Abstract
The anode properties of Nb-doped rutile TiO2 electrodes were investigated in an ionic liquid electrolyte comprised of N-methyl-N-propylpyrrolidinium cation and bis(fluorosulfonyl)amide anion for use in a safe Na-ion battery. Although the electrolyte’s conductivity was lower than that of a conventional organic electrolyte at 30 oC, it showed high conductivity comparable to that of the organic electrolyte at 60 oC. The Nb-doped TiO2 electrode showed excellent cyclability in the ionic liquid electrolyte at 60 oC: a high capacity retention of 97% was observed even at the 350th cycle, which is comparable to value in the organic electrolyte (91%). In a non-flammability test in a closed system, no ignition was observed with the ionic liquid electrolyte even at 300 oC. These results indicate that combination of a Nb-doped TiO2 anode and ionic liquid electrolyte gives not only an excellent cyclability but also high safety for a Na-ion battery operating at a temperature below the sodium’s melting point of 98 oC.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced battery technologies research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Komaba · Adv. Funct. Mater. · 2011 · 21 · 385910.1002/adfm.201100854 ↗
2. Ellis · Curr. Opin. Solid State Mat. Sci. · 2012 · 16 · 16810.1016/j.cossms.2012.04.002 ↗
3. Oshima · Int. J. Appl. Ceram. Technol. · 2004 · 1 · 26910.1111/j.1744-7402.2004.tb00179.x ↗
4. Yamamoto · J. Power Sources · 2013 · 237 · 9810.1016/j.jpowsour.2013.02.076 ↗
5. Monti · J. Power Sources · 2014 · 245 · 63010.1016/j.jpowsour.2013.06.153 ↗
6. Chen · J. Power Sources · 2014 · 246 · 78310.1016/j.jpowsour.2013.08.027 ↗
7. Ding · J. Power Sources · 2014 · 269 · 12410.1016/j.jpowsour.2014.06.033 ↗
8. Ponrouch · Electrochem. Commun. · 2014 · 54 · 5110.1016/j.elecom.2015.03.002 ↗
9. Hasa · J. Power Sources · 2016 · 303 · 20310.1016/j.jpowsour.2015.10.100 ↗
10. Chagas · J. Power Sources · 2014 · 247 · 37710.1016/j.jpowsour.2013.08.118 ↗
11. Wongittharom · ACS Appl. Mater. Interfaces · 2014 · 6 · 1756410.1021/am5033605 ↗
12. Wongittharom · J. Mater. Chem. A · 2014 · 2 · 565510.1039/c3ta15273a ↗
13. Wang · J. Power Sources · 2015 · 274 · 101610.1016/j.jpowsour.2014.10.143 ↗
14. Usui · J. Power Sources · 2011 · 196 · 391110.1016/j.jpowsour.2010.12.027 ↗
15. Usui · Chem. Lett. · 2012 · 41 · 52110.1246/cl.2012.521 ↗
16. Usui · J. Power Sources · 2013 · 235 · 2910.1016/j.jpowsour.2013.01.188 ↗
17. Shimizu · J. Electrochem. Soc. · 2014 · 161 · A176510.1149/2.0021412jes ↗
18. Shimizu · J. Phys. Chem. C · 2015 · 119 · 297510.1021/jp5121965 ↗
19. Shimizu · Int. J. Electrochem. Sci. · 2015 · 10 · 1013210.1016/S1452-3981(23)11248-X ↗
20. Usui · Electrochemistry · 2015 · 83 · 81010.5796/electrochemistry.83.810 ↗
21. Usui · ACS Appl. Mater. Interfaces · 2015 · 7 · 656710.1021/am508670z ↗
22. Sakaguchi · Electrochem. Solid-State Lett. · 2007 · 10 · J14610.1149/1.2772409 ↗
23. Usui · Thin Solid Films · 2012 · 520 · 700610.1016/j.tsf.2012.07.093 ↗
24. Kim · Nano Lett. · 2014 · 14 · 41610.1021/nl402747x ↗
25. Lalia · J. Power Sources · 2010 · 195 · 742610.1016/j.jpowsour.2010.05.040 ↗
26. Arbizzani · J. Power Sources · 2011 · 196 · 480110.1016/j.jpowsour.2011.01.068 ↗
27. Nagasubramanian · Electrochim. Acta · 2013 · 101 · 310.1016/j.electacta.2012.09.065 ↗
28. Li · RSC Adv. · 2013 · 3 · 1390710.1039/c3ra40275d ↗
29. Quinzeni · J. Power Sources · 2013 · 237 · 20410.1016/j.jpowsour.2013.03.036 ↗
30. Montanino · J. Power Sources · 2014 · 269 · 60810.1016/j.jpowsour.2014.07.027 ↗
31. Yang · Electrochim. Acta · 2014 · 148 · 3910.1016/j.electacta.2014.10.001 ↗