A novel 3D-layered electrochemical-thermal coupled model strategy for the nail-penetration process simulation
Source abstract
Abstract
Abstract The safety is one of the persisting concerns related with Lithium-ion (Li-ion) batteries, among which the internal short-circuit is the most dangerous abusive situation and has always been the root cause for several catastrophic accidents in recent years. In this work, a 3D-layered electrochemical-thermal coupled model is employed to investigate the nail-penetration process in a Li-ion cell. The model is based on multilayer construction of a cell, and an effective strategy to evaluate the short-circuit area equivalent resistance (i.e. the equivalent resistance of short-circuit area that is caused by nail-penetration) during the penetration process is proposed. The developed model is proved to have capability of estimating the thermal runaway time, as well as the temperature distribution during nail-penetration process. It is also found that the active material loss during the nail-penetration process can be reconstructed by utilizing the developed model, which could provide understandings about the side reactions inside the cell during the nail-penetration process. The present study provides some insights about the nail-penetration process, and can be treated as a useful tool that helps the design of Li-ion cells for improving safety.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Battery Technologies Research · Advancements in Battery Materials · Electrical Contact Performance and Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. He · Appl. Energy · 2013 · 101 · 80810.1016/j.apenergy.2012.08.031 ↗
2. Thielmann · 2012
3. Armand · Nature · 2008 · 451 · 65210.1038/451652a ↗
4. Wang · J. Power Sources · 2012 · 208 · 21010.1016/j.jpowsour.2012.02.038 ↗
5. Huang · Appl. Energy · 2016 · 183 · 65910.1016/j.apenergy.2016.08.160 ↗
6. Wang · Int. J. Heat Mass Transf. · 2016 · 93 · 89610.1016/j.ijheatmasstransfer.2015.11.007 ↗
7. Capozzo · 2006
8. Xiang · J. Power Sources · 2009 · 191 · 57510.1016/j.jpowsour.2009.02.045 ↗
9. Feng · J. Power Sources · 2014 · 255 · 29410.1016/j.jpowsour.2014.01.005 ↗
10. Ribiere · J. RSC · 2012 · 5 · 5271
11. Liu · J. Power Sources · 2016 · 304 · 910.1016/j.jpowsour.2015.10.106 ↗
12. Maleki · J. Power Sources · 2009 · 191 · 56810.1016/j.jpowsour.2009.02.070 ↗
13. Doughty · 2010
14. Fang · J. Power Sources · 2014 · 248 · 109010.1016/j.jpowsour.2013.10.004 ↗
15. Abada · J. Power Sources · 2016 · 306 · 17810.1016/j.jpowsour.2015.11.100 ↗
16. Yamauchi · J. Power Sources · 2004 · 136 · 9910.1016/j.jpowsour.2004.05.011 ↗
17. Ren · J. Power Sources · 2014 · 249 · 15610.1016/j.jpowsour.2013.10.058 ↗
18. Scrosati · 2015
19. Santhanagopalan · J. Power Sources · 2009 · 194 · 55010.1016/j.jpowsour.2009.05.002 ↗
20. Zhao · J. Electrochem. Soc. · 2015 · 162 · A135210.1149/2.1031507jes ↗
21. Orendorff · J. Power Sources · 2011 · 196 · 655410.1016/j.jpowsour.2011.03.035 ↗
22. Pistoia · 2014
23. Liu · J. Automot. Saf. Energy · 2013 · 4 · 82
24. F. Bianchi, B. Tevene, IEEE (2015)1068 – 1071.10.1109/I2MTC.2015.7151419 ↗
25. Kim · J. Power Sources · 2015 · 289 · 4110.1016/j.jpowsour.2015.04.010 ↗
26. Tobishima · J. Power Sources · 1999 · 81 · 88210.1016/S0378-7753(98)00240-7 ↗
27. Wu · Electrochim. Acta · 2004 · 49 · 180310.1016/j.electacta.2003.12.012 ↗
28. Tobishima · J. Power Sources · 2000 · 188 · 18810.1016/S0378-7753(00)00409-2 ↗
29. Chiu · J. Power Sources · 2014 · 251 · 25410.1016/j.jpowsour.2013.11.069 ↗
30. Zhang · J. Automot. Eng. · 2015 · 37 · 743
31. Feng · Appl. Energy · 2015 · 154 · 7410.1016/j.apenergy.2015.04.118 ↗
32. Feng · J. Power Sources · 2015 · 275 · 26110.1016/j.jpowsour.2014.11.017 ↗
33. Zhao · J. Electrochem. Soc. · 2015 · 162 · A20710.1149/2.1071501jes ↗
34. Lee · J. Power Sources · 2015 · 293 · 49810.1016/j.jpowsour.2015.05.095 ↗
35. Zhao · Appl. Energy · 2016 · 173 · 2910.1016/j.apenergy.2016.04.016 ↗
36. Cui · 2014 · 20
37. C.T. Lin, C. Cui. Numerical simulation of nail test for Li-ion battery. Unpublished work.
38. Li · Chin. J. Power Sources · 2009 · 10 · 927
39. Kima · J. Power Sources · 2007 · 170 · 47610.1016/j.jpowsour.2007.04.018 ↗
40. Hatchard · J. Electrochem, Soc. · 2001 · 148 · A75510.1149/1.1377592 ↗
41. Kim · J. Solid State Electrochem · 2008 · 12 · 86710.1007/s10008-008-0552-0 ↗
42. Kima · J. Power Sources · 2007 · 171 · 91710.1016/j.jpowsour.2007.06.028 ↗
43. Wang · Chin. J. Chem. · 2011 · 29 · 158310.1002/cjoc.201180284 ↗
44. Spotnitza · J. Power Sources · 2003 · 113 · 8110.1016/S0378-7753(02)00488-3 ↗
45. Sato · J. Power Sources · 2001 · 99 · 7010.1016/S0378-7753(01)00478-5 ↗