journal article·2014-12

Additive effect of ionic liquids on the electrochemical property of a sulfur composite electrode for all-solid-state lithium–sulfur battery

Shunji Kinoshita, Kazuya Okuda, Nobuya Machida, Toshihiko Shigematsu

Publisher page

Abstract

Abstract We investigated additive effect of five kinds of ionic liquids, such as 1-ethyl-3-methyl-imidazolium bis(trifluoromethane-sulfonyl)imide [EMI][TFSI], 1-ethyl-3-methyl-imidazolium tetrafluoroborate [EMI][BF4], 1-buthyl-3-methyl-imidazolium bis(trifluoromethane- sulfonyl) imide [BMI][TFSI], 1-buthyl-3-methyl-imidazolium tetrafluoroborate [BMI][BF4], and/or 1-buthyl-3-methyl-imidazolium iodide [BMI][I], on electrochemical properties of the sulfur composite electrode for all-solid-state lithium–sulfur batteries. The sulfur composite electrode that was composed of sulfur (29.9 wt%), vapor-grown carbon fiber (VGCF, 9.9 wt%), solid electrolyte (amorphous Li3PS4, 60.0 wt%), and [EMI][TFSI] (0.2 wt%) showed high initial specific capacity of 1270 mAh g−1 at 25 °C, which was calculated on the base of the weight of sulfur. To construct a laboratory-scale all-solid-state battery, amorphous Li3PS4 and meta-stable Li4.4Si alloy were used as solid electrolyte and as negative electrode materials, respectively. The laboratory-scale all-solid-state battery showed good discharge–charge cycle performance under a constant current density of 0.1 mA cm−2 (24 mA g−1) at room temperature and retained the large specific capacity more than 1230 mAh g−1 even after 50 cycles at 25 °C. The capacity after 50 cycles was about 97% of the initial capacity of the test cell.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Battery Materials and Technologies · Perovskite Materials and Applications · Advanced battery technologies research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Bruce · Nat. Mater. · 2012 · 11 · 1910.1038/nmat3191 ↗
2. 2012
3. Rauh · J. Electrochem. Soc. · 1979 · 126 · 52310.1149/1.2129079 ↗
4. Ellis · Chem. Mater. · 2012 · 22 · 69110.1021/cm902696j ↗
5. Mikhaylik · J. Electrochem. Soc. · 2004 · 151 · A196910.1149/1.1806394 ↗
6. Peled · J. Power Sources · 1989 · 26 · 26910.1016/0378-7753(89)80133-8 ↗
7. Peramunage · Science · 1993 · 261 · 102910.1126/science.261.5124.1029 ↗
8. Ji · J. Mater. Chem. · 2010 · 20 · 982110.1039/b925751a ↗
9. Peled · J. Electrochem. Soc. · 1989 · 136 · 162110.1149/1.2096981 ↗
10. Cheon · J. Electrochem. Soc. · 2003 · 150 · A79610.1149/1.1571532 ↗
11. Rao · J. Electrochem. Soc. · 1981 · 128 · 94210.1149/1.2127579 ↗
12. Hayashi · Electrochem. Commun. · 2003 · 5 · 70110.1016/S1388-2481(03)00167-X ↗
13. Nagao · J. Mater. Chem. · 2012 · 22 · 1001510.1039/c2jm16802b ↗
14. Machida · Solid State Ionics · 2004 · 175 · 24710.1016/j.ssi.2003.11.033 ↗
15. Machida · Chem. Lett. · 2004 · 33 · 37610.1246/cl.2004.376 ↗
16. Nagao · J. Power Sources · 2013 · 222 · 23710.1016/j.jpowsour.2012.08.041 ↗
17. Nagao · J. Power Sources · 2013 · 243 · 6010.1016/j.jpowsour.2013.05.037 ↗
18. Kinoshita · Solid State Ionics · 2014 · 256 · 9710.1016/j.ssi.2013.12.045 ↗
19. Hayashi · J. Am. Ceram. Soc. · 2001 · 84 · 47710.1111/j.1151-2916.2001.tb00685.x ↗
20. Hayashi · Electrochem. Commun. · 2003 · 5 · 11110.1016/S1388-2481(02)00555-6 ↗
21. Nagao · Electrochim. Acta · 2011 · 56 · 605510.1016/j.electacta.2011.04.084 ↗
22. Agostini · Solid State Ionics · 2013 · 244 · 4810.1016/j.ssi.2013.04.024 ↗
23. Nagao · Energy Technol. · 2013 · 1 · 18610.1002/ente.201200019 ↗
24. Bonhôte · Inorg. Chem. · 1996 · 35 · 116810.1021/ic951325x ↗
25. Turner · J. Phys. Chem. A · 2003 · 107 · 227710.1021/jp021694w ↗
26. Tsuzuki · J. Phys. Chem. B · 2005 · 109 · 1647410.1021/jp0533628 ↗
27. Atilhan · Ind. Eng. Chem. Res. · 2013 · 52 · 1677410.1021/ie403065u ↗
28. Welton · Chem. Rev. · 2008 · 99 · 229
29. Wasserscheid · Angew. Chem. Int. Ed. · 2000 · 39 · 377210.1002/1521-3773(20001103)39:21<3772::AID-ANIE3772>3.0.CO;2-5 ↗
30. Seddon · Nat. Mater. · 2003 · 2 · 36310.1038/nmat907 ↗
31. Seki · J. Power Sources · 2013 · 243 · 32310.1016/j.jpowsour.2013.06.005 ↗
32. Ueno · J. Phys. Chem. C · 2013 · 117 · 2050910.1021/jp407158y ↗
33. Park · J. Phys. Chem. C · 2013 · 117 · 2053110.1021/jp408037e ↗
34. Armand · Nat. Mater. · 2009 · 8 · 62110.1038/nmat2448 ↗
35. Park · J. Phys. Chem. C · 2013 · 117 · 443110.1021/jp400153m ↗
36. Machida · Solid State Ionics · 2005 · 176 · 47310.1016/j.ssi.2004.08.019 ↗
37. Hashimoto · Solid State Ionics · 2004 · 175 · 17710.1016/j.ssi.2004.08.022 ↗
38. Tamori · J. Jpn. Soc. Powder Powder Metall. · 2001 · 48 · 26710.2497/jjspm.48.267 ↗