journal article·2009-06

Proton-exchange-membrane fuel cells durability evaluated by load-on/off cycling

G.J.M. Janssen, E.F. Sitters, A. Pfrang

Journal of Power Sources· Volume 191· Issue 2
Publisher page

Abstract

Abstract Load-on/off cycles at 80 °C, with near-saturated H 2 and air at ambient pressure were applied to investigate the durability of several types of membrane-electrode-assemblies (MEAs) for proton-exchange-membrane fuel cells (PEMFC). The ohmic resistance, H 2 cross-over, electrochemically active surface area (ECSA), protonic resistance of the cathode as well as the performances with H 2 /air and H 2 /O 2 were measured at regular intervals. These data enabled a breakdown of the increase in cell voltage losses upon cycling. Increase of kinetic losses was found in all MEAs but significant differences were obtained for the transport losses in the cathode catalyst layer, which either had a small or a substantial contribution to the overall voltage decay, depending on the carbon type and ionomer loading. Membrane degradation did not contribute significantly in these tests.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advanced battery technologies research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Mathias · Electrochem. Soc.-Interface · 2005 · 14 · 2410.1149/2.F05053IF ↗
2. Garland · ECS Trans. · 2007 · 11 · 92310.1149/1.2781004 ↗
3. Borup · Chem. Rev. · 2007 · 107 · 390410.1021/cr050182l ↗
4. de Bruijn · Fuel Cells · 2008 · 8 · 310.1002/fuce.200700053 ↗
5. Ferreira · J. Electrochem. Soc. · 2005 · 152 · A225610.1149/1.2050347 ↗
6. Aoki · Electrochem. Commun. · 2005 · 7 · 143410.1016/j.elecom.2005.10.008 ↗
7. Mittal · J. Electrochem. Soc. · 2007 · 154 · B65210.1149/1.2734869 ↗
8. Mittal · J. Electrochem. Soc. · 2006 · 153 · A175510.1149/1.2219708 ↗
9. Mittal · Electrochem. Solid-State Lett. · 2006 · 9 · A29910.1149/1.2192696 ↗
10. Liu · ECS Trans. · 2006 · 1 · 28310.1149/1.2214561 ↗
11. Guilminot · J. Electrochem. Soc. · 2007 · 154 · B110610.1149/1.2775218 ↗
12. Cleghorn · J. Power Sources · 2006 · 158 · 410.1016/j.jpowsour.2005.09.062 ↗
13. Xie · J. Electrochem. Soc. · 2005 · 152 · A10410.1149/1.1830355 ↗
14. Lee · J. Electrochem. Soc. · 2007 · 154 · B19410.1149/1.2403083 ↗
15. Reiser · Electrochem. Solid-State Lett. · 2005 · 8 · A27310.1149/1.1896466 ↗
16. Gasteiger · J. Power Sources · 2004 · 127 · 16210.1016/j.jpowsour.2003.09.013 ↗
17. Neyerlin · J. Electrochem. Soc. · 2007 · 154 · B63110.1149/1.2733987 ↗
18. Zhang · J. Power Sources · 2006 · 163 · 53210.1016/j.jpowsour.2006.09.026 ↗
19. Gasteiger · 2003 · vol. 3 · 593
20. Kocha · 2003 · vol. 3 · 538
21. Janssen · J. Power Sources · 2007 · 171 · 810.1016/j.jpowsour.2006.11.008 ↗
22. Eikerling · J. Electroanal. Chem. · 1998 · 453 · 8910.1016/S0022-0728(98)00214-9 ↗
23. Perry · J. Electrochem. Soc. · 1998 · 145 · 510.1149/1.1838202 ↗
24. Springer · J. Electrochem. Soc. · 1993 · 140 · 351310.1149/1.2221120 ↗
25. Neyerlin · J. Electrochem. Soc. · 2006 · 153 · A195510.1149/1.2266294 ↗
26. Eikerling · J. Electroanal. Chem. · 1999 · 475 · 10710.1016/S0022-0728(99)00335-6 ↗
27. Lefebvre · Electrochem. Solid-State Lett. · 1999 · 2 · 25910.1149/1.1390804 ↗
28. Makharia · J. Electrochem. Soc. · 2005 · 152 · A97010.1149/1.1888367 ↗
29. Hoare · J. Electrochem. Soc. · 1962 · 109 · 85810.1149/1.2425569 ↗
30. Gasteiger · Appl. Catal. B: Environ. · 2005 · 56 · 910.1016/j.apcatb.2004.06.021 ↗
31. Ball · J. Power Sources · 2007 · 17110.1016/j.jpowsour.2006.11.004 ↗
32. Kundu · J. Power Sources · 2008 · 179 · 69310.1016/j.jpowsour.2007.11.117 ↗