journal article·2012-01

Preparation of core (Ni base)–shell (Silicalite-1) catalysts and their application for alkali resistance in direct internal reforming molten carbonate fuel cell

Jian Zhang, Xiongfu Zhang, Min Tu, Weifeng Liu, Haiou Liu, Jieshan Qiu, Li Zhou, Zhigang Shao, Hung Lai Ho, King Lun Yeung

Publisher page

Abstract

Abstract Alkali-resistant Ni/SiO 2 –Sil-1 and Ni/Al 2 O 3 –Sil-1 core–shell catalysts were prepared for use in direct internal reforming molten carbonate fuel cell (DIR-MCFC). A thin zeolite shell was grown on the surface of catalyst beads to create a diffusion barrier against alkali poisons in the vapors generated from the electrolyte during DIR-MCFC operation. The synthesis of low defect zeolite shell was investigated and the effects of shell thickness on catalyst activity were examined. A mathematical model of the reaction and alkali-poisoning was developed and the optimum zeolite shell thickness was determined. The experimental and modeling results demonstrated that the core–shell catalyst is more resistant to alkali poisoning and a zeolite shell thickness of 3.5 μm can protect the catalyst for at least 100 h following a failure of the anode barrier in DIR-MCFC to give sufficient time for repair.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Catalysis and Hydrodesulfurization Studies · Fuel Cells and Related Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. Manfred · J. Power Sources · 2006 · 160 · 84210.1016/j.jpowsour.2006.04.118 ↗
2. Verda · Int. J. Hydrogen Energy · 2010 · 35 · 79410.1016/j.ijhydene.2009.10.104 ↗
3. Bischoff · J. Power Sources · 2002 · 105 · 21610.1016/S0378-7753(01)00942-9 ↗
4. Dick · Curr. Opin. Solid State Mater. Sci. · 2004 · 8 · 37910.1016/j.cossms.2004.12.005 ↗
5. Katikaneni · Catal. Today · 2002 · 77 · 9910.1016/S0920-5861(02)00236-5 ↗
6. Freni · Int. J. Hydrogen Energy · 1994 · 19 · 33710.1016/0360-3199(94)90065-5 ↗
7. Clarke · Catal. Today · 1997 · 38 · 41110.1016/S0920-5861(97)00052-7 ↗
8. Rostrup-Nielsen · Appl. Catal. A · 1995 · 126 · 38110.1016/0926-860X(95)00028-3 ↗
9. Passalacqua · Mater. Lett. · 1996 · 29 · 17710.1016/S0167-577X(96)00141-3 ↗
10. Passalacqua · Mater. Lett. · 1998 · 34 · 25710.1016/S0167-577X(97)00176-6 ↗
11. L.G. Marianowski, Dual compartment anode structure, US: 4702973, 1987-10-27.
12. Tagawa · Appl. Organomet. Chem. · 2001 · 15 · 12710.1002/1099-0739(200102)15:2<127::AID-AOC107>3.0.CO;2-J ↗
13. Berger · Appl. Catal. A: Gen. · 1996 · 143 · 34310.1016/0926-860X(96)00099-3 ↗
14. Choi · Catal. Today · 2004 · 93–95 · 55310.1016/j.cattod.2004.06.004 ↗
15. Park · Int. J. Hydrogen Energy · 2010 · 35 · 567310.1016/j.ijhydene.2010.03.043 ↗
16. Yeung · J. Catal. · 1998 · 174 · 110.1006/jcat.1997.1890 ↗
17. Yeung · Chem. Eng. Sci. · 1994 · 49 · 482310.1016/S0009-2509(05)80062-4 ↗
