Abstract In this work, a cerium-gadolinium oxide (CGO)/nickel (Ni)-CGO hollow fibre (HF) for micro-tubular solid oxide fuel cells (SOFCs), which consists of a fully gas-tight outer electrolyte layer supported on a porous inner composite anode layer, has been developed via a novel single-step co-extrusion/co-sintering technique, followed by an easy reduction process. After depositing a multi-layers cathode layer and applying current collectors on both anode and cathode, a micro-tubular SOFC is developed with the maximum power densities of 440–1000 W m−2 at 450–580 °C. Efforts have been made in enhancing the performance of the cell by reducing the co-sintering temperature and improving the cathode layer and current collection from inner (anode) wall. The improved cell produces maximum power densities of 3400–6800 W m−2 at 550–600 °C, almost fivefold higher than the previous cell. Further improvement has been carried out by reducing thickness of the electrolyte layer. Uniform and defect-free outer electrolyte layer as thin as 10 μm can be achieved when the extrusion rate of the outer layer is controlled. The highest power output of 11,100 W m−2 is obtained for the cell of 10 μm electrolyte layer at 600 °C. This result further highlights the potential of co-extrusion technique in producing high quality dual-layer HF support for micro-tubular SOFC.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Catalytic Processes in Materials Science

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. Kendall · 2003 · 197
2. Suzuki · Journal of Power Sources · 2006 · 160 · 7310.1016/j.jpowsour.2006.01.037 ↗
3. Droushiotis · Electrochemistry Communications · 2009 · 11 · 179910.1016/j.elecom.2009.07.022 ↗
4. Othman · Journal of Membrane Science · 2010 · 351 · 19610.1016/j.memsci.2010.01.050 ↗
5. Droushiotis · Electrochemistry Communications · 2010 · 12 · 79210.1016/j.elecom.2010.03.035 ↗
6. Othman · Journal of Membrane Science · 2010 · 365 · 38210.1016/j.memsci.2010.09.036 ↗
7. Tan · Journal of Membrane Science · 2001 · 188 · 8710.1016/S0376-7388(01)00369-6 ↗
8. Kingsbury · Journal of Membrane Science · 2009 · 328 · 13410.1016/j.memsci.2008.11.050 ↗
9. Kim · Journal of Membrane Science · 2001 · 187 · 4710.1016/S0376-7388(00)00648-7 ↗
10. Chen · Materials Research Bulletin · 2007 · 42 · 167410.1016/j.materresbull.2006.11.031 ↗
11. Suzuki · 2009 · 141