Effect of the deposition temperature on the electrochemical properties of La0.6Sr0.4Co0.8Fe0.2O3−δ cathode prepared by conventional spray-pyrolysis
Source abstract
Abstract
Abstract La 0.6 Sr 0.4 Co 0.8 Fe 0.2 O 3− δ (LSCF) cathodes have been deposited by conventional spray pyrolysis on Ce 0.8 Gd 0.2 O 1.9 (CGO) electrolytes at different temperatures between 250 and 450 °C, obtaining electrodes with different microstructure and porosity. Highly porous and macroporous electrodes are obtained at deposition temperatures of 250 °C and 450 °C, respectively, with an average grain size of 30–50 nm. The influence of the post-annealing treatment on the microstructure and on the electrochemical properties is investigated by scanning electron microscopy and impedance spectroscopy in air and as a function of the oxygen partial pressure to identify the different contributions to the polarization. Samples annealed at 650 °C show similar values of area specific resistance 0.04–0.06 Ω cm 2 at a measured temperature of 650 °C. However, after annealing the samples at 850 °C, the ASR values increase up to 0.1–0.6 Ω cm 2 with the lowest value corresponding to the film deposited at 250 °C due to the large porosity and surface area of this film. The performance degradation upon annealing is attributed to decreasing reaction sites induced by grain growth and densification.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Minh · 1995
2. Steele · Nature · 2001 · 414 · 34510.1038/35104620 ↗
3. Adler · Chem. Soc. Rev. · 2004 · 104 · 479110.1021/cr020724o ↗
4. Fleig · Annu. Rev. Mater. Res. · 2003 · 33 · 36110.1146/annurev.matsci.33.022802.093258 ↗
5. Tsipis · J. Solid State Electrochem. · 2008 · 12 · 103910.1007/s10008-007-0468-0 ↗
6. Tai · Solid State Ionics · 1995 · 76 · 25910.1016/0167-2738(94)00244-M ↗
7. Shao · Nature · 2004 · 431 · 17010.1038/nature02863 ↗
8. Tarancón · J. Mater. Chem. · 2007 · 17 · 317510.1039/b704320a ↗
9. Švarcová · Solid State Ionics · 2008 · 178 · 178710.1016/j.ssi.2007.11.031 ↗
10. Joshi · J. Power Sources · 2007 · 164 · 63110.1016/j.jpowsour.2006.10.101 ↗
11. Marrero-López · J. Solid State Chem. · 2008 · 181 · 68510.1016/j.jssc.2008.01.008 ↗
12. Ruiz-Morales · Energy Environ. Sci. · 2010 · 3 · 167010.1039/c0ee00166j ↗
13. Beckel · J. Power Sources · 2007 · 173 · 32510.1016/j.jpowsour.2007.04.070 ↗
14. Princivalle · Chem. Mater. · 2004 · 16 · 373310.1021/cm049158z ↗
15. Princivalle · Chem. Mater. · 2005 · 17 · 122010.1021/cm048503h ↗
16. Chang · J. Power Sources · 2008 · 179 · 73410.1016/j.jpowsour.2008.01.019 ↗
17. Chang · J. Eur. Ceram. Soc. · 2012 · 32 · 91510.1016/j.jeurceramsoc.2011.11.001 ↗
18. Dieterle · Adv. Energy Mater. · 2011 · 1 · 24910.1002/aenm.201000036 ↗
19. Marinha · Chem. Mater. · 2011 · 23 · 534010.1021/cm2016998 ↗
20. Beckel · Solid State Ionics · 2007 · 178 · 40710.1016/j.ssi.2007.01.019 ↗
21. Karageorgakis · J. Power Sources · 2010 · 195 · 815210.1016/j.jpowsour.2010.06.089 ↗
22. Taniguchi · Solid State Ionics · 2003 · 156 · 110.1016/S0167-2738(02)00615-X ↗
23. Hsu · J. Electrochem. Soc. · 2006 · 153 · A147810.1149/1.2205153 ↗
24. Ayouchi · J. Power Sources · 2000 · 87 · 10610.1016/S0378-7753(99)00435-8 ↗
25. Marrero-López · Solid State Ionics · 2007 · 178 · 136610.1016/j.ssi.2007.07.008 ↗
26. Rodríguez-Carvajal · Phys. B: Condens. Matter · 1993 · 192 · 5510.1016/0921-4526(93)90108-I ↗
27. 2004
28. Abrantes · 2001
29. Johnson · 2005
30. Wang · Solid State Ionics · 2003 · 159 · 7110.1016/S0167-2738(03)00027-4 ↗
31. Sathe · J. Phys. Condens. Matter · 1998 · 10 · 404510.1088/0953-8984/10/18/014 ↗
32. Acuña · J. Power Sources · 2011 · 196 · 927610.1016/j.jpowsour.2011.07.067 ↗
33. Kingery · J. Am. Ceram. Soc. · 1965 · 48 · 54610.1111/j.1151-2916.1965.tb14665.x ↗
34. Simrick · Solid State Ionics · 2012 · 206 · 710.1016/j.ssi.2011.10.029 ↗
35. Grunbaum · Solid State Ionics · 2009 · 180 · 144810.1016/j.ssi.2009.09.005 ↗
36. Baumann · Solid State Ionics · 2006 · 177 · 107110.1016/j.ssi.2006.02.045 ↗
37. Ringuedé · Solid State Ionics · 2001 · 139 · 16710.1016/S0167-2738(01)00692-0 ↗
38. Marinha · J. Power Sources · 2012 · 197 · 8010.1016/j.jpowsour.2011.09.049 ↗
39. Shah · Solid State Ionics · 2008 · 179 · 205910.1016/j.ssi.2008.07.002 ↗
40. Mantzavinos · Solid State Ionics · 2000 · 134 · 10310.1016/S0167-2738(00)00718-9 ↗
41. Escudero · J. Electroanal. Chem. · 2007 · 611 · 10710.1016/j.jelechem.2007.08.006 ↗
42. Siebert · Electrochim. Acta · 1995 · 11 · 174110.1016/0013-4686(94)00361-4 ↗
43. Jiang · Int. J. Hydrogen Energy · 2010 · 35 · 832210.1016/j.ijhydene.2009.12.008 ↗
44. Grimaud · J. Mater. Chem. · 2012 · 22 · 1601710.1039/c2jm31812a ↗
45. Adler · Solid State Ionics · 1998 · 111 · 12510.1016/S0167-2738(98)00179-9 ↗