Abstract
Abstract Ceramic fuel cells employing lithium compounds show very high ionic conductivity and remarkable power density at temperatures of 350–600 °C. A composite electrolyte made of ceramic powder and lithium compound can reach ionic conductivities >0.1 S cm−1 at 550 °C, even up to 0.5 S cm−1. This is more than 100-times higher than the electrolyte conductivity of traditional solid oxide fuel cells employing e.g. yttria stabilized zirconia, yttrium doped barium zirconate, or strontium and magnesium doped lanthanum gallate. A fuel cell with a lithium compound for symmetrical electrode and single-oxide or composite oxide as electrolyte can reach a power density above 1 W cm−2. Here, the development and progress of the ceramic lithium compound composite electrolyte fuel cell is reviewed to better understand its working mechanism, the origins for the high ionic conductivity, and the excellent low-temperature catalytic activity of the electrode.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. Zhu · Electrochem. Commun. · 2009 · 11 · 95810.1016/j.elecom.2009.02.034 ↗
2. Jiang · J. Power Sources · 2013 · 232 · 27910.1016/j.jpowsour.2013.01.064 ↗
3. Meng · Int. J. Hydrogen Energy · 2014 · 39 · 453110.1016/j.ijhydene.2014.01.008 ↗
4. Mao · J. Alloys Compd. · 2015 · 637 · 28610.1016/j.jallcom.2015.02.001 ↗
5. Zhao · Int. J. Hydrogen Energy · 2013 · 38 · 1636510.1016/j.ijhydene.2013.10.003 ↗
6. Jiang · Electrochim. Acta · 2014 · 133 · 36410.1016/j.electacta.2014.04.064 ↗
7. Chen · J. Power Sources · 2014 · 250 · 18810.1016/j.jpowsour.2013.11.010 ↗
8. Wachsman · Science · 2011 · 334 · 93510.1126/science.1204090 ↗
9. Sadykov · Carbon Resour. Convers. · 2020 · 3 · 112
10. Ding · Energy Environ. Sci. · 2014 · 7 · 55210.1039/c3ee42926a ↗
11. Suzuki · Science · 2009 · 325 · 85210.1126/science.1176404 ↗
12. Waldbillig · J. Power Sources · 2005 · 145 · 20610.1016/j.jpowsour.2004.12.071 ↗
13. Zhu · Fuel Cell. Bull. · 2002 · 1 · 810.1016/S1464-2859(02)80005-0 ↗
14. Zhu · J. Power Sources · 2003 · 118 · 4710.1016/S0378-7753(03)00060-0 ↗
15. Xia · J. Power Sources · 2009 · 188 · 15610.1016/j.jpowsour.2008.11.068 ↗
16. Huang · Electrochem. Commun. · 2006 · 8 · 78510.1016/j.elecom.2006.03.016 ↗
17. Raza · Int. J. Energy Res. · 2014 · 38 · 52410.1002/er.3150 ↗
18. Zhang · Int. J. Hydrogen Energy · 2010 · 35 · 693410.1016/j.ijhydene.2010.04.026 ↗
19. Amar · Solid State Ionics · 2011 · 182 · 13310.1016/j.ssi.2010.11.009 ↗
20. Zhu · J. Power Sources · 2003 · 114 · 110.1016/S0378-7753(02)00592-X ↗
21. Afzal · Electrochim. Acta · 2015 · 178 · 38510.1016/j.electacta.2015.07.183 ↗
22. Wu · J. Power Sources · 2012 · 201 · 16410.1016/j.jpowsour.2011.10.084 ↗
23. Zhu · Nano Energy · 2016 · 19 · 15610.1016/j.nanoen.2015.11.015 ↗
24. Qiao · J. Power Sources · 2018 · 392 · 3310.1016/j.jpowsour.2018.04.096 ↗
25. Zhu · Electrochem. Commun. · 2011 · 13 · 22510.1016/j.elecom.2010.12.019 ↗
