journal article·2014-02

Effects of oxidation on structure and performance of LiVPO4F as cathode material for lithium-ion batteries

Rui Ma, Lianyi Shao, Kaiqiang Wu, Miao Shui, Dongjie Wang, Nengbing Long, Yuanlong Ren, Jie Shu

Publisher page

Abstract

Abstract In this paper, a series of LiVPO 4 F-based samples are prepared through sintering LiVPO 4 F at different temperatures under air. Experimental results show that the pristine sample is oxidized to a new compound Li 1 − x VPO 4 F 1 − y O z (0 x y ≤ 1, 0.9 z ≤1) with similar structure of LiVPO 4 O under air at 550 °C or higher one. In - situ X-ray diffraction patterns indicate that the original material LiVPO 4 F undergoes two two-phase structural evolutions upon Li + electrochemical extraction at average operating potentials at 4.26 and 4.30 V, corresponding to the continuous transformation of LiVPO 4 F → Li 0.72 VPO 4 F → VPO 4 F in the first charge process. In the reverse discharge process, there is only one two-phase structural transition VPO 4 F → LiVPO 4 F without the appearance of the intermediate phase Li 0.72 VPO 4 F on Li + insertion reaction at 4.18 V. Therefore, the extraction/insertion process of LiVPO 4 F is an asymmetrical phase transformation. When the sintering temperature is raised to 550 °C, Li 1− x VPO 4 F 1− y O z exhibits extremely poor electrochemical performance, which is attributed to the volatilization loss of lithium and the replacement of fluorine by oxygen in the structure during the sintering process under air. However, Li 1 − x VPO 4 F 1 − y O z has a very stable structure during the whole process of galvanostatic charge/discharge cycles as confirmed by in - situ X-ray diffraction technique.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Scrosati · Nature · 1995 · 373 · 55710.1038/373557a0 ↗
2. Armand · Nature · 2008 · 451 · 65210.1038/451652a ↗
3. Tarascon · Nature · 2001 · 414 · 35910.1038/35104644 ↗
4. Scrosati · J. Power Sources · 2010 · 195 · 241910.1016/j.jpowsour.2009.11.048 ↗
5. Wang · Prog. Chem. · 2011 · 23 · 284
6. Li · Prog. Chem. · 2011 · 23 · 349
7. Bruce · J. Mater. Chem. · 1999 · 9 · 19310.1039/a803938k ↗
8. Nedoseykina · Electrochim. Acta · 2006 · 52 · 146710.1016/j.electacta.2006.02.047 ↗
9. Shokoohi · Appl. Phys. Lett. · 1991 · 59 · 126010.1063/1.105470 ↗
10. Huang · Solid State Ionics · 2000 · 127 · 3110.1016/S0167-2738(99)00057-0 ↗
11. Padhi · J. Electrochem. Soc. · 1997 · 144 · 118810.1149/1.1837571 ↗
12. Kang · Nature · 2009 · 458 · 19010.1038/nature07853 ↗
13. Chen · Ionics · 2012 · 18 · 63510.1007/s11581-012-0677-0 ↗
14. Yamada · J. Electrochem. Soc. · 2001 · 148 · A22410.1149/1.1348257 ↗
15. Ellis · Electrochim. Acta · 2012 · 84 · 14510.1016/j.electacta.2012.04.113 ↗
16. Liu · Electrochim. Acta · 2002 · 47 · 323910.1016/S0013-4686(02)00174-3 ↗
17. Pan · J. Mater. Chem. · 2011 · 21 · 115310.1039/C0JM02810J ↗
18. Wang · J. Mater. Chem. · 2011 · 21 · 636510.1039/c0jm04398b ↗
19. Patoux · J. Power Sources · 2003 · 119-121 · 27810.1016/S0378-7753(03)00150-2 ↗
20. Saidi · J. Power Sources · 2003 · 119-121 · 26610.1016/S0378-7753(03)00245-3 ↗
21. Ramesh · Electrochem. Solid State Lett. · 2010 · 13 · A4310.1149/1.3298353 ↗
22. Lee · J. Appl. Phys. · 2012 · 111 · 07E38
23. Tripathi · Energy Environ. Sci. · 2012 · 5 · 623810.1039/c2ee03222h ↗
24. Xu · Mater. Sci. Eng. R. · 2012 · 73 · 5110.1016/j.mser.2012.05.003 ↗
25. Gover · Solid State Ionics · 2006 · 177 · 263510.1016/j.ssi.2006.04.049 ↗
26. Barker · J. Electrochem. Soc. · 2003 · 150 · A139410.1149/1.1609998 ↗
27. Hamelet · J. Mater. Chem. · 2009 · 19 · 397910.1039/b901491h ↗
28. Ma · Ionics · 2012 · 19 · 72510.1007/s11581-012-0807-8 ↗
29. Shu · J. Mater. Chem. · 2012 · 22 · 303510.1039/c1jm14894j ↗
30. Shu · Ionics · 2011 · 17 · 50310.1007/s11581-011-0544-4 ↗
31. Lyczko · Ind. Eng. Chem. Res. · 2012 · 51 · 29210.1021/ie201799x ↗
32. Barker · J. Power Sources · 2005 · 146 · 51610.1016/j.jpowsour.2005.03.126 ↗
33. Yi · J. Electrochem. Soc. · 2011 · 158 · A26610.1149/1.3533391 ↗
34. Naghash · Electrochim. Acta · 2001 · 46 · 94110.1016/S0013-4686(00)00657-5 ↗
35. Xia · J. Electrochem. Soc. · 2001 · 148 · A72310.1149/1.1376117 ↗
36. Reddy · J. Power Sources · 2010 · 195 · 576810.1016/j.jpowsour.2010.03.032 ↗
37. Li · J. Power Sources · 2006 · 160 · 63310.1016/j.jpowsour.2006.01.067 ↗
38. Zheng · J. Power Sources · 2012 · 202 · 38010.1016/j.jpowsour.2011.10.144 ↗
39. Rho · J. Electrochem. Soc. · 2007 · 154 · A28310.1149/1.2433539 ↗
40. Kuo · J. Phys. Chem. B · 2008 · 112 · 1125010.1021/jp803210w ↗
41. Dai · Mater. Rev. · 2005 · 19 · 69
42. Harrison · Inorg. Chem. · 2011 · 50 · 361310.1021/ic1025747 ↗
43. Barker · J. Electrochem. Soc. · 2004 · 151 · A167010.1149/1.1785796 ↗
44. Yang · Solid State Sci. · 2008 · 10 · 129210.1016/j.solidstatesciences.2008.01.028 ↗
45. Azmi · J. Power Sources · 2005 · 146 · 52510.1016/j.jpowsour.2005.03.101 ↗
46. Basir · 2009
47. Mba · J. Electrochem. Soc. · 2012 · 159 · A117110.1149/2.022208jes ↗
48. Barker · J. Electrochem. Soc. · 2005 · 152 · A177610.1149/1.1990068 ↗
49. Mba · Chem. Mater. · 2012 · 24 · 122310.1021/cm3003996 ↗