Effect of pinhole location on degradation in polymer electrolyte fuel cells
Source abstract
Abstract
Abstract This work analyses the impact of the location of pinholes in polymer electrolyte fuel cells on the degradation of the electrodes. Defects with a diameter of 0.45 mm were created in a 25 cm 2 membrane electrode assembly (MEA) of a fuel cell. The MEA was operated and characterised using a segmented single cell. The effects of the pinholes on degradation were measured and evaluated. Defects affected the fuel cell behaviour during periods of hydrogen starvation, thus accelerating the degradation process of the carbon support as well as the loss of active platinum catalyst surface area. Furthermore, the effects of the induced pinholes on membrane degradation and performance decay were determined. Pinholes close to the anode inlet in general have shown a more severe effect on the fuel cell operation parameters, such as open circuit voltage, performance, membrane resistance and hydrogen crossover, than pinholes at any other locations. Also, electrode degradation was accelerated. These effects were mainly due to locally increased temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advanced battery technologies research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Perspective on hydrogen energy carrier and its automotive applications
2. H2 generation from alkaline electrolyzer10.1002/wene.150 ↗
3. Design and optimization of a proton exchange membrane fuel cell CHP system for residential use10.1016/j.enbuild.2013.11.022 ↗
4. An overview of fuel cell technology: fundamentals and applications10.1016/j.rser.2014.01.012 ↗
5. A review of accelerated stress tests of MEA durability in PEM fuel cells10.1016/j.ijhydene.2008.10.012 ↗
6. Degradation analysis and modeling of reinforced catalyst coated membranes operated under OCV conditions10.1016/j.jpowsour.2008.05.074 ↗
7. Accelerated durability testing via reactants relative humidity cycling on PEM fuel cells10.1016/j.apenergy.2011.05.011 ↗
8. Application of a segmented cell setup to detect pinhole and catalyst loading defects in proton exchange membrane fuel cells10.1016/j.electacta.2012.04.138 ↗
9. The operation characteristics of MEAs with pinholes for polymer electrolyte membrane fuel cells10.1149/1.2937450 ↗
10. Experimental investigation of pinhole effect on MEA/cell aging in PEMFC10.1016/j.ijhydene.2012.09.058 ↗
11. Nafion degradation in PEFCs from end plate iron contamination10.1016/S0013-4686(03)00026-4 ↗
12. Is H2O2 involved in the membrane degradation mechanism in PEMFC?10.1149/1.2192696 ↗
13. Gas crossover and membrane degradation in polymer electrolyte fuel cells10.1016/j.electacta.2006.03.008 ↗
14. Mechanisms of membrane degradation
15. The chemistry of fuel cell membrane chemical degradation10.1149/1.2981859 ↗
16. Degradation rates of PEM fuel cells running at open circuit voltage10.1149/1.2356197 ↗
17. Thermal stability of nafion® in simulated fuel cell environments10.1149/1.1836669 ↗
18. The effect of platinum on carbon corrosion behavior in polymer electrolyte fuel cells10.1016/j.electacta.2011.06.093 ↗
19. Investigation of thermal and electrochemical degradation of fuel cell catalysts10.1016/j.jpowsour.2006.03.033 ↗
20. A review of platinum-based catalyst layer degradation in proton exchange membrane fuel cells10.1016/j.jpowsour.2009.06.073 ↗
21. Polarization study of a PEMFC with four reference electrodes at hydrogen starvation conditions10.1016/j.jpowsour.2008.01.001 ↗
22. Relationship between carbon corrosion and positive electrode potential in a proton-exchange membrane fuel cell during start/stop operation10.1016/j.jpowsour.2009.03.039 ↗
23. Study of the cell reversal process of large area proton exchange membrane fuel cells under fuel starvation10.1016/j.jpowsour.2009.06.059 ↗
24. Characteristics of electrode potential behavior and degradation under hydrogen-starved operation in PEFC
25. Effect of anode catalyst support on degradation of MEA caused by hydrogen starvation operation in PEFC
26. Recent advances in activity and durability enhancement of Pt/C catalytic cathode in PEMFC10.1016/j.jpowsour.2007.07.049 ↗
27. Inbody M a. PEM fuel cell electrocatalyst durability measurements10.1016/j.jpowsour.2006.03.009 ↗
28. The realcondition of electrochemically oxidised platinum surfaces10.1016/S0022-0728(73)80307-9 ↗
29. Instability of supported platinum nanoparticles in low-temperature fuel cells10.1007/s11244-007-9000-0 ↗
30. Effects of crossover hydrogen on platinum dissolution and agglomeration10.1016/j.jpowsour.2011.05.034 ↗
31. Platinum dissolution and deposition in the polymer electrolyte membrane of a PEM fuel cell as studied by potential cycling10.1039/B514342J ↗
32. Analytical TEM study of Pt particle deposition in the proton-exchange membrane of a membrane-electrode-assembly10.1016/j.jpowsour.2005.10.111 ↗
33. Local degradation at membrane defects in polymer electrolyte fuel cells10.1149/1.023306jes ↗
34. Understanding membrane failure in PEMFC: comparison of diagnostic tools at different observation scales10.1002/fuce.201100161 ↗
35. Membrane degradation during combined chemical and mechanical accelerated stress testing of polymer electrolyte fuel cells10.1016/j.jpowsour.2014.01.106 ↗
36. Selective real-time quantification of hydrogen within mixtures of gases via an electrochemical method10.1016/j.ijhydene.2014.11.126 ↗