26. Zhu · Adv. Funct. Mater. · 2011 · 21 · 246510.1002/adfm.201002471 ↗
27. Meng · Int. J. Hydrogen Energy · 2018 · 43 · 1269710.1016/j.ijhydene.2018.01.209 ↗
28. Khan · Ceram. Int. · 2014 · 40 · 977510.1016/j.ceramint.2014.02.064 ↗
29. Yousaf Shah · Int. J. Hydrogen Energy · 2020 · 45 · 1447010.1016/j.ijhydene.2020.03.147 ↗
30. Rauf · ACS Appl. Mater. Interfaces · 2020 · 12 · 3507110.1021/acsami.0c10061 ↗
31. An · Nat. Energy · 2018 · 3 · 87010.1038/s41560-018-0230-0 ↗
32. Lee · Nano Lett. · 2020 · 20 · 294310.1021/acs.nanolett.9b02344 ↗
33. Lee · Nat. Commun. · 2014 · 5 · 404510.1038/ncomms5045 ↗
34. Chen · ACS Appl. Mater. Interfaces · 2018 · 10 · 3317910.1021/acsami.8b10087 ↗
35. Chen · ACS Appl. Mater. Interfaces · 2019 · 11 · 1064210.1021/acsami.8b20454 ↗
36. Chen · Int. J. Hydrogen Energy · 2018 · 43 · 41710.1016/j.ijhydene.2017.11.056 ↗
37. Chen · J. Mater. Chem. A · 2019 · 7 · 963810.1039/C9TA00499H ↗
38. Chen · Int. J. Hydrogen Energy · 2018 · 43 · 1276510.1016/j.ijhydene.2018.04.006 ↗
39. Chen · Int. J. Hydrogen Energy · 2020 · 45 · 2410810.1016/j.ijhydene.2019.07.223 ↗
40. He · Ceram. Int. · 2020 · 46 · 1754510.1016/j.ceramint.2020.04.053 ↗
41. Zhang · Int. J. Hydrogen Energy · 2021 · 46 · 994810.1016/j.ijhydene.2020.04.192 ↗
42. He · ACS Appl. Energy Mater. · 2020 · 3 · 413410.1021/acsaem.0c00364 ↗
43. Zha · Mater. Chem. Phys. · 2002 · 77 · 59410.1016/S0254-0584(02)00111-6 ↗
44. Sun · Int. J. Electrochem. Sci. · 2007 · 2 · 46210.1016/S1452-3981(23)17086-6 ↗
45. Raza · J. Power Sources · 2010 · 195 · 806710.1016/j.jpowsour.2010.07.044 ↗
46. Raza · Int. J. Hydrogen Energy · 2010 · 35 · 268410.1016/j.ijhydene.2009.04.038 ↗
47. Gao · Int. J. Hydrogen Energy · 2010 · 35 · 1290510.1016/j.ijhydene.2010.08.077 ↗
48. Fan · Int. J. Hydrogen Energy · 2012 · 37 · 1938810.1016/j.ijhydene.2011.09.124 ↗
49. Wang · J. Power Sources · 2011 · 196 · 275410.1016/j.jpowsour.2010.11.033 ↗
50. Fan · J. Power Sources · 2013 · 234 · 15410.1016/j.jpowsour.2013.01.138 ↗
51. Raza · Mater. Today Energy · 2020 · 15 · 10037310.1016/j.mtener.2019.100373 ↗
52. Chen · Int. J. Hydrogen Energy · 2014 · 39 · 1230910.1016/j.ijhydene.2014.04.004 ↗
53. Ma · Int. J. Hydrogen Energy · 2014 · 39 · 1746010.1016/j.ijhydene.2014.01.143 ↗
54. Asghar · Mater. Today Energy · 2017 · 5 · 33810.1016/j.mtener.2017.07.017 ↗
55. Khan · Int. J. Hydrogen Energy · 2017 · 42 · 2090410.1016/j.ijhydene.2017.05.152 ↗
56. Asghar · Int. J. Hydrogen Energy · 2018 · 43 · 1289210.1016/j.ijhydene.2018.05.045 ↗
57. Ali · ACS Appl. Mater. Interfaces · 2018 · 10 · 80610.1021/acsami.7b17010 ↗
58. Wang · Electrochem. Commun. · 2008 · 10 · 161710.1016/j.elecom.2008.08.023 ↗
59. Zhang · Int. J. Hydrogen Energy · 2011 · 36 · 1464310.1016/j.ijhydene.2011.08.054 ↗
60. Fan · Int. J. Hydrogen Energy · 2011 · 36 · 998710.1016/j.ijhydene.2011.05.055 ↗
61. Tan · Int. J. Hydrogen Energy · 2013 · 38 · 37010.1016/j.ijhydene.2012.09.160 ↗
62. Fan · Int. J. Hydrogen Energy · 2013 · 38 · 1139810.1016/j.ijhydene.2013.06.050 ↗
