °C and 1300 °C, SiCN 800 and SiCN 1300, are found amorphous. Raman spectroscopy measurements indicate the increase in ordering of the free carbon phase with increasing pyrolysis temperature which leads to lower capacity recovered by SiCN 1300. Significant hysteresis is found for materials pyrolysed at 800 °C during electrochemical lithium insertion/extraction. This feature is attributed to much higher hydrogen content in SiCN 800 sample. An aging of SiCN 800 reflected by a change of elemental composition upon contact to air and a strong film formation are attenuated at a higher pyrolysis temperature. Single particle microelectrode investigation on SiCN 800 and SiCN 1300 clarify different electrochemical behavior of the materials. Much lower charge transfer resistance of SiCN 1300 in comparison to SiCN 800 explains better high currents electrochemical performance. Lithium ions diffusion coefficient Dmin ranges from 3.2 10 −9 cm 2 s −1 to 6.4 10–11 cm 2 s −1 and is independent on the potential.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced ceramic materials synthesis · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. J.R. Dahn, A.M. Wilson, W. Xing, G.A. Zank, inventors; Dow Corning Corp., assignee, Electrodes for lithium ion batteries using polysilazanes ceramic with lithium, United States Patent US 5631106(A), 1997, May 20.
2. Xing · J. Electrochem Soc. · 1997 · 144 · 241010.1149/1.1837828 ↗
3. Fukui · Acs Appl. Mater. Inter · 2010 · 2 · 99810.1021/am100030f ↗
4. Sanchez-Jimenez · J. Am. Ceram. Soc. · 2010 · 93 · 112710.1111/j.1551-2916.2009.03539.x ↗
5. Graczyk-Zajac · J. Eur. Ceram. Soc. · 2010 · 30 · 323510.1016/j.jeurceramsoc.2010.07.010 ↗
6. Kaspar · Electrochimica Acta · 2010 · 56 · 17410.1016/j.electacta.2010.08.103 ↗
7. Reinold · J. Power Sources · 2013 · 236 · 22410.1016/j.jpowsour.2013.02.046 ↗
8. Baek · J. Power Sources · 2014 · 253 · 34210.1016/j.jpowsour.2013.12.065 ↗
9. Colombo · J. Am. Ceram. Soc. · 2010 · 93 · 180510.1111/j.1551-2916.2010.03876.x ↗
10. Mera · J. Mater. Chem. A · 2013 · 1 · 382610.1039/c2ta00727d ↗
11. Kaspar · J. Power Sources · 2013 · 244 · 45010.1016/j.jpowsour.2012.11.086 ↗
12. Fukui · J. Power Sources · 2013 · 243 · 15210.1016/j.jpowsour.2013.05.124 ↗
13. Su · J. Am. Ceram. Soc. · 2009 · 92 · 296210.1111/j.1551-2916.2009.03317.x ↗
14. Mera · J. Eur. Ceram. Soc. · 2009 · 29 · 287310.1016/j.jeurceramsoc.2009.03.026 ↗
15. Widgeon · Chem. Mater. · 2012 · 24 · 118110.1021/cm2038238 ↗
16. Janakiraman · J. Eur. Ceram. Soc. · 2009 · 29 · 16310.1016/j.jeurceramsoc.2008.05.028 ↗
17. Bard · 1980
18. Ahn · J. Power Sources · 2011 · 196 · 217910.1016/j.jpowsour.2010.09.086 ↗
19. Widgeon · Chem. Mater. · 2010 · 22 · 622110.1021/cm1021432 ↗
20. Bonino · Electrochim Acta · 2006 · 51 · 340710.1016/j.electacta.2005.09.036 ↗
21. Sadezky · Carbon · 2005 · 43 · 173110.1016/j.carbon.2005.02.018 ↗
22. Tuinstra · J. Chem. Phys. · 1970 · 53
23. Dippel · Phys. Chem. Chem. Phys. · 1999 · 1 · 470710.1039/a904529e ↗
24. Ferrari · Phys. Rev. B · 2000 · 61 · 1409510.1103/PhysRevB.61.14095 ↗
25. Ferrari · Phys. Rev. B · 2001 · 6410.1103/PhysRevB.64.075414 ↗
26. Pradeep · Electrochim Acta · 2014 · 119 · 7810.1016/j.electacta.2013.12.037 ↗
27. Zheng · Chem. Mater. · 1996 · 8 · 38910.1021/cm950304y ↗
28. Zheng · J. Electrochem Soc. · 1996 · 143 · 213710.1149/1.1836972 ↗
29. Reinold · J. Power Sources · 2013 · 236 · 22410.1016/j.jpowsour.2013.02.046 ↗
30. Liu · Carbon · 1996 · 34 · 19310.1016/0008-6223(96)00177-7 ↗
31. Zheng · J. Electrochem Soc. · 1995 · 142 · 258110.1149/1.2050057 ↗
32. Fukui · Acs Appl. Mater. Inter · 2011 · 3 · 231810.1021/am2002422 ↗
33. Claye · Electrochim Acta · 1999 · 45 · 10710.1016/S0013-4686(99)00197-8 ↗
34. Shah · Acta Mater. · 2002 · 50 · 409310.1016/S1359-6454(02)00206-9 ↗
35. Nishimura · J. Mater. Sci. · 1998 · 33 · 523710.1023/A:1004440122266 ↗
36. Kaspar · Electrochim Acta · 2014 · 115 · 66510.1016/j.electacta.2013.10.184 ↗
37. Dokko · J. Phys. Chem. C · 2010 · 114 · 864610.1021/jp101166d ↗
38. Dokko · J. Power Sources · 2009 · 189 · 78310.1016/j.jpowsour.2008.07.081 ↗
39. Munakata · J. Power Sources · 2012 · 217 · 44410.1016/j.jpowsour.2012.06.037 ↗
40. Gao · 2014
41. Trassl · J. Eur. Ceram. Soc. · 2003 · 23 · 78110.1016/S0955-2219(02)00155-3 ↗
42. Haluschka · J. Eur. Ceram. Soc. · 2000 · 20 · 136510.1016/S0955-2219(00)00009-1 ↗