Influence of mechanical grinding on lithium insertion and extraction properties of iron silicide/silicon composites
Source abstract
Abstract
We prepared composite electrodes of iron silicide/Si by using mechanical grinding for mixtures of ferrosilicon and Si followed by gas-deposition, and investigated their electrochemical properties as Li-ion battery anode. With increasing the mechanical grinding time, the phase transformation from FeSi to FeSi2 took place more significantly, and the composite electrode showed better cycle stabilities. There was no remarkable difference in mechanical properties and electronic conductivity between FeSi and FeSi2. On the other hand, the FeSi2 exhibited about three times larger capacities in comparison with the FeSi electrode. In addition, a result of our first principle calculation indicates that Li ion can diffuse more easily in FeSi2 lattice than in FeSi lattice. It is suggested that the better cyclability of the composite electrodes was attributed to the moderate reactivity of FeSi2 with Li and the smooth Li-ion diffusion in it.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Semiconductor materials and interfaces · Advancements in Battery Materials · Silicon and Solar Cell Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Hatchard · J. Electrochem. Soc. · 2004 · 151 · A83810.1149/1.1739217 ↗
2. Obrovac · Electrochem. Solid State Lett. · 2004 · 7 · A9310.1149/1.1652421 ↗
3. Obrovac · J. Electrochem. Soc. · 2007 · 154 · A10310.1149/1.2402112 ↗
4. Chan · J. Power Sources · 2009 · 189 · 3410.1016/j.jpowsour.2008.12.047 ↗
5. Misra · ACS Nano · 2012 · 6 · 546510.1021/nn301339g ↗
6. Sakaguchi · J. Power Sources · 2003 · 119–121 · 5010.1016/S0378-7753(03)00123-X ↗
7. Nagao · J. Electrochem. Soc. · 2004 · 151 · A157210.1149/1.1787173 ↗
8. Sakaguchi · Electrochemistry · 2006 · 74 · 46310.5796/electrochemistry.74.463 ↗
9. Sakaguchi · Electrochem. Solid State Lett. · 2007 · 10 · J14610.1149/1.2772409 ↗
10. Iida · Electrochemistry · 2008 · 76 · 64410.5796/electrochemistry.76.644 ↗
11. Sakaguchi · IOP Conf. Ser. Mater. Sci. Eng. · 2009 · 1 · 01203010.1088/1757-8981/1/1/012030 ↗
12. Usui · J. Power Sources · 2010 · 195 · 364910.1016/j.jpowsour.2009.12.072 ↗
13. Usui · Electrochemistry · 2010 · 78 · 32910.5796/electrochemistry.78.329 ↗
14. Usui · J. Power Sources · 2011 · 196 · 214310.1016/j.jpowsour.2010.10.013 ↗
15. Usui · Int. J. Electrochem. Sci. · 2011 · 6 · 224610.1016/S1452-3981(23)18181-8 ↗
16. Usui · J. Power Sources · 2011 · 196 · 1024410.1016/j.jpowsour.2011.08.018 ↗
17. Usui · Int. J. Electrochem. Sci. · 2012 · 7 · 432210.1016/S1452-3981(23)19541-1 ↗
18. Usui · Electrochemistry · 2012 · 80 · 73710.5796/electrochemistry.80.737 ↗
19. Usui · J. Power Sources · 2013 · 235 · 2910.1016/j.jpowsour.2013.01.188 ↗
20. Usui · Electrochim. Acta · 2013 · 111 · 57510.1016/j.electacta.2013.08.015 ↗
21. Usui · J. Power Sources · 2011 · 196 · 391110.1016/j.jpowsour.2010.12.027 ↗
22. Usui · Chem. Lett. · 2012 · 41 · 52110.1246/cl.2012.521 ↗
23. Usui · Thin Solid Films · 2012 · 520 · 700610.1016/j.tsf.2012.07.093 ↗
24. Usui · 2011
25. Usui · Mater. Lett. · 2014 · 130 · 6110.1016/j.matlet.2014.05.065 ↗
26. Chen · ACS Appl. Mater. Interfaces · 2012 · 4 · 375310.1021/am300952b ↗
27. Choi · Electrochim. Acta · 2011 · 56 · 981810.1016/j.electacta.2011.08.080 ↗
28. Kresse · Phys. Rev. B · 1993 · 47 · RC55810.1103/PhysRevB.47.558 ↗
29. Nakada · Solid State Commun. · 2011 · 151 · 1310.1016/j.ssc.2010.10.036 ↗
30. Acker · J. Chem. Thermodyn. · 1999 · 31 · 152310.1006/jcht.1999.0550 ↗
31. Sakaguchi · J. Power Sources · 1999 · 81−82 · 22910.1016/S0378-7753(98)00214-6 ↗
32. Momma · J. Appl. Crystallogr. · 2011 · 44 · 127210.1107/S0021889811038970 ↗