63. Fan · J. Power Sources · 2016 · 306 · 36910.1016/j.jpowsour.2015.12.015 ↗
64. Nakamura · Solid State Ionics · 1982 · 7 · 11910.1016/0167-2738(82)90004-2 ↗
65. Zhu · J. Power Sources · 2011 · 196 · 636210.1016/j.jpowsour.2011.03.078 ↗
66. Hu · J. Power Sources · 2014 · 248 · 57710.1016/j.jpowsour.2013.09.095 ↗
67. Mi · Int. J. Hydrogen Energy · 2017 · 42 · 2221410.1016/j.ijhydene.2017.03.025 ↗
68. Huang · 2005
69. Liu · Sci. Rep. · 2015 · 5 · 1194610.1038/srep11946 ↗
70. Di · J. Power Sources · 2010 · 195 · 469510.1016/j.jpowsour.2010.02.066 ↗
71. Fan · Int. J. Electrochem. Sci. · 2012 · 7 · 842010.1016/S1452-3981(23)18004-7 ↗
72. Fan · Nano Energy · 2012 · 1 · 63110.1016/j.nanoen.2012.04.004 ↗
73. Fan · J. Power Sources · 2012 · 203 · 6510.1016/j.jpowsour.2011.12.017 ↗
74. Gao · Int. J. Hydrogen Energy · 2011 · 36 · 398410.1016/j.ijhydene.2010.12.061 ↗
75. Zhao · Int. J. Hydrogen Energy · 2012 · 37 · 1935110.1016/j.ijhydene.2011.11.003 ↗
76. Wang · Int. J. Hydrogen Energy · 2012 · 37 · 1938010.1016/j.ijhydene.2011.10.061 ↗
77. Ma · Int. J. Hydrogen Energy · 2013 · 38 · 59710.1016/j.ijhydene.2012.07.018 ↗
78. Tan · Int. J. Hydrogen Energy · 2013 · 38 · 37010.1016/j.ijhydene.2012.09.160 ↗
79. Ahmed · Int. J. Hydrogen Energy · 2016 · 41 · 697210.1016/j.ijhydene.2016.02.095 ↗
80. Raza · Adv. Energy Mater. · 2011 · 1 · 122510.1002/aenm.201100318 ↗
81. Patakangas · Int. J. Hydrogen Energy · 2016 · 41 · 760910.1016/j.ijhydene.2015.10.133 ↗
82. Asghar · Int. J. Hydrogen Energy · 2018 · 43 · 1279710.1016/j.ijhydene.2018.03.232 ↗
83. Asghar · Front. Chem. Sci. Eng. · 2017 · 12 · 16210.1007/s11705-017-1642-2 ↗
84. Yao · Int. J. Hydrogen Energy · 2021 · 46 · 980910.1016/j.ijhydene.2020.06.091 ↗
85. Giorgi · J. Power Sources · 1994 · 49 · 22710.1016/0378-7753(93)01814-X ↗
86. Fan · J. Mater. Chem. A · 2014 · 2 · 539910.1039/c3ta14098a ↗
87. Xia · J. Power Sources · 2017 · 342 · 77910.1016/j.jpowsour.2016.12.120 ↗
88. Xu · Int. J. Hydrogen Energy · 2017 · 42 · 1749510.1016/j.ijhydene.2017.05.218 ↗
89. Wang · Int. J. Hydrogen Energy · 2017 · 42 · 1755210.1016/j.ijhydene.2017.05.158 ↗
90. Garcia-Barriocanal · Science · 2008 · 321 · 67610.1126/science.1156393 ↗
91. Lee · Nano Lett. · 2015 · 15 · 736210.1021/acs.nanolett.5b02726 ↗
92. Zhu · Nano Energy · 2017 · 37 · 19510.1016/j.nanoen.2017.05.003 ↗
93. Mi · Int. J. Hydrogen Energy · 2018 · 43 · 1275610.1016/j.ijhydene.2018.03.204 ↗
94. Cai · J. Power Sources · 2018 · 384 · 31810.1016/j.jpowsour.2018.03.012 ↗
95. Meng · J. Power Sources · 2019 · 421 · 3310.1016/j.jpowsour.2019.02.100 ↗
96. Xia · Nat. Commun. · 2019 · 10 · 170710.1038/s41467-019-09532-z ↗
97. Duan · Nature · 2018 · 557 · 21710.1038/s41586-018-0082-6 ↗
98. Duan · Nat. Energy · 2020 · 5 · 23010.1038/s41560-020-0669-7 ↗
99. Xing · ACS Energy Lett. · 2019 · 4 · 260110.1021/acsenergylett.9b01829 ↗
100. Maier · Nat. Mater. · 2005 · 4 · 80510.1038/nmat1513 ↗