journal article·2012-02

Deposition and activity stability of Pt–Co catalysts on carbon nanotube-based electrodes prepared by microwave-assisted synthesis

Chien-Te Hsieh, Wei-Yu Chen, I-Ling Chen, Anup Kumar Roy

Publisher page

Abstract

Abstract This work investigates the electrochemical activity and durability of bimetallic Pt–Co electrocatalysts on carbon nanotube (CNT) electrodes, which are prepared by using a microwave-assisted polyol process within a short period of ∼6 min. Multilayered CNTs are directly grown on carbon paper (CP) substrate by catalytic chemical vapor deposition with Ni catalyzing the growth of CNTs. The as-grown CNTs are employed as the support for the subsequent Pt–Co catalysts, which are deposited on the CNTs by using one- and two-step microwave-assisted reduction processes. Physicochemical characterizations are conducted to identify particle dispersion, particle-size distribution, and Pt/Co atomic ratio in the binary catalysts. It has been shown that Pt–Co–CNT/CP electrocatalyst, prepared by two-step microwave heating (i.e., deposition of Pt, followed by Co addition), offers highly electrochemical surface area and stable activity during potential cycling (1000 cycles). Such Pt–Co crystallographic phases on CNT-based support are found to be more corrosion-resistant in acidic electrolyte and represent the preferred phase structure under the consideration of activity stability. The fact that the microwave-assisted deposition of Pt–Co catalysts promotes electrochemical activity and stability has a great advancement on the development of binary electrocatalysts for fuel-cell applications.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrocatalysts for Energy Conversion · Fuel Cells and Related Materials · Advanced battery technologies research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Wang · Nano Lett. · 2003 · 4 · 34510.1021/nl034952p ↗
2. Wee · J. Power Sources · 2007 · 165 · 66710.1016/j.jpowsour.2006.12.051 ↗
3. Miura · J. Chem. Mater. · 2009 · 21 · 266110.1021/cm900048e ↗
4. Han · Int. J. Hydrogen Energy · 2009 · 34 · 242610.1016/j.ijhydene.2008.12.073 ↗
5. Takenaka · Electrochem. Soc. · 2008 · 155 · B92910.1149/1.2952665 ↗
6. Koh · J. Phys. Chem. C · 2007 · 111 · 374410.1021/jp067269a ↗
7. Kannan · J. Power Sources · 2009 · 192 · 29710.1016/j.jpowsour.2009.03.022 ↗
8. Kamavaram · J. Power Sources · 2009 · 188 · 5110.1016/j.jpowsour.2008.11.084 ↗
9. Wang · J. Power Sources · 2007 · 171 · 5510.1016/j.jpowsour.2006.12.028 ↗
10. Lebert · Catal. Today · 2009 · 143 · 6410.1016/j.cattod.2008.10.043 ↗
11. Maheshwari · Electrochim. Acta · 2009 · 54 · 747610.1016/j.electacta.2009.07.085 ↗
12. Tang · Electrochim. Acta · 2011 · 56 · 432710.1016/j.electacta.2011.01.035 ↗
13. Li · Phys. J. Chem. C · 2007 · 111 · 280310.1021/jp0655470 ↗
14. Hsieh · J. Alloys Compd. · 2008 · 466 · 23310.1016/j.jallcom.2007.11.014 ↗
15. Chen · Langmuir · 2007 · 23 · 1130310.1021/la7016648 ↗
16. Hsieh · Int. J. Hydrogen Energy · 2009 · 34 · 68510.1016/j.ijhydene.2008.11.008 ↗
17. Paunovic · Int. J. Hydrogen Energy · 2009 · 34 · 286610.1016/j.ijhydene.2009.01.024 ↗
18. Santiago · J. Phys. Chem. C · 2007 · 111 · 314610.1021/jp0670081 ↗
19. Xu · J. Am. Chem. Soc. · 2004 · 126 · 471710.1021/ja031701+ ↗
20. Salgado · J. Phys. Chem. B · 2004 · 108 · 1776710.1021/jp0486649 ↗
21. Hsieh · J. Power Sources · 2008 · 183 · 91
22. Lopes · J. Power Sources · 2007 · 164 · 11110.1016/j.jpowsour.2006.10.052 ↗
23. Yen · Energy Fuels · 2007 · 21 · 226810.1021/ef0606409 ↗
24. Yano · Langmuir · 2007 · 23 · 643810.1021/la070078u ↗
25. Lee · J. Power Sources · 2005 · 145 · 14710.1016/j.jpowsour.2005.02.067 ↗
26. Dupont · J. Am. Chem. Soc. · 2006 · 128 · 912910.1021/ja061303h ↗
27. Hsieh · Int. J. Hydrogen Energy · 2011 · 36 · 276510.1016/j.ijhydene.2010.11.030 ↗
28. Zignani · J. Power sources · 2008 · 182 · 8310.1016/j.jpowsour.2008.03.061 ↗
29. Chen · Mater. Chem. Phys. · 2005 · 91 · 12410.1016/j.matchemphys.2004.11.003 ↗
30. Liu · J. Phys. Chem. B · 2004 · 108 · 823410.1021/jp049422b ↗
31. Bock · J. Am. Chem. Soc. · 2004 · 126 · 802810.1021/ja0495819 ↗
32. Hsieh · Carbon · 2008 · 116 · 677
33. Hsieh · Carbon · 2010 · 48 · 61210.1016/j.carbon.2009.09.076 ↗
34. Steigerwalt · J. Phys. Chem. B · 2002 · 106 · 6010.1021/jp012707t ↗
35. Prabhuram · Electrochim. Acta · 2007 · 52 · 264910.1016/j.electacta.2006.09.027 ↗
36. Bonakdarpour · J. Electrochem. Soc. · 2008 · 155 · B10810.1149/1.2806166 ↗
37. Koh · J. Power Sources · 2007 · 172 · 5010.1016/j.jpowsour.2007.01.002 ↗
38. Corrias · Chem. Eng. Sci. · 2003 · 58 · 447510.1016/S0009-2509(03)00265-3 ↗
39. Hsieh · Powder Technol. · 2009 · 192 · 1610.1016/j.powtec.2008.11.004 ↗
40. Wagner · 1979
41. Halder · J. Phys. Chem. C · 2009 · 113 · 146610.1021/jp8072574 ↗
42. Xing · J. Phys. Chem. B · 2004 · 108 · 1925510.1021/jp046697i ↗
43. Shao · J. Electrochem. Soc. · 2006 · 153 · A109310.1149/1.2191147 ↗
44. Pourbaix · 1966
45. Hsieh · Int. J. Hydrogen Energy · 2007 · 32 · 345710.1016/j.ijhydene.2007.02.021 ↗
46. Travitsky · J. Power Sources · 2006 · 161 · 78210.1016/j.jpowsour.2006.05.035 ↗
47. Hernández-Fernández · Appl. Catal. B Environ. · 2007 · 77 · 1910.1016/j.apcatb.2007.07.002 ↗
48. Xu · Electrochim. Acta · 2009 · 54 · 632210.1016/j.electacta.2009.05.088 ↗
49. Oezaslan · J. Power Sources · 2011 · 196 · 524010.1016/j.jpowsour.2010.11.016 ↗
50. Chen · Electrochem. Commun. · 2009 · 11 · 207110.1016/j.elecom.2009.09.008 ↗