Improved thermal stability of lithium ion battery by using cresyl diphenyl phosphate as an electrolyte additive

Qingsong Wang, Ping Ping, Jinhua Sun, Chunhua Chen

Journal of Power Sources· Volume 195· Issue 21
Publisher page

Abstract

Abstract To enhance the safety of lithium ion battery, cresyl diphenyl phosphate (CDP) is explored as an additive in 1.0 M LiPF 6 /ethylene carbonate (EC) + diethyl carbonate (DEC) (1:1 wt.). The electrochemical performances of LiCoO 2 /CDP-electrolyte/C cells are tested. At the thermal aspect, the thermal stability of the electrolyte with CDP is detected firstly by using a C80 micro-calorimeter, and then the charged LiCoO 2 /CDP-electrolyte/C cells are disassembled and wrapped to detect the thermal behaviors. The results indicate that CDP-containing electrolyte enhances the thermal stabilities of electrolyte and lithium ion battery, and the electrochemical performances of LiCoO 2 /CDP-electrolyte/C cell become slightly worse by using CDP in the electrolyte. Furthermore, the cell with 10% (wt.) CDP-containing electrolyte shows better cycle efficiency than that of other CDP-containing electrolyte, such as containing 5% (wt.) CDP and 15% (wt.) CDP. This maybe because that the mass ratio between CDP and electrolyte is close to the reaction stoichiometric ratio in the 10% (wt.) CDP-containing electrolyte, where stable solid electrolyte interphase (SEI) is formed. Therefore, 10% CDP-containing electrolyte improves the safety of lithium ion battery and keeps its electrochemical performance.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Biensan · J. Power Sources · 1999 · 82 · 90610.1016/S0378-7753(99)00135-4 ↗
2. Tobishima · J. Power Sources · 1999 · 82 · 88210.1016/S0378-7753(98)00240-7 ↗
3. Doh · J. Power Sources · 2008 · 175 · 88110.1016/j.jpowsour.2007.09.102 ↗
4. Chen · Electrochim. Acta · 2009 · 54 · 560510.1016/j.electacta.2009.05.017 ↗
5. Balakrishnan · J. Power Sources · 2006 · 155 · 40110.1016/j.jpowsour.2005.12.002 ↗
6. Zhang · J. Power Sources · 2006 · 162 · 137910.1016/j.jpowsour.2006.07.074 ↗
7. Y. Qin, Z. H. Chen, J. Liu, K. Amine, Electrochem. Solid State 13 (2010) A11–A14.10.1149/1.3261738 ↗
8. Shim · J. Power Sources · 2008 · 175 · 53310.1016/j.jpowsour.2007.08.098 ↗
9. Nam · J. Power Sources · 2008 · 180 · 56110.1016/j.jpowsour.2008.01.061 ↗
10. Shim · Electrochim. Acta · 2009 · 54 · 227610.1016/j.electacta.2008.10.037 ↗
11. Chen · J. Power Sources · 2009 · 187 · 22910.1016/j.jpowsour.2008.10.091 ↗
12. Feng · Electrochim. Acta · 2008 · 53 · 826510.1016/j.electacta.2008.05.024 ↗
13. Xiang · J. Power Sources · 2007 · 173 · 56210.1016/j.jpowsour.2007.05.001 ↗
14. Shim · Met. Mater. Int. · 2009 · 15 · 61510.1007/s12540-009-0615-5 ↗
15. Zhou · J. Power Sources · 2008 · 184 · 58910.1016/j.jpowsour.2008.03.008 ↗
16. Wang · Mater. Lett. · 2007 · 61 · 333810.1016/j.matlet.2006.11.060 ↗
17. Zhang · J. Power Sources · 2003 · 113 · 16610.1016/S0378-7753(02)00537-2 ↗
18. Wang · Electrochem. Solid State · 2005 · 8 · A46710.1149/1.1993389 ↗
19. Yao · J. Power Sources · 2005 · 144 · 17010.1016/j.jpowsour.2004.11.042 ↗
20. Wang · Thermochim. Acta · 2005 · 437 · 1210.1016/j.tca.2005.06.010 ↗
21. Venugopal · J. Power Sources · 2001 · 101 · 23110.1016/S0378-7753(01)00782-0 ↗
22. Wang · J. Electrochem. Soc. · 2006 · 153 · A32910.1149/1.2139955 ↗