Abstract A Protonic Ceramic Fuel Cell based on commercial powder has been made by wet chemical routes. The NiO–BaCe0.9Y0.1O3−δ substrate was initially elaborated by tape-casting, pre-sintered then a BaCe0.9Y0.1O3−δ electrolyte was deposited by screen printing method. The whole half-cell is co-fired then Nd2NiO4+δ cathode is coated by screen-printing onto half-cells. A high and stable open circuit voltage was measured at the operating temperature of 600 °C (OCV = 1.06 V), indicating excellent gas-tightness of the protonic ceramic membrane. Although, the single cell shows modest power density of 60 mW cm−2, for the first time, nearly 1000 h at 600 °C have been successfully operated without any loss voltage. Post-test analysis didn't evidence any delamination, reactivity or decomposition of any layer, meaning a good chemical stability of selected materials during fuel cell operation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Fuel Cells and Related Materials · Thermal Expansion and Ionic Conductivity

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Khani · J. Solid State Chem. · 2009 · 182 · 79010.1016/j.jssc.2008.12.020 ↗
2. Ding · J. Power Sources · 2011 · 196 · 260210.1016/j.jpowsour.2010.10.069 ↗
3. Wang · J. Rare Earths · 2011 · 29 · 67810.1016/S1002-0721(10)60521-2 ↗
4. Pasierb · J. Power Sources · 2011 · 196 · 620510.1016/j.jpowsour.2011.03.080 ↗
5. Dailly · Electrochem. Acta · 2010 · 55 · 584710.1016/j.electacta.2010.05.034 ↗
6. Wang · Ceram. Int. · 2012 · 38 · 173710.1016/j.ceramint.2011.09.023 ↗
7. Dailly · J. Solid State Electrochem. · 2011 · 15 · 24510.1007/s10008-010-1188-4 ↗
8. Yang · Int. J. Hydrogen Energy · 2011 · 36 · 226610.1016/j.ijhydene.2010.11.053 ↗
9. Hibino · J. Electrochem. Soc. · 2002 · 149 · A150310.1149/1.1513983 ↗
10. Tao · J. Power Sources · 2010 · 195 · 348110.1016/j.jpowsour.2009.12.047 ↗
11. Fu · J. Power Sources · 2010 · 195 · 265910.1016/j.jpowsour.2009.10.069 ↗
12. Suksamai · Solid State Ionics · 2007 · 178 · 62710.1016/j.ssi.2007.02.003 ↗
13. Shimura · Solid State Ionics · 2005 · 176 · 294510.1016/j.ssi.2005.09.027 ↗
14. Katahira · Solid State Ionics · 2000 · 138 · 9110.1016/S0167-2738(00)00777-3 ↗
15. Kim · Thin Solid Films · 2011 · 520 · 101510.1016/j.tsf.2011.08.013 ↗
16. Zakowsky · Solid State Ionics · 2005 · 176 · 301910.1016/j.ssi.2005.09.040 ↗
17. Proton conducting ceramic cells: status and prospects
18. Guo · Int. J. Hydrogen Energy · 2011 · 36 · 168310.1016/j.ijhydene.2010.10.081 ↗
19. Sun · J. Power Sources · 2011 · 196 · 6210.1016/j.jpowsour.2010.07.038 ↗
20. Dailly · 2008
21. Taillades · Fuel Cells · 2010 · 10 · 16610.1002/fuce.200900033 ↗
22. Zhao · Int. J. Hydrogen Energy · 2010 · 35 · 376910.1016/j.ijhydene.2010.01.039 ↗
23. Bi · Int. J. Hydrogen Energy · 2009 · 34 · 242110.1016/j.ijhydene.2008.12.087 ↗