Abstract

Abstract LiCo 1/3 Ni 1/3 Mn 1/3 O 2 cathode electrodes were prepared onto Al current collectors with different surface morphologies through usual doctor blade technique. Their electrochemical performances, especially at high current rate, were influenced by the surface morphology of the current collector:. These implied the less polarization for the electrode prepared on the surface roughened current collector. In addition, the AC complex impedance analysis exhibited that the interface resistance between the film electrode and the current collector as well as the interface resistance between the electrode and the electrolyte was reduced in the case of the surface-roughened current collector, but that the Ohmic resistance was enlarged.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Supercapacitor Materials and Fabrication · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Dominko · Electrochem. Solid State Lett. · 2001 · 4 · A18710.1149/1.1407995 ↗
2. Dominko · J. Power Sources · 2003 · 119–121 · 77010.1016/S0378-7753(03)00250-7 ↗
3. Cornut · J. Electrochem. Soc. · 2012 · 159 · A82210.1149/2.081206jes ↗
4. Zheng · Electrochim. Acta · 2012 · 71 · 25810.1016/j.electacta.2012.03.161 ↗
5. Wu · Adv. Mater. · 2009 · 21 · 271010.1002/adma.200802998 ↗
6. Doherty · Chem. Mater. · 2009 · 21 · 530010.1021/cm9024167 ↗
7. Wang · Adv. Mater. · 2010 · 22 · 494410.1002/adma.201002045 ↗
8. Chen · Nat. Mater. · 2011 · 10 · 42410.1038/nmat3001 ↗
9. Kostecki · Electrochem. Solid State Lett. · 2002 · 5 · A16410.1149/1.1482199 ↗
10. Zhang · J. Electrochem. Soc. · 2001 · 148 · 46310.1149/1.1362541 ↗
11. Schmidt · J. Power Sources · 2011 · 196 · 534910.1016/j.jpowsour.2010.07.071 ↗
12. Edstrom · Electrochim. Acta · 2004 · 50 · 39710.1016/j.electacta.2004.03.049 ↗
13. Eriksson · Langmuir · 2002 · 18 · 360910.1021/la011354m ↗
14. Aurbach · J. Power Sources · 2006 · 162 · 78010.1016/j.jpowsour.2005.07.009 ↗
15. Aurbach · J. Power Sources · 2007 · 165 · 49110.1016/j.jpowsour.2006.10.025 ↗
16. Zhang · J. Electrochem. Soc. · 2005 · 152 · 44810.1149/1.2041867 ↗
17. Zhang · J. Power Sources · 2002 · 109 · 45810.1016/S0378-7753(02)00110-6 ↗
18. Yang · J. Electrochem. Soc. · 2000 · 147 · 439910.1149/1.1394077 ↗
19. Zhang · J. Power Sources · 2001 · 102 · 1610.1016/S0378-7753(01)00781-9 ↗
20. Hyams · J. Electrochem. Soc. · 2007 · 154 · C39010.1149/1.2742321 ↗