18. Yeung · J. Membr. Sci. · 1997 · 131 · 910.1016/S0376-7388(97)00352-9 ↗
19. Yeung · Stud. Surf. Sci. Catal. · 1996 · 101 · 134910.1016/S0167-2991(96)80347-8 ↗
20. He · Langmuir · 2005 · 21 · 169910.1021/la047217h ↗
21. Nishiyama · Ind. Eng. Chem. Res. · 2004 · 43 · 121110.1021/ie0341653 ↗
22. Yeung · Catal. Today · 1995 · 25 · 23110.1016/0920-5861(95)00077-S ↗
23. Guo · Chem. Commun. · 2009 · 589810.1039/b910168c ↗
24. Guo · Catal. Today · 2010 · 156 · 28210.1016/j.cattod.2010.07.008 ↗
25. Wang · Catal. Today · 2010 · 156 · 28810.1016/j.cattod.2010.03.034 ↗
26. Zhou · Catal. Commun. · 2009 · 10 · 180410.1016/j.catcom.2009.06.002 ↗
27. Caro · Micropor. Mesopor. Mater. · 2008 · 115 · 21510.1016/j.micromeso.2008.03.008 ↗
28. Au · J. Membr. Sci. · 2001 · 183 · 26910.1016/S0376-7388(00)00598-6 ↗
29. Chau · Lab Chip · 2003 · 3 · 5310.1039/b300052d ↗
30. Guo · Chem. Commun. · 2009 · 39 · 589810.1039/b910168c ↗
31. Wong · J. Membr. Sci. · 2001 · 191 · 14310.1016/S0376-7388(01)00453-7 ↗
32. Yang · J. Phys. Chem. Solids · 2007 · 68 · 2610.1016/j.jpcs.2006.09.009 ↗
33. Chau · J. Membr. Sci. · 2000 · 164 · 25710.1016/S0376-7388(99)00214-8 ↗
34. Lai · Micropor. Mesopor. Mater. · 2002 · 54 · 6310.1016/S1387-1811(02)00341-4 ↗
35. Jiang · Catal. Commun. · 2011 · 12 · 95110.1016/j.catcom.2011.02.021 ↗
36. Au · J. Membr. Sci. · 2001 · 194 · 3310.1016/S0376-7388(01)00489-6 ↗
37. Au · Micropor. Mesopor. Mater. · 2001 · 47 · 20310.1016/S1387-1811(01)00380-8 ↗
38. Chau · Chem. Eng. J. · 2002 · 88 · 18710.1016/S1385-8947(01)00287-X ↗
39. Ha · Micropor. Mesopor. Mater. · 2004 · 72 · 9110.1016/j.micromeso.2004.04.008 ↗
40. Heng · J. Membr. Sci. · 2004 · 243 · 6910.1016/j.memsci.2004.05.025 ↗
41. Motuzas · Micropor. Mesopor. Mater. · 2007 · 99 · 19710.1016/j.micromeso.2006.06.042 ↗
42. Bons · Micropor. Mesopor. Mater. · 2003 · 62 · 910.1016/S1387-1811(03)00384-6 ↗
43. Gouzinis · Chem. Mater. · 1998 · 10 · 249710.1021/cm9802402 ↗
44. Bartholomew · Appl. Catal. A: Gen. · 2001 · 212 · 1710.1016/S0926-860X(00)00843-7 ↗
45. Takenake · Fuel · 2004 · 83 · 4710.1016/S0016-2361(03)00211-4 ↗
46. Lai · Micropor. Mesopor. Mater. · 2000 · 37 · 910.1016/S1387-1811(99)00188-2 ↗
47. Takahashi · Appl. Catal. A: Gen. · 2004 · 273 · 21110.1016/j.apcata.2004.06.033 ↗
48. Roh · J. Mol. Catal. A: Chem. · 2002 · 181 · 13710.1016/S1381-1169(01)00358-2 ↗
49. Kapteijn · Catal. Today · 1995 · 25 · 21310.1016/0920-5861(95)00078-T ↗
50. Ahunbay · J. Phys. Chem. B · 2002 · 106 · 516310.1021/jp013613m ↗
51. Li · Int. J. Hydrogen Energy · 2010 · 35 · 1304110.1016/j.ijhydene.2010.04.058 ↗
52. Arruebo · Chem. Mater. · 2008 · 20 · 48610.1021/cm703269w ↗
53. Lam · J. Phys. Chem. C · 2011 · 116 · 17610.1021/jp1065874 ↗
54. Kwan · Chem. Commun. · 2008 · 363110.1039/b809019j ↗
55. Han · Chem. Commun. · 2011 · 47 · 808510.1039/c1cc12081f ↗